| 板条马氏体钢的断裂韧性与缺口韧性、拉伸塑性的关系 |
| 梁益龙;雷旻;钟蜀辉;江山 |
| 贵州工业大学冶金系;贵阳;550003;贵州工业大学冶金系;贵阳;550003;贵州工业大学冶金系;贵阳;550003;贵州工业大学冶金系;贵阳;550003 |
|
| THE RELATIONSHIP BETWEEN FRACTURE TOUGHNESS AND NOTCH TOUGHNESS, TENSILE DUCTILITIES IN LATH MARTENSITE STEEL |
| LIANG Yilong; LEI Min; ZHONG Shuhui; JIANG Shan (Guizhou University of Technology; Guiyang 550003)Correspondent: LIANG Yilong; associate professor; Tel. (0851)4818011; Fax: (0851)4818381 |
引用本文:
梁益龙;雷旻;钟蜀辉;江山. 板条马氏体钢的断裂韧性与缺口韧性、拉伸塑性的关系[J]. 金属学报, 1998, 34(9): 950-958.
,
,
,
.
THE RELATIONSHIP BETWEEN FRACTURE TOUGHNESS AND NOTCH TOUGHNESS, TENSILE DUCTILITIES IN LATH MARTENSITE STEEL[J]. Acta Metall Sin, 1998, 34(9): 950-958.
1 Zackay V F, Parker E R, Goolsby R D, Wood W E. NaturePhys Sci, 1972; 236: 108 2 Rao B V N, Thomas G Metall Trans, 1980; 11A: 441 3 Youngblood J L;Raghavan M. Metall Trans,1977; 8A: 1439 4 石德珂.熊漪.西安交通大学学报,1989;23(Sup2):194(Shi D K,Xiong Y. J Xian Jiaotong Univ, 1989;23(Sup2):194) 5 Lai G Y, Wood W E, Clark R A, Zackay V F, Parker E R. Metall Trans, 1974; 5: 1663 6 Ritchie R O; Francis B, Server W L. Metall Trans,1976 7A: 831 7 Ritchie R O, Horn R M. Metall Trans, 1978; 9A: 331 8 Lee S, Majno L, Asaro R J. Metall Trans, 1985; 16A: 1633 9 邓增杰,周敬恩.工程材料的断裂与疲劳北京:机械工业出版社,1995:32,22(Deng Z J,Zhou J E. Fracture and Fatigue of Engineering Materials. Beijing: Chinese Press of Mechanical Industry; 1995: 32,22) 10 Mackenzie A C, Hancock J W; Brown D K. Eng FracMech, 1977 9: 167 11 梁益龙,雷,谢源章,刘其斌,张德恩.理化检验(物理分册)1993; 29(10):11(Liang Y L, Lei M, Xie Y Z; Liu Q B, Zhang D E. Phys Test Chem Anal, Part A: Phys Test. 1993; 29: 11) 12 Sarikkaya M, Jhingan A K, Thomas G. Metall Trans, 1983; 14A: 1121 13 McMeeking R M. J Mech Phys Solids, 1977 25: 357 14 林吉忠,刘淑华.金属材料的断裂与疲劳北京:中国铁道出版社,1989:156(Lin J Z,Liu SH. Fracture and Fatigue of Metal Materials. Beijing: Chinese Press of Railway, 1989:156) 15 刘禹门.机械工程学报,1985; 21:27(Liu Y M.Chinese Journal of Mechanical Engineering , 1985; 21: 27) 16 Cao Weidi, Lu Xiaoping. Metall Trans, 1987 18A: 1569 17 Handerhan K J,Garrison W M.Metall Trans,1988;19A:2989 18 McDarmaid D S. Met Technol, 1980; 7: 372 |
|