PHASE BOUNDARIES OF SINGLE-PHASE ε-AND γ′-FIELDS IN Fe-C-N PHASE DIAGRAM
XU Zuyao (T. Y. Hsu);LI Lin Professor Department of Materials Science and Engtneering Shanghai Jiaotong University; Shandong polytechnic University
Cite this article: 

XU Zuyao (T. Y. Hsu);LI Lin Professor Department of Materials Science and Engtneering Shanghai Jiaotong University; Shandong polytechnic University. PHASE BOUNDARIES OF SINGLE-PHASE ε-AND γ′-FIELDS IN Fe-C-N PHASE DIAGRAM. Acta Metall Sin, 1988, 24(1): 71-76.

Download:  PDF(385KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The activity of N in α-Fe was derived from the solubility data at580℃ in the Fe-N diagram. The interaction coefficients of Fe-N, Fe-C and C-Nwere obtained and the phase boundaries of single-phase ε-and γ_1-fields were subse-quently calculated. The results show that the γ_1-region of Naumann and LangescheidFe-C-N ternary phase diagram is correct, but the ε-region requires revision. Calcu-lation give an evidence that most of the experimental data on the ε-phase report-ed by Wells and Bell appears reasonable. Calculations taking graphite as a standaredstate confirms the above conclusions.
Key words:  phase diagram calculation      phase diagram of Fe-C-N     
Received:  18 January 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I1/71

1 Naumann F K, Langenscheid G A. Arch Eisenhuettenwesen, 1965; 36: 677
2 Raghavan V. Trans Indian Inst Met, 1984; 37(4) : 293
3 Wells A, Bell T. Heat Treat Met, 1983; 10: 39
4 Elliott J F, Gleiser M, Ramarkrishna V. In: Elliott J F, Gleiser M eds., Thermochemistry for Steelmaking, London: Addison-Wesley Publishing Co. Inc. 1963: 405
5 Darken L S, Gurry R W. Physical Chemistry of Metals, McGraw-Hill, 1953: 379
6 Reed T B. Free Energy of Formation of Binary Compounds, MIT Press, 1971: 26
7 Dew-Hughes D, Kaufman L. CALPHAD. 1979; 3: 175
8 冯端,王业宁,邱第荣.金属物理,上册,科学出版社,1964:69
9 Kaufman L.CALPHAD,1978;2:295
10 徐祖耀.金属材料热力学,科学出版社,1981:254
11 范鸣玉,张莹.最优化技术基础,清华大学出版社,1982:164B
[1] ZHANG Weibin SHA Chunsheng DU Yong WEN Guanghua XIE Wen WANG Shequan. COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. 金属学报, 2011, 47(10): 1307-1314.
No Suggested Reading articles found!