| 单相合金定向凝固的特征尺度和过冷度研究 |
| 王琳琳 林 鑫 黄卫东 苏云鹏 李 涛 |
| 西北工业大学凝固技术国家重点实验室 |
|
| Research on the solidification characteristic scale and undercooling during directional solidification of single-phase alloy |
| ;;;; |
| 西北工业大学凝固技术国家重点实验室 |
引用本文:
王琳琳; 林鑫; 黄卫东; 苏云鹏; 李涛 . 单相合金定向凝固的特征尺度和过冷度研究[J]. 金属学报, 2006, 42(10): 1025-1030 .
[1]Kurz W,Fisher D J.Fundamentals of Solidification.3rd edition,Aedermansdorf,Switzerland:Trans Tech Publications,1992 [2]Huang W D,Shang B L,Zhou Y H.Chin J Aeronaut,1992;13A:376(黄卫东,商宝禄,周尧和.航空学报,1992;13A:376) [3]Huang W D,Shang B L,Zhou Y H.Acta Phys Sin,1991;40:323(黄卫东,商宝禄,周尧和.物理学报,1991;40:323) [4]Burden M H,Hunt J D.J Cryst Growth,1974;22:99 [5]Burden M H,Hunt J D.J Cryst Growth,1974;22:109 [6]Somboonsuk K,Mason J T,Trivedi R.Metall Trans,1984;15A:967 [7]Huang W D.PhD Dissertation,Northwestern Polytechnical University,Xi'an,1989(黄卫东.西北工业大学博士学位论文,西安,1989) [8]Somboonsuk K,Mason J T,Trivedi R.Metall Trans,1984;15A:977 [9]Huang W D,Geng X G,Zhou Y H.J Cryst Growth,1993;134:105 [10]Lin X,Huang W D,Pan Q Y,Ding G L,Xue Y F,Zhou Y H.Acta Metall Sin,1997;33:1140(林鑫,黄卫东,潘清跃,丁国陆,薛玉芳,周尧和.金属学报,1997;33:1140) [11]Lin X,Huang W D,Fen J,Li T,Zhou Y H.Acta Mater,1999;47:3271 [12]Ding G L,Huang W D,Huang X,Lin X,Zhou Y H.Acta Mater,1996;44:3705 [13]Ding G L,Lin X,Huang W D,Zhou Y H.Acta Metall Sin,1995;31:20(丁国陆,林鑫,黄卫东,周尧和.金属学报,1995;31:20) [14]Esaka H,Kurz W.J Cryst Growth,1985;72:578 [15]Lin X,Li Y M,Liu Z X,Li T,Huang W D.Sci Technol Adv Mater,2001;2:293 [16]Lin X.PhD Dissertation,Northwestern Polytechnical University,Xi'an,2000(林鑫.西北工业大学博士学位论文,西安,2000) [17]Huang W D,Ding G L,Zhou Y H.Chin J Mater Res,1995;9:193(黄卫东,丁国陆,周尧和.材料研究学报,1995;9:193) [18]Lin X,Li T,Wang L L,Su Y P,Huang W D.Acta Phys Sin,2004;53:3971(林鑫,李涛,王琳琳,苏云鹏,黄卫东.物理学报,2004;53:3971) [19]Huang W D,Lin X,Li T,Wang L L,Inatomi Y.Acta Phys Sin,2004;53:3978(黄卫东,林鑫,李涛,王琳琳,Inatomi Y.物理学报,2004;53:3978) [20]Mullins W W,Sekerka R F.J Appl Phys,1963;34:323 [21]Mullins W W,Sekerka R F.J Appl Phys,1964;35:444 [22]Ding G L.PhD Dissertation,Northwestern Polytechnical University,Xi'an,1996(丁国陆.西北工业大学博士学位论文,西安,1996) [23]Eshelman M A,Seetharaman V,Trivedi R.Acta Metall,1988;36:1165 [24]Burden M H,Hunt J D.J Cryst Growth,1974;22:109 [25]Laxmanan V.Acta Metall,1985;33:1037 [26]Laxmanan V.J Cryst Growth,1986;75:5733 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|