A PARAMETER FOR EVALUATING ABILITY OF GRAIN REFINEMENT OF SOLUTE ELEMENTS
HAN Qingyou;HU Hanqi Beijing University of Iron and Steel Technology
Cite this article: 

HAN Qingyou;HU Hanqi Beijing University of Iron and Steel Technology. A PARAMETER FOR EVALUATING ABILITY OF GRAIN REFINEMENT OF SOLUTE ELEMENTS. Acta Metall Sin, 1988, 24(5): 392-396.

Download:  PDF(356KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The gradient of the equilibrium melting temperature on liquid side ofadvancing solid-liquid interface has been derived. From it, a parameter, H, used forevaluating the ability of grain refinement of solute elements has been proposed.Experiments on Al-base alloys show that the grain size of alloys decrease withincreasing H value. This indicates that parameter H can be used as an index forselecting the grain refiners.
Key words:  Solute elements      grain refinement     
Received:  18 May 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/392

1 胡汉起.金属凝固,冶金工业出版社,1985:89
2 Winegard W C, Chalmers B. Trans Am Soc Met, 1954; 46: 1214
3 Genolers R. J Inst Met, 1926; 35: 259
4 Papapetron A Z. Krist, 1935; A92: 89
5 大野笃美,唐彦斌,张正德译.金属凝固学,机械工业出版社,1983:88
6 韩青有,胡汉起.北京钢铁学院学报,1985;(1) :1
7 张兴中.溶质分配系数的研究,北京钢铁学院硕士研究生论文,1985
8 Smithells C J. Metals Reference Book, 5th ed., London: Butterworths, 1976
9 Rinaldi M D, Sharp R M, Flemings M C. Metall Trans. 1972; 3: 3133
10 胡汉起,钟雪友,力航.金属学报,1984;20:A247
11 胡汉起,钟雪友,韩青有,金属学报,1987;23:A176{
[1] LI Xiaobing, QIAN Kun, SHU Lei, ZHANG Mengshu, ZHANG Jinhu, CHEN Bo, LIU Kui. Effect of W Content on the Phase Transformation Behavior in Ti-42Al-5Mn- xW Alloy[J]. 金属学报, 2023, 59(10): 1401-1410.
[2] WU Guohua, TONG Xin, JIANG Rui, DING Wenjiang. Grain Refinement of As-Cast Mg-RE Alloys: Research Progress and Future Prospect[J]. 金属学报, 2022, 58(4): 385-399.
[3] LIU Jie, XU Le, SHI Chao, YANG Shaopeng, HE Xiaofei, WANG Maoqiu, SHI Jie. Effect of Rare Earth Ce on Sulfide Characteristics and Microstructure in Non-Quenched and Tempered Steel[J]. 金属学报, 2022, 58(3): 365-374.
[4] DING Ning, WANG Yunfeng, LIU Ke, ZHU Xunming, LI Shubo, DU Wenbo. Microstructure, Texture, and Mechanical Properties of Mg-8Gd-1Er-0.5Zr Alloy by Multi-Directional Forging at High Strain Rate[J]. 金属学报, 2021, 57(8): 1000-1008.
[5] LI Xiucheng,SUN Mingyu,ZHAO Jingxiao,WANG Xuelin,SHANG Chengjia. Quantitative Crystallographic Characterization of Boundaries in Ferrite-Bainite/Martensite Dual-Phase Steels[J]. 金属学报, 2020, 56(4): 653-660.
[6] WU Huajian, CHENG Renshan, LI Jingren, XIE Dongsheng, SONG Kai, PAN Hucheng, QIN Gaowu. Effect of Al Content on Microstructure and Mechanical Properties of Mg-Sn-Ca Alloy[J]. 金属学报, 2020, 56(10): 1423-1432.
[7] ZHANG Jun,JIE Ziqi,HUANG Taiwen,YANG Wenchao,LIU Lin,FU Hengzhi. Research and Development of Equiaxed Grain Solidification and Forming Technology for Nickel-Based Cast Superalloys[J]. 金属学报, 2019, 55(9): 1145-1159.
[8] Liping DENG,Kaixuan CUI,Bingshu WANG,Hongliang XIANG,Qiang LI. Microstructure and Texture Evolution of AZ31 Mg Alloy Processed by Multi-Pass Compressing Under Room Temperature[J]. 金属学报, 2019, 55(8): 976-986.
[9] Shubo LI, Wenbo DU, Xudong WANG, Ke LIU, Zhaohui WANG. Effect of Zr Addition on the Grain Refinement Mechanism of Mg-Gd-Er Alloys[J]. 金属学报, 2018, 54(6): 911-917.
[10] Yizhe MAO, Jianguo LI, Lei FENG. Effect of Coarse β(Al3Mg2) Phase on Microstructure Evolution in 573 K Annealed Al-10Mg Alloy by Uniaxial Compression[J]. 金属学报, 2018, 54(10): 1451-1460.
[11] Lili ZHANG, Hongxiang JIANG, Jiuzhou ZHAO, Lu LI, Qian SUN. A New Understanding Toward Effect of Solute Ti on Grain Refinement of Aluminum by Al-Ti-B Master Alloy: Kinetic Behaviors of TiB2 Particles and Effect of Solute Ti[J]. 金属学报, 2017, 53(9): 1091-1100.
[12] Zhiqiang ZHANG,Limin DONG,Shaoxuan GUAN,Rui YANG. Microstructure and Mechanical Properties of TC16 Titanium Alloy by Room Temperature Roller Die Drawing[J]. 金属学报, 2017, 53(4): 415-422.
[13] Ning LI,Rong ZHANG,Limin ZHANG,Hui XING,Pengfei YIN,Yaoyan WU. Study on Grain Refinement Mechanism of Hypoeutectic Al-7%Si Alloy Under Low Voltage Alternating Current Pulse[J]. 金属学报, 2017, 53(2): 192-200.
[14] Jinrong ZUO,Longgang HOU,Jintao SHI,Hua CUI,Linzhong ZHUANG,Jishan ZHANG. PRECIPITATES AND THE EVOLUTION OF GRAIN STRUCTURES DURING DOUBLE-STEP ROLLING OF HIGH-STRENGTH ALUMINUM ALLOYAND RELATED PROPERTIES[J]. 金属学报, 2016, 52(9): 1105-1114.
[15] Yuefei TENG,Yingju LI,Xiaohui FENG,Yuansheng YANG. EFFECT OF RECTANGLE ASPECT RATIO ON GRAIN REFINEMENT OF SUPERALLOY K4169 UNDER PULSED MAGNETIC FIELD[J]. 金属学报, 2015, 51(7): 844-852.
No Suggested Reading articles found!