| 喷丸强化过程及冲击效应的数值模拟 |
| 张洪伟; 张以都; 吴琼 |
| 北京航空航天大学机械工程及自动化学院; 虚拟现实技术与系统国家重点实验室; 北京 100191 |
|
| NUMERICAL SIMULATIONS OF SHOT-PEENING PROCESS AND IMPACT EFFECT |
| ZHANG Hongwei; ZHANG Yidu; WU Qiong |
| School of Mechanical Engineering and Automation; Beihang University; State Key Laboratory of Virtual Reality Technology and Systems; Beijing 100191 |
引用本文:
张洪伟 张以都 吴琼. 喷丸强化过程及冲击效应的数值模拟[J]. 金属学报, 2010, 46(1): 111-117.
,
,
.
NUMERICAL SIMULATIONS OF SHOT-PEENING PROCESS AND IMPACT EFFECT[J]. Acta Metall Sin, 2010, 46(1): 111-117.
| [1] Luan W L, Tu S D. Chin Mech Eng, 2005; 16: 1405.
(栾伟玲, 涂善东. 中国机械工程, 2005; 16: 1405)
[2] Al–Hassani S T S. In: Niku–lari A ed., Proc 1st Int Conf on Shot Peening, Paris: Pergamon Press, 1981: 583
[3] Al–Obaid Y F. Mech Mater, 1995; 19: 251
[4] Kobayashi M, Matsui T, Murakami Y. Int J Fatigue, 1998; 20: 351
[5] Johnson W. Impact Strength of Materials. London: Arnold, 1972: 3
[6] Meguid S A, Klair M S. J Mech Work Technol, 1985; 11: 87
[7] Meguid S A, Klair M S. Int J Mech Sci, 1985; 27: 157
[8] Al–Obaid Y F T. Comput Struct, 1990; 36: 681
[9] Schiffner K, Helling C D G. Comput Struct, 1999; 72: 329
[10] Meguid S A, Shagal G, Stranart J C, Daly J. Finite Elem Anal Des, 1999; 31: 179
[11] Hong T, Ooi J Y, Shaw B A. Adv Eng Software, 2008; 39: 743
[12] Baragetti S. Int J Comput Appl Technol, 2001; 14: 51
[13] Meguid S A, Shagal G, Stranart J C. Int J Impact Eng, 2002; 27: 119
[14] Majzoobi G H, Azizi R, Alavi Nia A. A. J Mater Process Technol, 2005; 164–165: 1226
[15] Ling X, PengWW, Ni H F. J Mech Eng, 2006; 42: 182
(凌祥, 彭薇薇, 倪红芳. 机械工程学报, 2006; 42: 182)
[16] Wang L L. Foundation of Stress Waves. Beijing: National Defense Industry Press, 2005: 1
(王礼立. 应力波基础. 北京:国防工业出版社, 2005: 1)
[17] Hallquist J O. LS–dyna Keyword User’s Manual Version 970. California: Livermore Software Technology Corporation, 2003: 818
[18] Mandal S, Rice J, Elmustafa A A. J Mater Process Technol, 2008; 203: 401 |
|
Viewed |
|
|
|