| NiAl-28Cr-5Mo-1Hf合金的高温氧化行为研究 |
| 徐春梅 郭建亭 杨福宝 |
| 中国科学院金属研究所;沈阳110016 |
|
引用本文:
徐春梅; 郭建亭; 杨福宝 . NiAl-28Cr-5Mo-1Hf合金的高温氧化行为研究[J]. 金属学报, 2001, 37(8): 857-860 .
[1] Guha S, Monroe P R, Baker I. Mater Sci Eng, 1991; 131A:27 [2] Darolia R, Lahrman D, Field R. Scr Metall Maten 1992;26: 1007 [3] Chen X F, Johnson D R, Oliver B F. Scr Metall Mater,1994; 30: 975 [4] Chen X F, Johnson D R, Noebe R D, Oliver B F. J MaterRes, 1995; 10: 1159 [5] Johnson D R, Chen X F, Oliver B P, Noebe R D, Whit-tenberger J D. Intermet, 1995; 3: 99 [6] Cui C Y, Guo J T. Acta Metall Sin, 1999; 35: 477(崔传勇、郭建亭 金属学报,1999;35:477) [7] Cui C Y, Guo J T, Li G S, Qi Y H, Ye H Q. Acta MetallSin, 2000; 36: 1144(崔传勇,郭建亭,李谷松,齐义辉,叶恒强 金属学报,2000;36:1144) [8] Rybicki G C, Smialek J L. Oxid Met, 1989; 32: 275 [9] Grabke H J, Steinhorst M, Brumm M, Wiemer D. OxidMet, 1991; 35: 199 [10] Guo J T. Acta Metall Sin, 1979; 15: 203(郭建亭 金属学报,1979; 15:203) [11] Zeng C L, Rizzo F C, Wu W T, Guo J T. J Chin SocCorro Prot, 1999; 19: 39(曾潮流,Rizzo F C,吴维■.郭建亭.中国腐蚀与防护学报,1999;19:39) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|