Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (6): 5-9    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF AUSTENITE STRENGTHENING ON MARTENSITIC TRANSFORMATION IN Fe-Mn-C ALLOYS
PAN Mu;XU Zuyao T. Y. Hsu Shanghai Jiao Tong University XU Zuyao; professor; Dept. of Materials Science; Shanghai Jiao Tong University;Huashan Road; Shanghai 200030 China
Cite this article: 

PAN Mu;XU Zuyao T. Y. Hsu Shanghai Jiao Tong University XU Zuyao; professor; Dept. of Materials Science; Shanghai Jiao Tong University;Huashan Road; Shanghai 200030 China. INFLUENCE OF AUSTENITE STRENGTHENING ON MARTENSITIC TRANSFORMATION IN Fe-Mn-C ALLOYS. Acta Metall Sin, 1989, 25(6): 5-9.

Download:  PDF(538KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The M_5 temperature and the yield strength of austenite at M_5 tem-perature have been measured for five Fe-Mn-C alloys. The experimental results showthat there is a linear relationship between them. The effect of the solution strength-ening of austenite on martensite morphology is also studied. It is pointed outthat there is a characteristic temperature of strengthening in austenite, T_c. Marten-site morphology is mainly dislocated laths when M_5>T_c, and is mainly twinnedplates when M_5
Key words:  Fe-Mn-C alloy      austenite strengthening      martensitic transformation     
Received:  18 June 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I6/5

1 Nichol T J, Judd G, Ansell G S. Metall Trans, 1977; 8A: 1877
2 Hsu T Y (徐祖耀), Li Jian (李箭), Zeng Zhenpeng (曾振鹏), Metallography, 1986; 19: 305
3 Hsu T Y (徐祖耀), Chen Weichong (陈卫中). Scr Metall, 1987; 21: 1289
4 Thomas G. Metall Trans, 1971; 2A: 2373
S Kung C Y, Rayment J J. Metall Trans, 1982; 13A: 328
6 徐祖耀,金属学报,1979;15:329
7 Haasen P. In: Nabarro F R N ed, Dislocation in Solids, Vol. 4, Dislocations in Metallurgy, Amsterdan: North-Holland, 1979: 155
8 Huang D, Thomas G, Metall Trans, 1971; 2A: 1587
[1] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite[J]. 金属学报, 2023, 59(11): 1419-1427.
[2] LI Wei, JIA Xingqi, JIN Xuejun. Research Progress of Microstructure Control and Strengthening Mechanism of QPT Process Advanced Steel with High Strength and Toughness[J]. 金属学报, 2022, 58(4): 444-456.
[3] CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih. Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation[J]. 金属学报, 2022, 58(2): 175-183.
[4] YUAN Jiahua, ZHANG Qiuhong, WANG Jinliang, WANG Lingyu, WANG Chenchong, XU Wei. Synergistic Effect of Magnetic Field and Grain Size on Martensite Nucleation and Variant Selection[J]. 金属学报, 2022, 58(12): 1570-1580.
[5] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[6] ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang. Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys[J]. 金属学报, 2021, 57(11): 1396-1415.
[7] XIAO Fei, CHEN Hong, JIN Xuejun. Research Progress in Elastocaloric Cooling Effect Basing on Shape Memory Alloy[J]. 金属学报, 2021, 57(1): 29-41.
[8] CHEN Lei , HAO Shuo , MEI Ruixue , JIA Wei , LI Wenquan , GUO Baofeng . Intrinsic Increment of Plasticity Induced by TRIP and Its Dependence on the Annealing Temperature in a Lean Duplex Stainless Steel[J]. 金属学报, 2019, 55(11): 1359-1366.
[9] Lishan CUI, Daqiang JIANG. Progress in High Performance Nanocomposites Based ona Strategy of Strain Matching[J]. 金属学报, 2019, 55(1): 45-58.
[10] Cheng WEI, Changbo KE, Haitao MA, Xinping ZHANG. A Modified Phase Field Model Based on Order Parameter Gradient and Simulation of Martensitic Transformation in Large Scale System[J]. 金属学报, 2018, 54(8): 1204-1214.
[11] Zhaozhao WEI, Xiao MA, Xinping ZHANG. Topological Modelling of the B2-B19' Martensite Transformation Crystallography in NiTi Alloy[J]. 金属学报, 2018, 54(10): 1461-1470.
[12] Jilan YANG, Yuankai JIANG, Jianfeng GU, Zhenghong GUO, Haiyan CHEN. Effect of Austenitization Temperature on the Dry Sliding Wear Properties of a Medium Carbon Quenching and Partitioning Steel[J]. 金属学报, 2018, 54(1): 21-30.
[13] Xue WANG,Lei HU,Dongxu CHEN,Songtao SUN,Liquan LI. Effect of Martensitic Transformation on Stress Evolution in Multi-Pass Butt-Welded 9%Cr Heat-Resistant Steel Pipes[J]. 金属学报, 2017, 53(7): 888-896.
[14] Kejian LI,Zhipeng CAI,Yao WU,Jiluan PAN. Research on Austenite Transformation of FB2 Heat-Resistant Steel During Welding Heating Process[J]. 金属学报, 2017, 53(7): 778-788.
[15] Xiaosong ZHANG,Yong XU,Shihong ZHANG,Ming CHENG,Yonghao ZHAO,Qiaosheng TANG,Yuexia DING. Research on the Collaborative Effect of Plastic Deformation and Solution Treatment in the Intergranular Corrosion Property of Austenite Stainless Steel[J]. 金属学报, 2017, 53(3): 335-344.
No Suggested Reading articles found!