Abstract  Ca-O equilibria in liquid Fe and Fe-C (C≤0.83 wt-%) have beendetermined by means of Ca vapor method in a sealed Mo chamber. The differenceof the equilibrium constants between them are quite small. Following results wereobtained for Fe-Ca-O system at 1600℃:K_(Ca-O)=4.3×10~(-8), e_O~(Ca)=-178
Key words:  calcium      oxygen      molten iron      equilibrium constent      interaction coefficient     
Received:  18 January 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I1/77

1 小林三郎,大森康男,三本木贡治.铁钢,1970; 56:998
2 宫下芳雄,西川胜彦.铁钢,1971;57:1969
3 音谷登平,形浦安治,出川通,铁钢,1975;61:2167
4 Gustafsson S, Li Y. In: doctor Dissertation (by Gustafsson), Roy inst of Techn, Stockholm, Sweden, 1982, To be Published
5 Gustafsson S, Mellberg P O. Scand J Metall. 1980; 9: 111
6 Sigworth G K, Elliott J F. Met Sci, 1974; 8: 298
7 Han Qiyong, Chen Dong, Wang Pengfei, Zhang Xiaodong. Proc 4th Japan-China Symp on Sci and Tech of Iron and Steel, Kobe, Japan, Nov. 26--27, 1987: 157--66
8 小沢.日本学术振与会第19委员会,No.9837,1975年6月
9 Janke D. Fundamental Aspects of Calcium Treatment of Steel, (待发表)
10 铃木健一郎,江岛彬夫,仲村秀夫,三本木贡治.铁钢.1977;63(11) :S585
[1] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[2] CAO Shuting, ZHANG Shaohua, ZHANG Jian. Combustion Behavior of GH4061 Alloy in High Pressure and Oxygen-Enriched Atmosphere[J]. 金属学报, 2023, 59(4): 547-555.
[3] LIAO Jingjing, ZHANG Wei, ZHANG Junsong, WU Jun, YANG Zhongbo, PENG Qian, QIU Shaoyu. Periodic Densification-Transition Behavior of Zr-Sn-Nb-Fe-V Alloys During Uniform Corrosion in Superheated Steam[J]. 金属学报, 2023, 59(2): 289-296.
[4] JU Tianhua, SHU Nian, HE Wei, DING Xueyong. A Predicted Model for Activity Interaction Coefficient Between Solutes in Alloy Solutions[J]. 金属学报, 2023, 59(11): 1533-1540.
[5] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[6] Xiaohua MIN, Li XIANG, Mingjia LI, Kai YAO, Satoshi EMURA, Congqian CHENG, Koichi TSUCHIYA. Effect of {332}<113> Twins Combined with Isothermal ω-Phase on Mechanical Properties in Ti-15Mo Alloy with Different Oxygen Contents[J]. 金属学报, 2018, 54(9): 1262-1272.
[7] Shuaipeng WANG, Wenhua LUO, Gan LI, Haibo LI, Guangfeng ZHANG. Effect of La Content on Hydriding Kinetics of Ce-La Alloys[J]. 金属学报, 2018, 54(8): 1187-1192.
[8] Shizheng ZHANG,Yaohui XU,Tingyu WANG,Ruixing LI,Hongnian CAI. SOLID SOLUBILITY AND OXYGEN STORAGE CAPABILITY OF In3+-DOPED CeO2[J]. 金属学报, 2016, 52(5): 607-613.
[9] Tianguo WEI,Jiankang LIN,Chongsheng LONG,Hongsheng CHEN. EFFECT OF DISSOLVED OXYGEN IN STEAM ON THE CORROSION BEHAVIORS OF ZIRCONIUM ALLOYS[J]. 金属学报, 2016, 52(2): 209-216.
[10] Shengbo CEN,Hui CHEN,Yan LIU,Yuanming MA,Ying WU. EFFECT OF CeO2 ON CORROSION BEHAVIOR OF WC-12Co COATINGS BY HIGH VELOCITY OXYGEN FUEL[J]. 金属学报, 2016, 52(11): 1441-1448.
[11] Chuan HONG,Yunming GAO,Chuanghuang YANG,Zhibo TONG. ELECTROCHEMICAL BEHAVIOR OF Ni2+ IN SiO2-CaO-MgO-Al2O3 MOLTEN SLAG AT 1673 K[J]. 金属学报, 2015, 51(8): 1001-1009.
[12] ZHONG Xiaocong, JIANG Liangxing, LÜ Xiaojun, LAI Yanqing, LI Jie, LIU Yexiang. EFFECTS OF CHLORIDE ION ON THE ELECTRO- CHEMICAL BEHAVIOR OF Pb-Ag-RE ALLOY ANODE[J]. 金属学报, 2015, 51(3): 378-384.
[13] WANG Yong, ZHENG Yugui, WANG Jianqiang, LI Meiling, SHEN Jun. PASSIVATION BEHAVIOR OF Fe-BASED AMORPHOUS METALLIC COATING IN NaCl AND H2SO4 SOLUTIONS[J]. 金属学报, 2015, 51(1): 49-56.
[14] ZHANG Zhiming, WANG Jianqiu, HAN En-Hou, KE Wei. ANALYSIS OF SURFACE OXIDE FILM FORMED ON ELETROPOLISHED ALLOY 690TT IN HIGH TEMPERATURE AND HIGH PRESSURE WATER WITH SEQUENTIALLY DISSOLVED HYDROGEN AND OXYGEN[J]. 金属学报, 2015, 51(1): 85-92.
[15] YU Qiaohong, LIU Chao, PANG Xiaolu, LIU Quanlin, GAO Kewei. CREVICE CORROSION BEHAVIORS OF Q235 WELD JOINT[J]. 金属学报, 2014, 50(11): 1319-1326.
No Suggested Reading articles found!