| TiAl合金PST晶体高温蠕变特性及蠕变失稳机制 |
| 林建国;张永刚;陈昌麒 |
| 北京航空航天大学材料科学与工程系;北京;100083;北京航空航天大学材料科学与工程系;北京;100083;北京航空航天大学材料科学与工程系;北京;100083 |
|
| COMPRESSION CREEP BEHAVIOR AND INSTABILITY MECHANISM OF TiAl PST CRYSTALS AT HIGH TEMPERATURE |
| LIN Jianguo; ZHANG Yonggang; CHEN Changqi (Department of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083)Correspondent: Lin Jianguo; postdoctoral; Tel: (010)62017251-7809 |
引用本文:
林建国;张永刚;陈昌麒. TiAl合金PST晶体高温蠕变特性及蠕变失稳机制[J]. 金属学报, 1998, 34(9): 945-949.
,
,
.
COMPRESSION CREEP BEHAVIOR AND INSTABILITY MECHANISM OF TiAl PST CRYSTALS AT HIGH TEMPERATURE[J]. Acta Metall Sin, 1998, 34(9): 945-949.
1 Chesnutt J C. In:Antolovich S D,Stusrud R W , Mackay R A,Anton D L, Khan T, Kissinger R D. Klarstrom D L eds., Superulloys 1992, New York: The Minerals, Metals and Materials Society, 1992; 381 2 Beddoes J, Wallace W, Zhao L. Int Met Mater Rev, 1995; 40: 197 3 Zhang W J, Spigarelli S, Cerri E, Evangelister E, Franceconi L. Mater Sci Eng, 1996; A211: 15 4 Inui H, Oh M H, Nakamura A, Yamaguchi M. Acta Metall Mater, 1992; 27: 1253 5 FujiwaraT;Nakamura A,HosomiM,Nishtani S R,Shira Y,Yamaguchi M. Philos Mag A, 1990;61:591 6 Minonishi Y, OtsukaM; TanakaK. In: Izumi ed.,Intermetallic Compounds. Sendai: The Japan Institute of Metals,1991:543 7 Verhoeven J D. Fundamentals of Phsysical Metallurgy. New York: John Wiley & Sons, 1975:204 |
|