| The Effect of Cumulative Deformation on the Recrystallization Mechanisms of F316 Austenitic Stainless Steel |
LIU Zhonghan 1, CHEN Dongze 1, FENG Wei 1, HOU
Jixin 1, YU Yunhe 1, GU Chungang 2, GAO Jianfei 2, XIA
Zhixin 1
|
1 Shagang
School of Iron and Steel, Soochow University, Suzhou 215137, China
2 SUFA
Technology Industrial Co. Ltd., CNNC, Suzhou 215129, China
|
|
Cite this article:
. The Effect of Cumulative Deformation on the Recrystallization Mechanisms of F316 Austenitic Stainless Steel. Acta Metall Sin, 0, (): 0-0.
|
|
|
Abstract
The
forming of large and complex forgings typically relies on multistep cumulative
deformation processes that optimize microstructures and improve mechanical
properties. However, the mechanisms of the recrystallization that occurs during
these processes are not fully understood. This study examines the effects of deformation temperature, strain rate,
inter-pass holding time, and deformation distribution on the dynamic
recrystallization (DRX), static recrystallization (SRX), and metadynamic
recrystallization (MDRX) behaviors of F316 austenitic stainless steel. With a
combination of thermal simulation experiments and EBSD techniques, the
evolution of the geometrically necessary dislocation (GND) density, grain boundary
characteristics, and grain orientation under various deformation conditions was
comprehensively analyzed. Increasing the deformation temperature and decreasing
the strain rate facilitate DRX occurrence by reducing the critical energy.
Prolonged holding time results in excessive SRX and MDRX, which depletes the
stored deformation energy and hinders subsequent DRX. When the initial
deformation amount is large, sufficient MDRX tends to suppress DRX activity.
When the initial deformation amount is small, SRX contributes additional
nucleation sites. Increasing the final pass deformation amount tends to
promote DRX occurrence by preventing MDRX. Further
analysis indicates that although SRX consumes part of the deformation energy,
the effect of its grain refinement provides a greater number of nucleation
sites for subsequent DRX. MDRX is a process of grain growth that proceeds
directly from DRX grains and that consumes deformation energy, thereby
suppressing subsequent DRX and potentially resulting in a mixed grain structure
that would adversely affect the material’s final microstructure and properties.
An accumulated deformation energy model for F316 stainless steel is established
to evaluate the effects of various recrystallization processes. This model calculates
the energy consumption of SRX and MDRX during hot deformation, determines the
critical energy required for DRX in subsequent passes, and quantifies the
specific contributions to DRX from SRX and MDRX. The findings provide
theoretical support for the microstructural control and performance
optimization of large forgings, thereby offering practical guidance for
optimizing forging processes, especially under high-temperature and
high-strain-rate conditions.
|
|
Received: 27 December 2024
|
|
|
| Fund: National Basic Research Program of China;National Natural Science Foundation of China;National Natural Science Foundation of China |