Acta Metall Sin  1988, Vol. 24 Issue (6): 410-414    DOI:
Current Issue | Archive | Adv Search |
ELECTRONIC STRUCTURE OF γ′-PHASE IN SUPERALLOY CONTAINING Mg AND W
ZHU Kai;WANG Chongyu University of Science and Technology of China; Hefei Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing
Cite this article: 

ZHU Kai;WANG Chongyu University of Science and Technology of China; Hefei Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. ELECTRONIC STRUCTURE OF γ′-PHASE IN SUPERALLOY CONTAINING Mg AND W. Acta Metall Sin, 1988, 24(6): 410-414.

Download:  PDF(334KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The calculation of electronic structure of γ'-Ni_3 Al phase with orwithout Mg and W by the Recusion and LCAO mehtods clarified that Mg and Watoms lose their outer electrons partially after they entered γ'-Ni_3 Al. It causes thereduction of the radii of atoms (so it is preferable for Mg atom to enter γ' phase bythe substitution). Thus, the interaction between Mg and γ'-phase matrix may bestrengthened and a more stable structure of γ'-phase may be formed while Mg andW entered simultaneously γ'-Ni_3 Al.
Key words:  superalloy      Ni_3Al_1      electronic structure      Mg alloying     
Received:  18 June 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I6/410

1 马培立,庄景云,朱静,杨锦炎,仲增墉,高良.金属学报,1987;23:A484
2 马培立,庄景云,杨锦炎,高良,金属学报,1987;23:A195
3 Haydock R, Heine V, Kelly M J. J Phys, C, 1972; 5: 2845 Haydock R, Heine V, Kelly M J. J Phys, C, 1975; 8: 2591
4 Ehrenteich H, Seitz F, Turnbull D. Solid State Physics, Vol. 35, New York: Academic Press, 1980
5 Pettifor D G, Weaire D L. The Recursion Method and it's Applications, Berlin: Springer-Verlag, 1985
6 Nex C M M. J Phys, A1978; 11: 653
7 Harrison W A. Electronic Structure and Properties of Solids, Freeman, San Francisco, 1980: 482
[1] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[4] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[5] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[6] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[7] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[8] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[9] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[10] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[11] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[12] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[13] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[14] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[15] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
No Suggested Reading articles found!