| DZ40M钴基高温合金950℃长期时效后的组织与性能 |
| 姜文辉;姚向东;管恒荣;胡壮麒 |
| 中国科学院金属研究所;沈阳;110015;沈阳工业大学;沈阳;110023;中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015 |
|
| MICROSTRUCTURES AND PROPERTIES OF DZ40M Co-BASE SUPERALLOY AFTER LONG-TERM AGEING AT 950℃ |
| JIANG Wenhuil; YAO Xiangdong; GUAN Hengrong;HU Zhuangqi(Institute of Metal research; The Chinese Academy of Sciences; Shenyang 11O015)(Shenyang Polytechnic University; Shenyang 110023)Correspondent:JIANG Wenhui; Tel: (0U)2384353l-556o8; Fax: (024)23891320Manuscript received 1997-12-16; in revised form 1998-03-10 |
引用本文:
姜文辉;姚向东;管恒荣;胡壮麒. DZ40M钴基高温合金950℃长期时效后的组织与性能[J]. 金属学报, 1998, 34(12): 1289-1294.
,
,
,
.
MICROSTRUCTURES AND PROPERTIES OF DZ40M Co-BASE SUPERALLOY AFTER LONG-TERM AGEING AT 950℃[J]. Acta Metall Sin, 1998, 34(12): 1289-1294.
1管恒荣,姚向东,张静华,张志亚,李英敖,胡壮麒.金属学报,1995;31(Suppl).):308(Guan H G, YaO X D, Zhang J H, Zhang Z Y, Li Y G, Hu Z Q. Acta Metall sin ,1995; 31(Suppl.): 308 2姚向东,张静华,张志亚,李英敖,赵乃仁,管恒荣,胡壮麒.金属学报,1995;31:A32. (Yao X D,Zhang J H,Zhang Z y,Li Y G,ZHao N R,Guan H R,Hu Z Q.Acta Metall Sin.1995;31:A320) 3 Tawancy H M,J Mater Sci, 1983; 18: 2976 4 Vandenousen R F,Viatour P.Drapier J M.Coutsouradis D.Cobalt.1974;(1):6 5 Sims C T.In:sims C T.Hagel W C eds.The Superalloys.New York:John Wiley & Sons Inc,1972:154 6 Lane J R and Grant N J. 7YYI。 ASM, 1952; 44: 113 7姚向东,张静华,张志亚,李英敖,管恒荣,胡壮麒.金属学报,1995;31(suppl):304(YaO X D, Zhang J H, Zhang Z Y, Li Y G, Guan H R, Hu Z Q. Acta Metall Sin, 1995; 31(Suppl.): 304) 8Hamar-Thibault S, Durand-Charre M, Andries B. Metall Trans ,1982; 13A: 545 |
|