| fcc,压稳hcp和bcc-Cu的原子状态及物理性质随温度的变化关系 |
| 陶辉锦; 谢佑卿; 彭红建; 余方新; 刘锐锋; 李晓波 |
| 中南大学材料科学与工程学院 |
|
| Temperature Dependence of tom States and Physical Properties of fcc-, metastable hcp- and bcc- Cu |
| TAO Huijin; XIE Youqing; PENG Hongjian; YU Fangxin; LIU Ruifeng;LI Xiaobo |
| 中南大学材料科学与工程学院 |
引用本文:
陶辉锦; 谢佑卿; 彭红建; 余方新; 刘锐锋; 李晓波 . fcc,压稳hcp和bcc-Cu的原子状态及物理性质随温度的变化关系[J]. 金属学报, 2006, 42(6): 565-571 .
,
,
,
,
,
.
Temperature Dependence of tom States and Physical Properties of fcc-, metastable hcp- and bcc- Cu[J]. Acta Metall Sin, 2006, 42(6): 565-571 .
[1] Kaufman L, Bernstein H. Computer Calculation of Phase Diagram,. New York: Academic Press Inc., 1970: 1 [2] Saunders N, Miodownik A P. CALPHAD (Calculation of PhaseDiagrams): A Comprehensive Guide. New York: Pergamon, 1998: 1 [3] Dinsdale A T. CALPHAD, 1991; 15: 317 [4] Wang Y, Curtarolo S, Jiang C. CALPHAD, 2004; 28: 79 [5] Xie Y Q, Tao H J, Peng H J. Physica, 2005; 366B: 17 [6] Xie Y Q. Sci Chin, 1993; 36E: 90 [7] Xie Y Q. Trans Nonferrous Met Soc Chin, 1994; 4(3): 63 [8] Xie Y Q, Zhang X D, Zhao L Y. Sci Chin, 1993; 36A: 487 [9] Xie Y Q, Ma L Y, Zhang X D. Sci Chin, 1993; 36A: 612 [10] Xie Y Q. Ada. Metall Mater, 1994; 42: 3705 [11] Xie Y Q. Sci Chin, 1998; 41E: 146 [12] Xie Y Q, Zhang X D. Sci Chin, 1998; 41E: 157 [13] Xie Y Q, Zhang X D. Sci Chin, 1998; 41E: 225 [14] Xie Y Q, Zhang X D. Sci Chin, 1998; 41E: 348 [15] Xie Y Q, Peng K, Liu X B. Physica, 2004; 344B: 5 [16] Xie Y Q, Liu X B, Peng K. Physica, 2004; 353B: 15 [17] Xie Y Q, Peng H J, Liu X B. Physica, 2004; 362B: 1 [18] Yu F X, Xie Y Q, Nie Y Z. Trans Nonferrous Met Soc Chin, 2004; 14: 1041 [19] Xie Y Q. Acta Metall Sin, 1998; 34: 1233 (谢佑卿.金属学报, 1998;34:1233) [20] Xie Y Q, Zhang X D. Acta Metall Sin, 1994; 30: 531 (谢佑卿,张晓东.金属学报, 1994;30:531) [21] Guo Y Q, Yu R H, Zhang R L. J Phys Chem, 1998; 102B: 9 [22] Pauling L. The Nature of the Chemical Bond. Ithaca: Cornell University Press, 1960: 56 [23] Kirby R K, Hahn T A, Rothroch B D. American Institute of Physics Handbook. New York: McGraw-Hill Book Company, 1972: 4 [24] Eckardt H, Fritsche L, Noffke J. J Phys, 1984; 14F: 97 [25] Kittel C. Solid State Physics. New York: John Wiley and Sons. Inc., 1976: 55 [26] Ozolin V, Wolverton S C, Zunger A. Phys Rev, 1998; 57B: 6427 [27] Wei S H, Mbaye A A, Ferreira L G. Phys Rev, 1987; 36B: 4163 [28] Chen J R, Li C J. Phase Transitions of Solids in Metals and Alloys. Beijing: Metallurgical Industry Press, 1997: (陈景榕,李承基.金属与合金中的固态相变.北京:冶金工业 出版社,1997:8) [29] Zhang Z J. J Phys: Condens Matter, 1998; 10: L495M |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|