Abstract  Cyclic stress-strain responses and dislocation structures of copper sin-gle crystals with various tensile axes were systematically studied and comparedwith each other. Experimental results reveal that the evolution of microscopicdislocation configurations in a crystal and, accordingly, its macroscopic cyclicbehaviours are closely related with its orientation. Remarkable secondary slip hasbeen observed in some crystals with orientations well inside the ciystallographictriangle, which are usually considered as single-slip ones. Their cyclic behavioursand dislocation structures at saturation are similar to those of their neighbouringmulti-slip crystals. These results have constructed the experimental basis for thenewly proposed dislocation interaction model for cyclic deformation of fcc crystals,which will be described in the second part of this article.
Key words:  copper      single crystal orientation      cyclic deformation      dislocation configuration      multi-slip     
Received:  18 May 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/299

1 Lukas P, Klesnil M, Krejci J. Phys Status Solidi, 1968; 27: 545
2 Basinski S J. Basinski Z S, Howie A. Philos Mag. 1969; 19: 899
3 Woods P J. Philos Mag, 1973; 28: 155
4 Winter A T. Philos Mag. 1974; 30: 719
5 Finney J M, Laird C. Philos Mag, 1975; 81: 339
6 Mughrabi H. Mater Sci Eng, 1978; 33: 207
7 Basinski Z S, Korbel A S, Basinski S J. Acta Metall, 1980; 28: 191
8 Laird C. Finney J M, Kuhlmann-Wilsdorf D. Mater Sci Eng, 1981; 50: 127
9 Jin N Y (金能韫). Ph. D. Thesis, Cambridge University, U. K., 1983
10 Wang R (王仁卉), Mughrabi H. Mater Sci Eng. 1984; 63: 147
11 Brown L M. In: Ashby M F et al eds., Dislocation Modelling of Physical Systems, Gainesville, Florida, USA, June 22-27. 1980, Oxford: Pergamonpress. 1981: 51
12 Lepisto T, Kuokkala V-T, Kettunen P. Scr Metall, 1984; 18: 715
13 Ackermann F. Kubin L P. Lepinoux J, Mughrabi H. Acta Metall. 1984; 32: 715.
14 Cheng A S, Laird C. Mater Sci Eng, 1981; 51: 111
15 Jin N Y, (金能韫), Winter A T. Acta Metall, 1984; 32: 989
16 Jin N Y (金能韫), Winter A T. Acta Metall, 1984; 32: 1173
17 Jin N Y (金能韫). Philos Mag Letters, 1987; 56: 2
[1] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[2] CHEN Kaixuan, LI Zongxuan, WANG Zidong, Demange Gilles, CHEN Xiaohua, ZHANG Jiawei, WU Xuehua, Zapolsky Helena. Morphological Evolution of Fe-Rich Precipitates in a Cu-2.0Fe Alloy During Isothermal Treatment[J]. 金属学报, 2023, 59(12): 1665-1674.
[3] ZHAO Naiqin, GUO Siyuan, ZHANG Xiang, HE Chunnian, SHI Chunsheng. Progress on Graphene/Copper Composites Focusing on Reinforcement Configuration Design: A Review[J]. 金属学报, 2021, 57(9): 1087-1106.
[4] PENG Wuqingliang, LI Qiang, CHANG Yongqin, WANG Wanjing, CHEN Zhen, XIE Chunyi, WANG Jichao, GENG Xiang, HUANG Lingming, ZHOU Haishan, LUO Guangnan. A Review on the Development of the Heat Sink of the Fusion Reactor Divertor[J]. 金属学报, 2021, 57(7): 831-844.
[5] HUANG Songpeng, PENG Can, CAO Gongwang, WANG Zhenyao. Corrosion Behavior of Copper-Nickel Alloys Protected by BTA in Simulated Urban Atmosphere[J]. 金属学报, 2021, 57(3): 317-326.
[6] CHEN Lei, HAO Shuo, ZOU Zongyuan, HAN Shuting, ZHANG Rongqiang, GUO Baofeng. Mechanical Characteristics of TRIP-Assisted Duplex Stainless Steel Fe-19.6Cr-2Ni-2.9Mn-1.6Si During Cyclic Deformation[J]. 金属学报, 2019, 55(12): 1495-1502.
[7] Jianqiang REN, Shuhua LIANG, Yihui JIANG, Xiang DU. Research on the Microstructure and Properties of In Situ (TiB2-TiB)/Cu Composites[J]. 金属学报, 2019, 55(1): 126-132.
[8] Pengyue ZHAO, Yongbo GUO, Qingshun BAI, Feihu ZHANG. Research of Surface Defects of Polycrystalline Copper Nanoindentation Based on Microstructures[J]. 金属学报, 2018, 54(7): 1051-1058.
[9] Tingting ZHAO, Zhixin KANG, Xiayu MA. Fabricating Superhydrophobic Copper Meshes by One-Step Electrodeposition Method and Its Anti-Corrosion and Oil-Water Separation Abilities[J]. 金属学报, 2018, 54(1): 109-117.
[10] Tingbiao GUO, Qi LI, Chen WANG, Feng ZHANG, Zhi JIA. Deformation Characteristics and Mechanical Properties of Single Crystal Copper During Equal Channel Angular Pressing by Route A[J]. 金属学报, 2017, 53(8): 991-1000.
[11] Wei FU,Xiaoguo SONG,Long LONG,Jianhang CHAI,Jicai FENG,Guodong WANG. INTERFACIAL MICROSTRUCTURE AND MECHANI-CAL PROPERTIES OF INDIRECT BRAZED GRAPHITE/COPPER JOINT[J]. 金属学报, 2016, 52(6): 734-740.
[12] Kan SONG,Kai YU,Xin LIN,Jing CHEN,Haiou YANG,Weidong HUANG. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF HEAT TREATMENT LASER SOLID FORMING SUPERALLOY INCONEL 718[J]. 金属学报, 2015, 51(8): 935-942.
[13] Zhisheng WANG, Xiang CHEN, Yanxiang LI, Huawei ZHANG, Yuan LIU. EFFECTS OF B ON HIGH TEMPERATURE MECHA-NICAL PROPERTIES AND THERMAL FATIGUE BEHAVIOR OF COPPER DIE-CASTING DIE STEEL[J]. 金属学报, 2015, 51(5): 519-526.
[14] CHE Xin, LIANG Xingkui, CHEN Lili, CHEN Lijia, LI Feng. MICROSTRUCTURES AND LOW-CYCLE FATIGUE BEHAVIOR OF Al-9.0%Si-4.0%Cu-0.4%Mg(-0.3%Sc) ALLOY[J]. 金属学报, 2014, 50(9): 1046-1054.
[15] ZHUO Weijia, LIU Yuan, LI Yanxiang. EFFECT OF WITHDRAWING RATE ON PORE MORPHOLOGY OF LOTUS-TYPE POROUS COPPER PRODUCED BY SINGLE-MOLD GASAR TECHNIQUE[J]. 金属学报, 2014, 50(8): 921-929.
No Suggested Reading articles found!