| DISTRIBUTION OF Ce AND S IN Fe-C-Si ALLOY AND THEIR INFLUENCE ON MORPHOLOGY OF GRAPHITE |
| DU Weixi;HAN Qiyong;JIAN Qing;ZHANG Zhongzhi;ZHONG Weizhen;LIU Shaoshou Jilin University of Technology Beijing University of Iron and Steel Technology |
|
Cite this article:
DU Weixi;HAN Qiyong;JIAN Qing;ZHANG Zhongzhi;ZHONG Weizhen;LIU Shaoshou Jilin University of Technology Beijing University of Iron and Steel Technology. DISTRIBUTION OF Ce AND S IN Fe-C-Si ALLOY AND THEIR INFLUENCE ON MORPHOLOGY OF GRAPHITE. Acta Metall Sin, 1988, 24(5): 385-391.
|
|
|
Abstract Electrolytic extraction-radiometry and microradioautography tech-niques were used to study the distribution of nodulizing element Ce and anti-nodulizing element S in phases of high purity Fe-C-Si alloy. The results show that,besides forming inclusions, most of Ce atoms concentrate in graphite firstly. As theCe content increase, the concentration of Ce in graphite tends to saturate, relati-vely large amount of Ce dissolves in the alloy. Usually, the sulphur also concen-trates in graphite, however, it may exist in the form of FeS at the eutectic colonyboundaries, if the concentration of S is at a quite high level. Very little amountof S dissolves in the alloy. The morphology of graphite depends upon the degreeof saturation of Ce. It appears as nodula when Ce was saturated, and as vermicularwhile it was semi-saturated.
|
|
Received: 18 May 1988
|
1 蒋青,杜维玺,韩其勇,张钟植,孙大仁,刘绍收.采用放射性同位素示踪等方法研究稀土在铸铁中的作用机制,金属科学与工艺,(待发表) 2 韩其勇,吴卫江,方克明,卢静,张保军,谢德义,裴丽侠.金属学报,1979;15:1 3 蒋青,韩其勇,杜维玺,赵慧玲,于小芳,陈永泰.金属科学与工艺,1986;5(2) :49 4 霍成章,韩其勇,钟伟珍,李宝山.中国稀土学报,1986;4(1) :30 5 蒋青,杜维玺,韩其勇,钟伟珍,赵慧玲,于小芳.中国稀土学报,1986;4(3) :51 6 钟伟珍,韩其勇,霍成章,刘秀琨,姜玉贤,李晓光,张子荣,金属学报,1986;22:B197 7 杜维玺,蒋青,韩其勇,张钟植,孙大仁,曹占义.Ce.S在工业铸铁中的分布及交互作用,机械工程学报,(待发表) 8 韩其勇,董元篪,丰锡安,项长祥,杨斯馥.金属学报,1984;20:A204 10 #12 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|