THERMAL STABILITY OF PLASTICS BINDING ISOTROPIC Nd-Fe-B MAGNET
XIAO Yaofu;ZHANG Zhengyi;QIU Baoqin University of Science and Technology Beijing; YU Xiangli;ZHANG Qi;ZHANG Hong Factory No. 8272; Jilin
Cite this article: 

XIAO Yaofu;ZHANG Zhengyi;QIU Baoqin University of Science and Technology Beijing; YU Xiangli;ZHANG Qi;ZHANG Hong Factory No. 8272; Jilin. THERMAL STABILITY OF PLASTICS BINDING ISOTROPIC Nd-Fe-B MAGNET. Acta Metall Sin, 1991, 27(2): 154-156.

Download:  PDF(265KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The reversible and irreversible losses of open-circuit magnetic flux ofthe plastics binding isotropic Nd-Fe-B magnet were determined. The reversible tem-perature coefficient of the plastics binding Nd-Fe-B permanent magnet was detectedto be similar to that of sintering one, yet the irreversible loss and long-term agingloss of the former are far smaller than the later.
Key words:  binding Nd-Fe-B magnet      thermal stability      irreversible loss     
Received:  18 February 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I2/154

1 Lee R W. Appl Phys Lett, 1985; 46: 790
2 Martin D L. In: Strnat K J ed, Proc 5th International Workshop on Rare Earth-Cobalt Permanent Magnets and their Applications, University of Dayton, Dayton. Ohio. 1981: 371--401
3 肖耀福.磁性材料与器件,1989;20(3) :22--26
4 Li D, Mildrum H F, Strnat K J. J Appl Phys. 1985; 57: 414
[1] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[2] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[3] NIE Jinfeng, WU Yuli, XIE Kewei, LIU Xiangfa. Microstructure and Thermal Stability of Heterostructured Al-AlN Nanocomposite[J]. 金属学报, 2022, 58(11): 1497-1508.
[4] WANG Yihan, YUAN Yuan, YU Jiabin, WU Honghui, WU Yuan, JIANG Suihe, LIU Xiongjun, WANG Hui, LU Zhaoping. Design for Thermal Stability of Nanocrystalline Alloys Based on High-Entropy Effects[J]. 金属学报, 2021, 57(4): 403-412.
[5] WANG Xiaobo, WANG Yongzhe, CHENG Xudong, JIANG Rong. Thermal Stability of AlCrON-Based Solar Selective Absorbing Coating in Air[J]. 金属学报, 2021, 57(3): 327-339.
[6] PENG Yanyan, YU Liming, LIU Yongchang, MA Zongqing, LIU Chenxi, LI Chong, LI Huijun. Effect of Ageing Treatment at 650 ℃ on Microstructure and Properties of 9Cr-ODS Steel[J]. 金属学报, 2020, 56(8): 1075-1083.
[7] HUANG Yu, CHENG Guoguang, LI Shijian, DAI Weixing. Precipitation Mechanism and Thermal Stability of Primary Carbide in Ce Microalloyed H13 Steel[J]. 金属学报, 2019, 55(12): 1487-1494.
[8] Jianxiong ZOU,Bo LIU,Liwei LIN,Ding REN,Guohua JIAO,Yuanfu LU,Kewei XU. Microstructure and Thermal Stability of MoC DopedRu-Based Alloy Films as Seedless Diffusion Barrier[J]. 金属学报, 2017, 53(1): 31-37.
[9] Weiwei GUO,Chengjun QI,Xiaowu LI. INVESTIGATIONS ON THERMAL STABILITY OF FATIGUE DISLOCATION STRUCTURES IN CONJUGATE AND CRITICAL DOUBLE-SLIP-ORIENTED Cu SINGLE CRYSTALS[J]. 金属学报, 2016, 52(6): 761-768.
[10] YANG Bin, LI Xin, LUO Wendong, LI Yuxiang. EFFECT OF MINOR Sn AND Nb ADDITIONS ON THE THERMAL STABILITY AND COMPRESSIVE PLASTICITY OF Zr-Cu-Fe-Al BULK METALLIC GLASS[J]. 金属学报, 2015, 51(4): 465-472.
[11] LIU Wenbo, ZHANG Chi, YANG Zhigang, XIA Zhixin, GAO Guhui, WENG Yuqing. EFFECT OF SURFACE NANOCRYSTALLIZATION ON MICROSTRUCTURE AND THERMAL STABILITY OF REDUCED ACTIVATION STEEL[J]. 金属学报, 2013, 49(6): 707-716.
[12] ZHANG Lidong, WANG Fei, CHEN Shunli, WANG Yuan. FABRICATION AND THERMAL STABILITY OF AlCrTaTiNi/(AlCrTaTiNi)N BILAYER DIFFUSION BARRIER[J]. 金属学报, 2013, 49(12): 1611-1616.
[13] FANG Lu,DING Xianfei, ZHANG Laiqi, HAO Guojian, LIN Junpin. MICROSTRUCTURE STABILITY IN A FULLY LAMELLAR HIGH Nb-TiAl ALLOY AFTER LONG-TERM THERMAL CYCLING[J]. 金属学报, 2013, 49(11): 1416-1422.
[14] ZHANG Yanpo, REN Ding, LIN Liwei,YANG Bin, WANG Shanling,LIU Bo1), XU Kewei. CONTROLLED REACTION ON INTERFACE OF Cu/Cu(Ge, Zr)/SiO2/Si MULTILAYER FILM AND ITS THERMAL STABILITY[J]. 金属学报, 2013, 49(10): 1264-1268.
[15] GUO Weiwei, QI Chengjun, LI Xiaowu. INVESTIGATIONS ON THERMAL STABILITY OF FATIGUE DISLOCATION STRUCTURES IN A DOUBLE-SLIPORIENTED Cu SINGLE CRYSTAL[J]. 金属学报, 2013, 49(1): 107-114.
No Suggested Reading articles found!