| INITIAL COMPOSITION TRANSIENT DURING CRYSTAL GROWTH |
| LI Yanxiang;LIU Baicheng Department of Mechanical Engineering; Tsinghua University; Beijing |
|
Cite this article:
LI Yanxiang;LIU Baicheng Department of Mechanical Engineering; Tsinghua University; Beijing. INITIAL COMPOSITION TRANSIENT DURING CRYSTAL GROWTH. Acta Metall Sin, 1988, 24(1): 82-86.
|
|
|
Abstract The solute distribution in the initial transient during unidirectionalplanar crystal growth has been studied. An expression of solute distributionin liquid phase near liquid-solid interface at the initial growth stage was derived.A method for reducing the length of initial transient was put forward and theshortest initial transient length was determined. The growth velocity function re-quired for realizing the shortest transient length at the initial stage was then ob-tained.
|
|
Received: 18 January 1988
|
1 Tiller W A, Jackson K A, Rutter J W, Chalmers B. Acta Metall, 1953; 1: 428 2 闵乃本.晶体生长的物理基础,上海科学技术出版社,1982:58 3 Pohl R G. J Appl Phys, 1954; 23: 1170 4 Flemings M C. Solidification Processing, New York: McGraw-Hill, 1974: 4 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|