| 金属液体凝固中直接挤压过程的数值模拟 |
| 任向前;李贺军 |
| 武汉交通科技大学;西北工业大学 |
|
| NUMERICAL SIMULATION OF DIRECT EXTRUSION PROCESS APPLIED TO LIQUID METAL DURING SOLIDIFICATION |
| REN Xiangqian(Wuhan Transportation University; Wuhan 430063); LI Hejun (Northwestern Polytechnical University; Xi'an 710072)(Manuscript received 1995-09-20) |
引用本文:
任向前;李贺军. 金属液体凝固中直接挤压过程的数值模拟[J]. 金属学报, 1996, 32(7): 755-762.
,
.
NUMERICAL SIMULATION OF DIRECT EXTRUSION PROCESS APPLIED TO LIQUID METAL DURING SOLIDIFICATION[J]. Acta Metall Sin, 1996, 32(7): 755-762.