| Al薄膜纳米压痕过程的多尺度模拟 |
| 黎军顽1;倪玉山1;林逸汉1;罗诚1;江五贵2 |
1.复旦大学力学与工程科学系; 上海 200433
2.Faculty of Built Environment and Engineering; Queensland University of Technology; Brisbane QLD4001; Australia |
|
| MULTISCALE SIMULATION OF NANOINDENTATION ON Al THIN FILM |
| LI Junwan1; NI Yushan1; LIN Yihan1; LUO Cheng1; JIANG Wugui2 |
1.Department of Mechanics and Engineering Science; Fudan University; Shanghai 200433
2.Faculty of Built Environment and Engineering; Queensland University of Technology; Brisbane QLD4001; Australia |
引用本文:
黎军顽 倪玉山 林逸汉 罗诚 江五贵. Al薄膜纳米压痕过程的多尺度模拟[J]. 金属学报, 2009, 45(2): 129-136.
,
,
,
,
.
MULTISCALE SIMULATION OF NANOINDENTATION ON Al THIN FILM[J]. Acta Metall Sin, 2009, 45(2): 129-136.
| [1] Oliver W C, Pharr G M. J Mater Res, 1992; 7: 1564
[2] Li X D, Bhushan B. Mater Charact, 2002; 48: 11
[3] Bamber M J, Cooke K E, Mann A B, Derby B. Thin Solid Films, 2001; 399: 299
[4] Bhushan B, Koinkar V N. Appl Phys Lett, 1994; 64: 1653
[5] Chen J, Bull S J. Thin Solid Films, 2006; 494: 1
[6] Sangwal K, Gorostiza P, Sanz F. Surf Sci, 2000; 446: 314
[7] Zimmerman J A, Kelchner C L, Klein P A, Hamilton J C, Foiles S M. Phys Rev Lett, 2001; 87: 165507
[8] Shankar R M. Appl Phys Lett, 2007; 90: 171924
[9] Kiely J D, Hwang R Q, Houston J E. Phys Rev Lett, 1998;81: 4424
[10] Yang B, Vehoff H. Acta Mater, 2007; 55: 849
[11] Soifer Y M, Verdyan A, Kazakevich M, Rabkin E. Scr Mater, 2002; 47: 799
[12] Liu Y, Varghese S, Ma J, Yoshino M, Lu H, Komanduri R. Int J Plast, 2008; 24: 1990
[13] Kiely J D, Houston J E. Phys Rev, 1998; 19B: 12588
[14] Phillips R, Rodney D, Shenoy V, Tadmor E, Ortiz M. Modell Simul Mater Sci Eng, 1999; 7: 769
[15] Shenoy V B, Phillips R, Tadmor E B. J Mech Phys Solids,2000; 48: 649
[16] Ni Y S, Wang H T. Chin Q Mech, 2005; 26: 366
(倪玉山, 王华滔.力学季刊, 2005; 26: 366)
[17] Tadmor E B, Miller R, Phillips R. J Mater Res, 1999; 14:2233
[18] Shan D, Yuan L, Guo B. Mater Sci Eng, 2005; A412: 264
[19] Iglesias R A, Leiva E P. Acta Mater, 2006; 54: 2655
[20] Li J W, Jiang W G. Acta Metall Sin, 2007; 43: 851
(黎军顽, 江五贵.金属学报, 2007; 43: 851)
[21] Jiang W G, Li J W, Su J J, Tang J L. Acta Mech Solida Sin, 2007; 28: 375
(江五贵, 黎军顽, 苏建君, 汤井伦.固体力学学报, 2007; 28:375)
[22] Ni Y S, Wang H T. Chin J Mech Eng, 2007; 43: 101
(倪玉山, 王华滔.机械工程学报, 2007; 43: 101)
[23] Tadmor E B, Hai S. J Mech Phys Solids, 2003; 51: 765
[24] Miller R, Ortiz M, Phillips R, Shenoy V, Tadmor E B. Eng Fract Mech, 1998; 61: 427
[25] Gannepalli A, Mallapragada S K. Phys Rev, 2002; 66B:104103
[26] Jarausch K F, Kiely J D, Houston J E, Russell P E. J Mater Res, 2000; 15: 1693
[27] Smith R, Christopher D, Kenny S D, Richter A, Wolf B. Phys Rev, 2003; 67B: 245405
[28] Van Vliet K J, Li J, Zhu T, Choi Y J, Yip S, Suresh S. Solid Mech Its Appl, 2004; 115: 203
[29] Kelchner C L, Plimpton S J, Hamilton J C. Phys Rev, 1998; 58B: 11085
[30] Tadmor E B. PhD Thesis, Brown University, Providence, Rhode Island, 1996
[31] Tadmor E B, Ortiz M, Phillips R. Philos Mag, 1996; 73A: 1529
[32] Tadmor E B, Phillips R, Ortiz M. Langmuir, 1996; 12: 4529
[33] Shenoy V B, Miller R, Tadmor E B, Rodney D, Phillips R, Ortiz M. J Mech Phys Solids, 1999; 47: 611
[34] Ercolessi F, Adams J B. Europhys Lett, 1994; 28: 538
[35] Minor A M, Lilleodden E T, Stach E A, Morris J W. J Mater Res, 2004; 19: 176
[36] Hirth J P, Lothe J. Theory of Dislocations. New York: John Wiley and Sons, 1982: 757
[37] Kosugi T, Kino T. Mater Sci Eng, 1993; A164: 368 |
|