| 连铸二冷区铸坯展宽现象的黏弹塑性分析 |
| 付建勋1;2);李京社1);张慧2) |
1) 北京科技大学冶金与生态工程学院; 北京 100083
2) 中国钢研集团连铸技术国家工程研究中心; 北京 100081 |
|
| VISCOELASTIC-PLASTIC ANALYSIS OF BROADENING OF SLAB IN THE SECONDARY COOLING ZONE OF CONTINUOUS CASTING |
| FU Jianxun1;2); LI Jingshe1); ZHANG Hui2) |
1) School of Metallurgical and Ecological Engineering; University of Science and Technology Beijing; Beijing 100083
2) National Engineering Research Center of Continuous Casting Technology; China Iron $\&$ Steel Research Institute Group; Beijing 100081 |
引用本文:
付建勋 李京社 张慧. 连铸二冷区铸坯展宽现象的黏弹塑性分析[J]. 金属学报, 2010, 46(1): 91-96.
,
,
.
VISCOELASTIC-PLASTIC ANALYSIS OF BROADENING OF SLAB IN THE SECONDARY COOLING ZONE OF CONTINUOUS CASTING[J]. Acta Metall Sin, 2010, 46(1): 91-96.
| [1] Yoshii A, Kihara S. Trans ISIJ, 1986; 26: 891
[2] Maeno S, Wada K, Itoh Y, Nagano Y. Trans ISIJ, 1983; 24: 83
[3] Siyasiya C, van Rooyen G T. Stumpf W E. J South Afr Inst Mining Metall, 2005; 105: 473
[4] Lin Q Y, Zhu M Y. Acta Metall Sin, 2007; 43: 1301
(林启勇, 朱苗勇. 金属学报, 2007; 43: 1301)
[5] Chen Z P, Cheng N L, Cui L X, Zhang J Q. Iron Steel, 2004; 39(suppl): 457
(陈志平, 程乃良, 崔立新, 张家泉. 钢铁, 2004; 39(增刊): 457
[6] Fu J X. PhD Thesis, University of Science and Technology Beijing, 2009
(付建勋. 北京科技大学博士学位论文, 2009)
[7] Kim K H, Yeo T J, Oh K H, Lee D N. ISIJ Int, 1996; 36: 284
[8] Grill A, Schwerdtfeger K. Ironmak Steelmak, 1979; 6: 131
[9] Barber B, Lewis B A, Leckenby B M. Ironmak Steelmak, 1985; 12: 171
[10] Okamura K, Kawashima H. ISIJ Int, 1989; 29: 666
[11] Sorimachi K, Brimacombe J K. Ironmak Steelmak, 1977; 4: 240
[12] Wang X C. Finite Element Method. Beijing: Tsinghua University Press, 2003: 125
(王勖成. 有限单元法. 北京: 清华大学出版社, 2003: 125)
[13] Fu J X, Li J S, Wang C L, Zhu J T. Mater Rev, 2009; 23(9): 68
(付建勋, 李京社, 汪春雷, 朱经涛. 材料导报, 2009; 29(9): 68)
[14] Uehara M, Samarasekera I V, Brimacombe J K. Iro nmak Steelmak, 1986; 13: 138
[15] Chen S Q. PhD Thesis, Central Iron and Steel Research Institute, Beijing, 2004
(陈素琼. 钢铁研究总院博士学位论文, 北京, 2004) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|