SUPERPLASTICITY OF Al-Zn-Mg-Zr-RE AND Al-Zn-Mg-Ti ALLOYS AND THEIR CAVITA-TION BEHAVIOUR DURING DEFORMATION
ZHAO Youchang;LIU Aihong Jilin University; Changchun
Cite this article: 

ZHAO Youchang;LIU Aihong Jilin University; Changchun. SUPERPLASTICITY OF Al-Zn-Mg-Zr-RE AND Al-Zn-Mg-Ti ALLOYS AND THEIR CAVITA-TION BEHAVIOUR DURING DEFORMATION. Acta Metall Sin, 1990, 26(5): 137-141.

Download:  PDF(568KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The superplasticity of the Al-Zn-Mg-Zr-RE (alloy A) and Al-Zn-Mg-Ti (alloy B), their change of volume fraction of metastable micro-cavitiesunder various reduction and strain rates, as well as the growth of stable cavitiesin them have been studied by small X-ray scattering analysis and quantitative me-tallography respectively. Experimental results show that the volume fraction ofmetastable micro-cavities of the alloy A is more than that of the alloy B, butthe growing rate of stable cavities of the alloy A is less than that of the alloyB. Thus, it is believed that the superplasticity of the al1oy A is superior to thatof the alloy B.
Key words:  Al-Zn-Mg alloy      superplasticity      cavity      strain rate     
Received:  18 May 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I5/137

1 Matsuki K, Morita H, Yamada M, Murakami Y. Met Sci, 1977; 11: 156
2 Grimes R. Stowell M J, Watts B M. Met Technol, 1976; 3: 154
3 Towler B. J Inst Met, 1973; 101: 332
4 金华,柳善英.轻金属,1983;(7) :55
5 崔建忠.东北工学院学报,1986;(4) :1
6 Zhang J Y, Liu C L. Mod Dev Powder Metall, 1981; 12: 47
7 Shei S A, Langdon T G. Mater Sci J, 1978; 13: 1084
8 Livesey D W, Ridley N. Metall Trans, 1978; 9A: 519
9 Stowell M J. Met Sci, 1980; 14: 267
[1] WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei. Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K[J]. 金属学报, 2023, 59(2): 277-288.
[2] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[3] WANG Nan, CHEN Yongnan, ZHAO Qinyang, WU Gang, ZHANG Zhen, LUO Jinheng. Effect of Strain Rate on the Strain Partitioning Behavior of Ferrite/Bainite in X80 Pipeline Steel[J]. 金属学报, 2023, 59(10): 1299-1310.
[4] CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng. Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact[J]. 金属学报, 2022, 58(5): 660-672.
[5] WANG Huiyuan, XIA Nan, BU Ruyu, WANG Cheng, ZHA Min, YANG Zhizheng. Current Research and Future Prospect on Low-Alloyed High-Performance Wrought Magnesium Alloys[J]. 金属学报, 2021, 57(11): 1429-1437.
[6] Xiangru GUO, Chaoyang SUN, Chunhui WANG, Lingyun QIAN, Fengxian LIU. Investigation of Strain Rate Effect by Three-Dimensional Discrete Dislocation Dynamics for fcc Single Crystal During Compression Process[J]. 金属学报, 2018, 54(9): 1322-1332.
[7] Xudong LI, Pingli MAO, Yanyu LIU, Zheng LIU, Zhi WANG, Feng WANG. Anisotropy and Deformation Mechanisms ofAs-Extruded Mg-3Zn-1Y Magnesium AlloyUnder High Strain Rates[J]. 金属学报, 2018, 54(4): 557-565.
[8] Guangming XIE, Zongyi MA, Peng XUE, Zongan LUO, Guodong WANG. Effects of Tool Rotation Rates on Superplastic Deformation Behavior of Friction Stir Processed Mg-Zn-Y-Zr Alloy[J]. 金属学报, 2018, 54(12): 1745-1755.
[9] Huiyuan WANG, Hang ZHANG, Xinyu XU, Min ZHA, Cheng WANG, Pinkui MA, Zhiping GUAN. Current Research and Future Prospect on Microstructure Stability of Superplastic Light Alloys[J]. 金属学报, 2018, 54(11): 1618-1624.
[10] Xifeng LI, Nannan CHEN, Jiaojiao LI, Xueting HE, Hongbing LIU, Xingwei ZHENG, Jun CHEN. Effect of Temperature and Strain Rate on Deformation Behavior of Invar 36 Alloy[J]. 金属学报, 2017, 53(8): 968-974.
[11] Xu YANG, Bo LIAO, Jian LIU, Wei YAN, Yiyin SHAN, Furen XIAO, Ke YANG. Embrittlement Phenomenon of China Low Activation Martensitic Steel in Liquid Pb-Bi[J]. 金属学报, 2017, 53(5): 513-523.
[12] Yun CAI,Chaoyang SUN,Li WAN,Daijun YANG,Qingjun ZHOU,Zexing SU. STUDY ON THE DYNAMIC RECRYSTALLIZATION SOFTENING BEHAVIOR OF AZ80 MAGNESIUM ALLOY[J]. 金属学报, 2016, 52(9): 1123-1132.
[13] Chao YANG,Jijie WANG,Zongyi MA,Dingrui NI,Mingjie FU,Xiaohua LI,Yuansong ZENG. FRICTION STIR WELDING AND LOW-TEMPERATURE SUPERPLASTICITY OF 7B04 Al SHEET[J]. 金属学报, 2015, 51(12): 1449-1456.
[14] SUN Chaoyang, HUANG Jie, GUO Ning, YANG Jing. A PHYSICAL CONSTITUTIVE MODEL FOR Fe-22Mn-0.6C TWIP STEEL BASED ON DISLOCATION DENSITY[J]. 金属学报, 2014, 50(9): 1115-1122.
[15] FU Mingjie, HAN Xiuquan, WU Wei, ZHANG Jianwei. SUPERPLASTICITY RESEARCH OF Ti-23Al-17Nb ALLOY SHEET[J]. 金属学报, 2014, 50(8): 955-961.
No Suggested Reading articles found!