| CORRELATION BETWEEN OXIDATION BEHAVIOUR AND BORON CONTENT IN Ni_3Al |
| GUO Jianting;SUN Chao;LI Hui;GUAN Hengrong Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
GUO Jianting;SUN Chao;LI Hui;GUAN Hengrong Institute of Metal Research; Academia Sinica; Shenyang. CORRELATION BETWEEN OXIDATION BEHAVIOUR AND BORON CONTENT IN Ni_3Al. Acta Metall Sin, 1989, 25(4): 120-125.
|
|
|
Abstract The effect of boron content (0 to 2.22 at.-%) on isothermal oxida-tion behaviour of Ni_3Al at 750 to 1150℃ for 3 to 100h has been studied. Theresults show that the isothermal oxidation kinetics of Ni_3Al with various B contentsat different temperatures obeys the parabolic law. The compounds with 0.52 to1.37 at.%B show the best oxidation resistance. The morphology and microstructureof the scales have also been investigated.
|
|
Received: 18 April 1989
|
1 青木清,和泉修.日本金属学会志,1979;43:1190 2 李辉,刘祥,郭建亭,胡壮麒.金属学报,1989;A25: 3 郭建亭.金属学报,1979;15:203 4 Chou T C, Chou Y T. In: Koch C C, Liu C T, Stoloff N S eds., High-Temperature Ordered Intermetallic Alloys, Mat. Res. Soc. Symp. Proc. Vol. 39, 1985: 461 5 Taniguehi S, Shibata T. Tsuruoka H. Oxid Met, 1986; 26: 1 6 郭建亭,李辉,孙超,朱耀宵.金属学报,待发表$ |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|