ZA62镁合金中AB2型金属间化合物的结构稳定性与弹性性能的第一原理计算
周惦武1); 徐少华2); 张福全2); 彭平2); 刘金水2)
1 湖南大学汽车车身先进设计制造国家重点实验室; 长沙 410082 2 湖南大学材料科学与工程学院; 长沙410082
FIRST-PRINCIPLES CALCULATIONS OF STRUCTURAL STABILITIES AND ELASTIC PROPERTIES OF AB2 TYPE INTERMETALLICS IN ZA62 MAGNESIUM ALLOY
ZHOU Dianwu1); XU Shaohua2); ZHANG Fuquan2); PENG Ping2); LIU Jinshui2)
1 State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body; Hunan University; Changsha 410082 2 School of Materials Science and Engineering; Hunan University; Changsha 410082
引用本文:

周惦武 徐少华 张福全 彭平 刘金水. ZA62镁合金中AB2型金属间化合物的结构稳定性与弹性性能的第一原理计算[J]. 金属学报, 2010, 46(1): 97-103.
. FIRST-PRINCIPLES CALCULATIONS OF STRUCTURAL STABILITIES AND ELASTIC PROPERTIES OF AB2 TYPE INTERMETALLICS IN ZA62 MAGNESIUM ALLOY[J]. Acta Metall Sin, 2010, 46(1): 97-103.

全文: PDF(982 KB)  
摘要: 

采用基于密度泛函理论Castep和Dmol程序软件包, 计算了ZA62镁合金中AB2型金属间化合物 MgZn2, Mg2Sn和MgCu2的结构稳定性、弹性性能与电子结构. 合金形成热和结合能的计算结果显示:  Mg2Sn具有最强的合金化形成能力, 而MgCu2结构最稳定; 体模量(B)、弹性各向异性系数(A)、Young's模量(E)、剪切模量(G)和Poisson比(ν)的计算结果表明: MgZn2和MgCu2为延性相, 而Mg2Sn为脆性相, MgZn2的塑性最好; 采用弹性常数、体模量和结合能的经验公式计算金属间化合物的熔点, 实验值均在采用弹性常数(±300 K)和体模量(±500 K)计算熔点预测的范围内, 采用弹性常数比采用体模量和结合能预测熔点的平均相对误差小, 其中采用弹性常数计算Mg2Sn的熔点与对应的实验值十分接近, 相对误差仅为0.31%. 不同温度下热力学性质的计算结果表明, 在298-573 K温度范围内, MgCu2的Gibbs自由能始终最小, 其结构热稳定性最好, 结构稳定性的强弱顺序并不随温度的升高而消失; 而对MgZn2和Mg2Sn, 以475 K为临界, 结构稳定性的强弱顺序随温度的升高发生了变化; 态密度和Mulliken电子占据数的计算结果表明: MgCu2 结构最稳定的原因主要在于体系在Fermi能级以下区域成键电子存在强烈的离子键作用.

关键词 镁合金金属间化合物电子结构结构稳定性弹性性能    
Abstract

Structural stabilities, elastic properties and electronic structures of Mg2Sn, MgZn2 and MgCu2 in ZA62 magnesium alloy have been determined from first-principles calculations by using Castep and Dmol program based on the density functional theory. The calculated heats of formation and cohesive energies showed that Mg2 Sn has the strongest alloying ability and MgCu2 the highest structural stability. The calculated bulk moduli (B), anisotropy values (A), Young's moduli (E), shear moduli (G) and Poisson ratio (ν) showed that MgZn2 and MgCu2 both are ductile, on the contrary, Mg2 Sn is brittle, and among the three phases MgZn2 is a phase with the best plasticity. Their tested melting temperatures are within the ranges calculated from elastic constants (±300 K) and bulk moduli (±500 K), the estimated values from elastic constant have the smallest average relative error, the calculated melting temperature of Mg2Sn phase is in well agreement with the experimental one and the error relative to the experiment result is about 0.31%. MgCu2 has higher melting temperature, i.e. better structural stability among the three compounds. The calculations of thermodynamic properties show that the Gibbs free energy of MgCu2 is also the smallest within 298-573 K range, indicating the structural stability of MgCu2  does not change with the elevated temperature. The calculations of the density of states (DOS) and Mulliken electronic populations showed that the reason of MgCu2 having highest structural stability in ZA62 magnesium alloy attributes to MgCu2 phase having more ionic bonds below Fermi level compared with those of Mg2 Sn and MgZn2 phases.

Key wordsmagnesium alloy    intermetallics    electronic structure    structural stability    elastic property
收稿日期: 2009-07-01     
ZTFLH: 

TG146.2

 
基金资助:

教育部博士点专项科研(新教师)基金项目200805321032, 国家自然科学基金项目50771044, 湖南省自然科学基金项目09JJ6079,
教育部长江学者与创新团队发展计划项目531105050037, 以及湖南大学汽车车身先进设计制造国家重点实验室自主研究课题项目60870005资助

作者简介: 周惦武, 男, 1971年生, 副教授, 博士

[1] Li Z J, Gu X N, Lou S Q, Zheng Y F. Biomaterials, 2008; 29: 1329
[2] Sun Y S,Wen K Z, Yuan G Y. Chin Nonferrous Met, 1999; 9: 55
(孙扬善, 翁坤忠, 袁广银. 中国有色金属学报, 1999; 9: 55)
[3] Au–Yang M Y, Cohen M L. Phys Rev, 1969; 178: 1358
[4] Arunsingh, Dayal B. J Phys, 1970; 3C: 2037
[5] Imai Y, Watanabe A. Intermetallics, 2002; 10: 333
[6] Grosch G H, Range K J. J Alloys Compd, 1996; 235: 250
[7] Ghosh G, Vaynman S, Asta M, Fine M E. Intermetallics, 2007; 15: 44
[8] Fast L, Wills J M, Johansson B, Eriksson O. Phys Rev, 1995; 51B: 17431
[9] Segall M D, Lindan P L D, Probert M J, Pickard C J, Hasnip P J, Clark S J, Payne M C. J Phys: Condens Matter, 2002; 14: 2717
[10] Marlo M, Milman V. Phys Rev, 2000; 62B: 2899
[11] Vanderbilt D. Phys Rev, 1990; 41B: 7892
[12] Hammer B, Hansen L B, Norkov J K. Phys Rev, 1999; 59B: 7413
[13] Franscis G P, Payne M C. J Phys: Condens Matter, 1990; 2: 4395
[14] Monkhorst H J, Pack J D. Phys Rev, 1976; 13B: 5188
[15] Huang K. Solid State Physics. Beijing: High Education Press, 1985: 68
(黄昆. 固体物理学. 北京: 高等教育出版社, 1985: 68)

[16] Zhang H, Shang S L, Saal J E, Saengdeejing A, Wang Y, Chen L Q, Liu Z K. Intermetallics, 2009; 17: 878
[17] Ganeshan S, Shang S L, Wang Y, Mantina M, Liu Z K. Intermetallics, 2009; 17: 313
[18] Corkill J L, Cohen M L. Phys Rev, 1993; 48B: 17138
[19] Medvedeva M I, Gornostyrev Y N , Novikov D L, Mryasov V, Freeman A J. Acta Mater, 1998; 46: 3433
[20] Sahu B R. Mater Sci Eng, 1997; B49: 74
[21] Li C H, Hoe J L, Wu P. Phys Chem Solids, 2003; 64: 201
[22] Ansara I, Dinsdale A T, Rand M H. Thermodynamic Database for Light Metal Alloys. Brussels: European Commission, 1998: 368
[23] Zubov V I, Tretiakov N P, Teixeira R J N, Sanchez O J F. Phys Lett, 1995; 198A: 470
[24] Ishii Y, Fujiwara T. Non–Cryst Solids, 2002; 312–314: 494
[25] Davis L C, Whitten W B, Danielson G C. J Phys Chem Solids, 1967; 28: 439
[26] Cheng C H. J Phys Chem Solids, 1967; 28: 413
[27] YuWY, Wang N, Xiao X B, Tang B Y, Peng L M, Ding W J. Solid State Sci, 2009; 11: 1400
[28] Hong S Y, Fu C L. Intermetallics, 1999; 7: 5
[29] Mehl M J, Osburn J E, Papaconstantopoulos D A, Klein B M. Phys Rev, 1990; 41B: 10311
[30] Mattesini M, Ahuja R, Johansson B. Phys Rev, 2003; 68B: 184108
[31] Fine M E, Brown H L M. Scr Metall Mater, 1984; 18: 951
[32] Zhang X D. Intermetallics, 1995; 3: 137

[1] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[2] 邵晓宏, 彭珍珍, 靳千千, 马秀良. 镁合金LPSO/SFs结构间{10ˉ12}孪晶交汇机制的原子尺度研究[J]. 金属学报, 2023, 59(4): 556-566.
[3] 沈朝, 王志鹏, 胡波, 李德江, 曾小勤, 丁文江. 镁合金抗高温氧化机理研究进展[J]. 金属学报, 2023, 59(3): 371-386.
[4] 朱云鹏, 覃嘉宇, 王金辉, 马鸿斌, 金培鹏, 李培杰. 机械球磨结合粉末冶金制备AZ61超细晶镁合金的组织与性能[J]. 金属学报, 2023, 59(2): 257-266.
[5] 唐伟能, 莫宁, 侯娟. 增材制造镁合金技术现状与研究进展[J]. 金属学报, 2023, 59(2): 205-225.
[6] 彭立明, 邓庆琛, 吴玉娟, 付彭怀, 刘子翼, 武千业, 陈凯, 丁文江. 镁合金选区激光熔化增材制造技术研究现状与展望[J]. 金属学报, 2023, 59(1): 31-54.
[7] 陈扬, 毛萍莉, 刘正, 王志, 曹耕晟. 高速冲击载荷下预压缩AZ31镁合金的退孪生行为与动态力学性能[J]. 金属学报, 2022, 58(5): 660-672.
[8] 曾小勤, 王杰, 应韬, 丁文江. 镁及其合金导热研究进展[J]. 金属学报, 2022, 58(4): 400-411.
[9] 丁宗业, 胡侨丹, 卢温泉, 李建国. 基于同步辐射X射线成像液/固复层界面氢气泡的形核、生长演变与运动行为的原位研究[J]. 金属学报, 2022, 58(4): 567-580.
[10] 皇甫顥, 王子龙, 刘永利, 孟凡顺, 宋久鹏, 祁阳. W1 - x Ir x 固溶合金几何结构、电子结构、力学和热力学性能的第一性原理计算[J]. 金属学报, 2022, 58(2): 231-240.
[11] 周丽君, 位松, 郭敬东, 孙方远, 王新伟, 唐大伟. 基于飞秒激光时域热反射法的微尺度Cu-Sn金属间化合物热导率研究[J]. 金属学报, 2022, 58(12): 1645-1654.
[12] 罗旋, 韩芳, 黄天林, 吴桂林, 黄晓旭. 层状异构Mg-3Gd合金的微观组织和力学性能[J]. 金属学报, 2022, 58(11): 1489-1496.
[13] 王硕, 王俊升. Al-Li合金中 δ′/θ′/δ复合沉淀相结构演化及稳定性的第一性原理探究[J]. 金属学报, 2022, 58(10): 1325-1333.
[14] 李少杰, 金剑锋, 宋宇豪, 王明涛, 唐帅, 宗亚平, 秦高梧. “工艺-组织-性能”模拟研究Mg-Gd-Y合金混晶组织[J]. 金属学报, 2022, 58(1): 114-128.
[15] 毛斐, 吕皓, 唐法威, 郭凯, 刘东, 宋晓艳. MnIn添加对SmCo7结构稳定性及磁矩影响的第一性原理计算[J]. 金属学报, 2021, 57(7): 948-958.