| 强磁场下电磁振荡对Al-Si过共晶合金凝固中初生硅分布和形貌的影响 |
| 余建波;任维丽;邓康;钟云波;王洪亮 |
| 上海大学 |
|
| Effect of the electromagnetic vibration on the distribution and morphology of primary silicon in Al-Si hypereutectic alloy solidified under a high magnetic field |
| YU Jian-Bo |
| 上海大学 |
引用本文:
余建波; 任维丽; 邓康; 钟云波; 王洪亮 . 强磁场下电磁振荡对Al-Si过共晶合金凝固中初生硅分布和形貌的影响[J]. 金属学报, 2007, 43(9): 994-998 .
,
,
,
,
.
Effect of the electromagnetic vibration on the distribution and morphology of primary silicon in Al-Si hypereutectic alloy solidified under a high magnetic field[J]. Acta Metall Sin, 2007, 43(9): 994-998 .
[1]David P.Mod Cast,1990;82(2):55 [2]Pan E N,Hu J F.AFS Trans,1998;105:413 [3]Bunk W G.Mater Sci Eng,1991;A134:1087 [4]Vives C.Mater Sci Eng,1993;A173:169 [5]Vives C.J Cryst Growth,1996;158:118 [6]Radjai A,Miwa K,Nishio T.Metall Mater Trons,1998; 29A:1477 [7]Radjai A,Miwa K,Nishio T.Metall Mater Trans,2002; 33A:3025 [8]Takagi T,Iwai K,Asai S.ISIJ Int,2003;43:842 [9]Iwai K,Sugiura K.Mater Sci Forum,2005;475:2695 [10]Wang H L,Ren Z M,Ren W L,Wang J,Deng K,Zhong Y B.Shanghai Met,2006;28(5):40 (王洪亮,任忠鸣,任维丽,王俊,邓康,钟云波.上海金属,2006;28(5):40) [11]Ren W L,Ren Z M,Wang H L,Zhong Y B,Deng K,Yu J B.Mater Sci Technol,in press (任维丽,任忠鸣,王洪亮,钟云波,邓康,余建波.材料科学与工艺,待发表) [12]Wang J,Deng K,Ren Z M,Ren W L,Li X,Zhong Y B, Xu K D.Shanghai Met,2006;28(6):7 (王俊,邓康,任忠鸣,任维丽,李喜,钟云波,徐匡迪.上海金属,2006;28(6):7) [13]Zhang Q,Cui J Z.Chin J Nouferrous Met,2003;13:1500 (张勤,崔建忠.中国有色金属学报,2003;13:1500) [14]Mao W M,Li S S,Zhao A M,Cui C L,Zhong X Y.Mater Sci Technol,2001;9:117 (毛为民,李树索,赵爱民,崔成林,钟雪友.材料科学与工艺,2001;9:117) [15]Zhang B W.PhD Dissertation,Shanghai University,2003: 26 (张邦文.上海大学博士学位论文,2003:26) [16]Zhou Y H,Hu Z Q,Jie W Q.Solidification Technology. Beijing:China Machine Press,1998:46 (周尧和,胡壮麒,介万奇.凝固技术.北京:机械工业出版社,1998:46)7 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|