| PREPARATION OF COMPOSITE COATING (Al+Al2O3) ON SiC LONG FIBER |
| ZHANG Lu, SHI Nanlin, GONG Jun, PEI Zhiliang, GAO Lijun, SUN Chao |
| Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
|
Cite this article:
ZHANG Lu SHI Nanlin GONG Jun PEI Zhiliang GAO Lijun SUN Chao. PREPARATION OF COMPOSITE COATING (Al+Al2O3) ON SiC LONG FIBER. Acta Metall Sin, 2011, 47(4): 497-501.
|
|
|
Abstract Reactive magnetron sputtering was used to prepare (Al+Al2O3) diffusion barrier layer on SiC fiber surface. The relationships between deposition process parameters with composition and deposition rate of the coating, and the influence of the coating on mechanical property of SiC fiber were measured. Results show that with increasing sputtering power, the deposition rate increases rapidly at first and then slowly. With increasing of working pressure, the deposition rate of the coating deceases slowly at first, and then sharply at a typical value of working pressure, finally drops gradually. (Al+Al2O3) protected C-rich layer of SiC fiber, and improved the adherence between fiber and diffusion barrier layer. Results of laser Raman spectrum show that the coating has little influence on surface residual stress of SiC fiber. The measured tensile strength of the composite fibers is 97.69% of the calculated tensile strength according to meaning rule, and is 98.77% of the calculated one for the fiber after vacuum treatment at 850 ℃ for 10 h, meaning that (Al+Al$_{2}$O$_{3}$) coating has not much influence on mechanical property of SiC fiber.
|
|
Received: 31 December 2010
|
| [1] Mileiko S T, Kiiko V M, Kolchin A A, Serebryakov A V, Korzhov V P, Starostin M Y, Sarkissyan N S. Compos Sci Technol, 2002; 62: 167[2] Yu Y X, Cao F, Li X D. Acta Mater Compos Sin, 2004; 21(5): 79(余煜玺, 曹峰, 李效东. 复合材料学报, 2004; 21(5): 79)[3] Schiepers R C J, Van Loo F J J, De With G. J Am Ceram Soc, 1988; 71: 284[4] Tang W M, Zheng Z X, Ding H F, Jin Z H. J Chin Ceram Soc, 2003; 31: 283(汤文明, 郑治祥, 丁厚福, 金志浩. 硅酸盐学报, 2003; 31: 283)[5] Wang Y Q, Zhou B L. Composites, 1996; 27A: 1139[6] Lin H T, Shi N L, Sun C, Gong J, Sun X D. Acta Metall Sin, 2007; 4: 444(林海涛, 石南林, 孙 超, 宫骏, 孙旭东. 金属学报, 2007; 4: 444)[7] King D E, Swartz W E Jr. J Chem Educ, 1987; 64: 981[8] Carney T J, Tsakiropoulos P, Watts J F, Castle J E. Int J Rapid Sol, 1990; 5: 189[9] Paparazzo E. Appl Surf Sci, 1986; 25: 1[10] Olefjord I, Mathieu H J, Marcus P. Surf Interface Anal, 1990; 15: 681[11] Kishi K, Ikeda S. Bull Chem Soc Jpn, 1973; 46: 341[12] Turner N H, Single A M. Surf Interface Anal, 1990; 15: 215[13] Rastogi R S, Pourrezaei K. J Mater Process Technol, 1994; 43: 89[14] Han Y W, Li D M, Zhao Z C, Yan G Y. Thin Film Sci Technol, 1990; 3(2): 20(韩耀文, 李大明, 赵志成, 燕广远. 薄膜科学与技术, 1990; 3(2): 20)[15] Liu G X, Jin Z Z,Wang Y J. Mater Sci Prog, 1991; 5: 498(刘桂新, 金宗哲, 王延籍. 材料科学进展, 1991; 5: 498)[16] Zhu W L, Zhu J L, Nishino S, Pezzotti G. Appl Surf Sci, 2006; 252: 2346[17] Shackelford J F, Alexander W. CRC Materials Science and Engineering Handbook. 3rd ed. Florida: CRC press, 2001: 406 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|