INFLUENCE OF MOULD ROTATION ON MACROSEGREGATION IN INGOT
YU Qiuping;ZHOU Yaohe Northwestern Polytechnical University; Xi'an
Cite this article: 

YU Qiuping;ZHOU Yaohe Northwestern Polytechnical University; Xi'an. INFLUENCE OF MOULD ROTATION ON MACROSEGREGATION IN INGOT. Acta Metall Sin, 1988, 24(5): 379-384.

Download:  PDF(950KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The macrosegregation formation in an ingot and the influence of rotat-ing mould upon it were analysed on the basis of the interdendritic flow. When theingot mould rotates unidirectionally, the centrifugal volume force acts on all innerparts and when the ingot mould rotates attenately, the tangential alternate force isalso formed, and both have various influences on the different modes of interden-dritic flow. It is shown that as the ingot mould rotates unidirectionally or alterna-tely with moderate angular speed, the interdendritic unstable flow may be control-led effectively and the formation of segregation may be restrained. Thus, it seemsto be significant for reducing the segregation such as A-type, etc., in the steel in-got.
Key words:  ingot      macrosegregation      interdendritic flow     
Received:  18 May 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/379

1 Kirkaldy J S, Youdelis W V. Trans Metall Soc AIME, 1958; 212: 833--840
2 Mehrabian R, Keane M, Flemings M C. Metall Trans, 1970; 1: 1209--1220
3 McDonald R J. Hunt J D. Trans Metall Soc AIME, 1969; 245: 1993--1997
4 Stewart M J, MacAulay L C. Weinberg P. Metall Trans, 1971; 2: 169--173
5 Kou S, Poirier D R Flemings M C. Metall Trans 1978; 9B: 711--719
6 Moore J J, Shah N A. Int Metall Rev, 1983; 28: 338--356
7 喻秋平,枝晶间液相流动与宏观偏析,西北工业大学科技资料,CL8613,1986
[1] FENG Miaomiao, ZHANG Hongwei, SHAO Jingxia, LI Tie, LEI Hong, WANG Qiang. Prediction of Macrosegregation of Fe-C Peritectic Alloy Ingot Through Coupling with Thermodynamic Phase Transformation Path[J]. 金属学报, 2021, 57(8): 1057-1072.
[2] WANG Tao,WAN Zhipeng,LI Zhao,LI Peihuan,LI Xinxu,WEI Kang,ZHANG Yong. Effect of Heat Treatment Parameters on Microstructure and Hot Workability of As-Cast Fine Grain Ingot of GH4720Li Alloy[J]. 金属学报, 2020, 56(2): 182-192.
[3] Chunlei WU,Dewei LI,Xiaowei ZHU,Qiang WANG. Influence of Electromagnetic Swirling Flow in Nozzle on Solidification Structure and Macrosegregation of Continuous Casting Square Billet[J]. 金属学报, 2019, 55(7): 875-884.
[4] Jun LI, Mingxu XIA, Qiaodan HU, Jianguo LI. Solutions in Improving Homogeneities of Heavy Ingots[J]. 金属学报, 2018, 54(5): 773-788.
[5] Houfa SHEN, Kangxin CHEN, Baicheng LIU. Numerical Simulation of Macrosegregation inSteel Ingot Casting[J]. 金属学报, 2018, 54(2): 151-160.
[6] Jun LI, Junge WANG, Fengli REN, Honghao GE, Qiaodan HU, Mingxu XIA, Jianguo LI. Experimental and Numerical Simulation Study on Layer Casting Method for Composition Homogeneityon Ingot Casting[J]. 金属学报, 2018, 54(1): 118-128.
[7] Jianbo YU, Yuan HOU, Chao ZHANG, Zhibin YANG, Jiang WANG, Zhongming REN. Effect of High Magnetic Field on the Microstructure in Directionally Solidified Co-Al-W Alloy[J]. 金属学报, 2017, 53(12): 1620-1626.
[8] Jun LI,Honghao GE,Menghuai WU,Andreas LUDWIG,Jianguo LI. A COLUMNAR & NON-GLOBULAR EQUIAXED MIXED THREE-PHASE MODEL BASED ON THERMOSOLUTAL CONVECTION AND GRAIN MOVEMENT[J]. 金属学报, 2016, 52(9): 1096-1104.
[9] Beijiang ZHANG,Guangpu ZHAO,Wenyun ZHANG,Shuo HUANG,Shifu CHEN. INVESTIGATION OF HIGH PERFORMANCE DISC ALLOY GH4065 AND ASSOCIATED ADVANCED PROCESSING TECHNIQUES[J]. 金属学报, 2015, 51(10): 1227-1234.
[10] LI Jizhan, FU Ying, JIE Jinchuan, ZHAO Jialei, Joonpyo Park, Jongho Kim,LI Tingju. CONTINUOUS CASTING OF THE CLADDING 3003/4004 ALUMINUM ALLOY CIRCULAR INGOT[J]. 金属学报, 2013, 49(3): 297-302.
[11] Hai-Dong ZHAO; Chao-Zhong WU; Yuan-Yuan LI; Itsuo OHNAKA. Modeling of Microporosity Formation in a Vertical Upward Unidirectional Solidification Al-Cu Casting[J]. 金属学报, 2008, 44(11): 1340-1347 .
[12] Tongmin Wang. MODELLING THE THERMO-SOLUTAL CONVECTION, SHRINKAGE FLOW AND GRAIN MOVEMENT DURING GLOBULAR EQUIAXED SOLIDIFICATION IN A MULTI-PHASE SYSTEM II. MODEL APPLICATION[J]. 金属学报, 2006, 42(6): 591-598 .
[13] D R Liu. SIMULATION OF MACROSTRUCTURE EVOLUTION IN Ti-(45~48)at%Al ALLOY INGOT[J]. 金属学报, 2006, 42(4): 437-442 .
[14] . COUPLED NUMBERICAL SIMULATION ON SOLIDIFICATION AND SOLUTE TRANSPORT IN THIN SLAB CONTINUOUS CASTING PROCESS[J]. 金属学报, 2006, 42(2): 211-217 .
[15] GUO Dayong; YANG Yuansheng; TONG Wenhui; HU Zhuangqi. Numerical Simulation of Macrosegregation During Electromagnetic Centrifugal Solidification[J]. 金属学报, 2004, 40(3): 275-280 .
No Suggested Reading articles found!