| 熔融Cu55团簇在冷却过程中结构变化的分子动力学模拟 |
| 张林;徐送宁;张彩碚;祁阳 |
| 东北大学理学院材料物理与化学研究所 |
|
| Modelling structural changes of a molten Cu55 cluster on cooling by molecular dynamics |
| zhang lin;;; |
| 东北大学 |
引用本文:
张林; 徐送宁; 张彩碚; 祁阳 . 熔融Cu55团簇在冷却过程中结构变化的分子动力学模拟[J]. 金属学报, 2008, 44(10): 1161-1166 .
,
,
,
.
Modelling structural changes of a molten Cu55 cluster on cooling by molecular dynamics[J]. Acta Metall Sin, 2008, 44(10): 1161-1166 .
[1]Ercolessi F,Andreoni W,Tosatti E.Phys Rev Lett,1991; 66:911 [2]Li T X,Ji Y L,Yu S W,Wang G H.Solid State Commun, 2000;116:547 [3]Zhang Z,Hu W Y,Xiao S F.Phys Rev,2006;73B:125443 [4]Liu H B,Ascencio J A,Alvarez M P,Yacaman M J.Surf Sci,2001;491:88 [5]Xu S N,Zhang L,Zhang C B,Qi Y.Acta Metall Sin,2007; 43:379 (徐送宁,张林,张彩碚,祁阳.金属学报,2007;43:379) [6]Lee Y J,Maeng J Y,Lee E K,Kim B,Kim S,Han K K. J Comput Chem,2000;21:380 [7]Chushak Y G,Bartell L S.J Phys Chem,2001;105B: 11605 [8]Valkealahti S,Manninen M.Phys Rev,1992;45B:9459 [9]Zhang L,Zhang C B,Qi Y.Chin Phys,2007;16:77 [10]Yang Q W,Zhu R Z,Wen Y H.Acta Phys Sin,2005;54: 89 (杨全文,朱如曾,文玉华.物理学报,2005:54:89) [11]Zhang L,Zhang C B,Qi Y.Phys Lett,2008;372A:2874 [12]Yildirim E K,Guven(?)Z B.Modell Simul Mater Sci Eng, 2006;14:947 [13]Nam H S,Hwang N M,Yu B D,Yoon J K.Phys Rev Lett, 2002;89:275502 [14]Ikeshoji T,Koga K.Phys Rev,2001;63E:031101 [15]Yang Q W,Zhu R Z.Acta Phys Sin,2005;54:4245 (杨全文,朱如曾.物理学报,2005;54:4245) [16]Qi W H,Wang M P,Li Z,Xie D.Chin J Nonferrous Met- als,2005;15:1854 (齐卫宏,汪明朴,李周,谢丹.中国有色金属学报,2005;15:1854) [17]Rosu M F,Pleiter F,Niesen L.Phys Rev,2001;63B: 165425 [18]Haberland H,Issendorff B V.Phys Rev Lett,1996;76: 1445 [19]Flelicke A,Kirilyuk A,Ratsch C,Behler J,Scheffler M, Von Helden G,Ferrando G.Phys Rev Lett,2004;93: 023401 [20]Chen S,Sommers J M.J Phys Chem,2001;105B:816 [21]Baumberger F,Greber T,Osterwalder J.Phys Rev,2000; 62B:15431 [22]Martin D S,Maunder A,Weightman P.Phys Rev,2001; 63B:155403 [23]Boisvert G,Lewis L J.Phys Rev,1997;56B:7643 [24]Trushin O S,Salo P,Al-Nissila T.Phys Rev,2000;62B: 1611 [25]Sprague J A,Montalenti F,Uberuaga B P,Kress J D, Voter A F.Phys Rev,2002;66B:205415 [26]Jacob T,Anton J,Sarpe-Tudoran C,Sepp W D,Fricke B,Bastu(?)T.Surf Sci,2003;536:45 [27]Frantz J,Rusanen M,Nordlund K,Koponen I T.J Phys: Condens Matter,2004;16:2995 [28]Darby S,Mortimer-Jones T V,Johnston R L,Roberts C. J Chem Phys,2002;116:1536 [29]Mei J,Davenport J W,Fernado G W.Phys Rev,1991; 43B:4653 [30]Liu J,Zhao J Z,Hu Z Q.Acta Metall Sin,2005;41:219 (刘俊,赵九洲,胡壮麒.金属学报,2005;41:219) [31]Zhang L,Wang S Q,Ye H Q.Chin Phys,2006;15:610 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|