Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (1): 122-127    DOI:
Current Issue | Archive | Adv Search |
MECHANISM OF Al/Cu CONTACTING REACTION BRAZING
CHEN Dinghua;QIAN Yiyu;HUANG Jihua Harbin Institute of Technology
Cite this article: 

CHEN Dinghua;QIAN Yiyu;HUANG Jihua Harbin Institute of Technology. MECHANISM OF Al/Cu CONTACTING REACTION BRAZING. Acta Metall Sin, 1989, 25(1): 122-127.

Download:  PDF(1708KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The reactive spread behaviour of Cu particles on the surface of Alhas been studied. The role of oxide film and the formation mechanism of the jointduring Al/Cu contacting reaction brazing have been discussed.
Key words:  Al/Cu interface      brazing      reaction spread      oxide film     
Received:  18 January 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I1/122

1 #12
2 宫崎邦本,五村达雄.日本金属学会讲演概要,1981;(88) :272
3 五村达雄,宫崎邦本,落合和泉.溶接学会全国大会讲演概要,1980;(27) :370
4 #12
5 Feng Z C, Yi Y S, Xu Y B, Hou L T. Quality and Reliability in Welding Proc Int Conf, Hangzhou, China, 6-8 Sept. 1984, Harbin, China: Welding Institution of the Chinese Mechanical Engineering Society (CMES), 1984, Vol. Ⅰ. Session A. Paper A11--6
6 Verhoeven J D著,卢光熙,赵子伟译,物理冶金学基础,上海科学技术出版社,1980:88
[1] SI Yongli, XUE Jintao, WANG Xingfu, LIANG Juhua, SHI Zimu, HAN Fusheng. Effect of Cr Addition on the Corrosion Behavior of Twinning-Induced Plasticity Steel[J]. 金属学报, 2023, 59(7): 905-914.
[2] SHEN Zhao, WANG Zhipeng, HU Bo, LI Dejiang, ZENG Xiaoqin, DING Wenjiang. Research Progress on the Mechanisms Controlling High-Temperature Oxidation Resistance of Mg Alloys[J]. 金属学报, 2023, 59(3): 371-386.
[3] LIU Laidi, DING Biao, REN Weili, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Multilayer Structure of DZ445 Ni-Based Superalloy Formed by Long Time Oxidation at High Temperature[J]. 金属学报, 2023, 59(3): 387-398.
[4] SUN Rongrong, YAO Meiyi, LIN Xiaodong, ZHANG Wenhuai, QIU Yunlong, HU Lijuan, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. Effect of Ti on the Corrosion Behavior of Fe22Cr5Al3Mo Alloy in 500oC Superheated Steam[J]. 金属学报, 2022, 58(5): 610-622.
[5] LIN Xiaodong, MA Haibin, REN Qisen, SUN Rongrong, ZHANG Wenhuai, HU Lijuan, LIANG Xue, LI Yifeng, YAO Meiyi. Corrosion Behaviors of Fe13Cr5Al4Mo Alloy in High-Temperature High-Pressure Water Environments[J]. 金属学报, 2022, 58(12): 1611-1622.
[6] QIAN Yue,SUN Rongrong,ZHANG Wenhuai,YAO Meiyi,ZHANG Jinlong,ZHOU Bangxin,QIU Yunlong,YANG Jian,CHENG Guoguang,DONG Jianxin. Effect of Nb on Microstructure and Corrosion Resistance of Fe22Cr5Al3Mo Alloy[J]. 金属学报, 2020, 56(3): 321-332.
[7] ZHAO Xu,SUN Yuan,HOU Xingyu,ZHANG Hongyu,ZHOU Yizhou,DING Yutian. Effect of Orientation Deviation on Microstructure and Mechanical Properties of Nickel-Based Single Crystal Superalloy Brazing Joints[J]. 金属学报, 2020, 56(2): 171-181.
[8] Xiaoyi ZHANG, Hailong SHANG, Bingyang MA, Rongbin LI, Geyang LI. Brazing of Coated Al Foil Filler to AlN Ceramic[J]. 金属学报, 2018, 54(4): 575-580.
[9] Geliang LIU, Bingyang MA, Hailong SHANG, Fan CHEN, Rongbin LI, Geyang LI. Wettability Improvement and Brazing of Si3N4by Sputtered Al[J]. 金属学报, 2017, 53(12): 1645-1650.
[10] Zhongbo YANG,Wenjin ZHAO,Zhuqing CHENG,Jun QIU,Hai ZHANG,Hong ZHUO. Effect of Nb Content on the Corrosion Resistance of Zr-xNb-0.4Sn-0.3Fe Alloys[J]. 金属学报, 2017, 53(1): 47-56.
[11] Yuan SUN,Jide LIU,Xingyu HOU,Guanglei WANG,Jinxia YANG,Tao JIN,Yizhou ZHOU. MICROSTRUCTURE EVOLUTION AND INTERFACIAL FORMATION MECHANISM OF WIDE GAP BRAZING OF DD5 SINGLE CRYSTAL SUPERALLOY[J]. 金属学报, 2016, 52(7): 875-882.
[12] Wei FU,Xiaoguo SONG,Long LONG,Jianhang CHAI,Jicai FENG,Guodong WANG. INTERFACIAL MICROSTRUCTURE AND MECHANI-CAL PROPERTIES OF INDIRECT BRAZED GRAPHITE/COPPER JOINT[J]. 金属学报, 2016, 52(6): 734-740.
[13] Jiazhen WANG,Jianqiu WANG,En-Hou HAN. CORROSION BEHAVIOR OF ALLOY 800 IN NaOH AND ETA SOLUTIONS AT 300 ℃[J]. 金属学报, 2016, 52(5): 599-606.
[14] Meiqiong OU,Yang LIU,Xiangdong ZHA,Yingche MA,Leming CHENG,Kui LIU. CORROSION BEHAVIOR OF A NEW NICKEL BASE ALLOY IN SUPERCRITICAL WATERCONTAINING DIVERSE IONS[J]. 金属学报, 2016, 52(12): 1557-1564.
[15] Jianqiu WANG, Fa HUANG, Wei KE. CORROSION BEHAVIORS OF INCONEL 690TT AND INCOLOY 800MA STEAM GENERATOR TUBES IN HIGH TEMPERATURE HIGH PRESSURE WATER[J]. 金属学报, 2016, 52(10): 1333-1344.
No Suggested Reading articles found!