| Ni基耐热合金凝固过程的元胞自动机方法模拟 |
| 张林 王元明 张彩碚 |
| 东北大学理学院;沈阳110004 |
|
引用本文:
张林; 王元明; 张彩碚 . Ni基耐热合金凝固过程的元胞自动机方法模拟[J]. 金属学报, 2001, 37(8): 882-888 .
[1] Brown S G R, Spittle J A. Mater Sci Technol, 1989; 5:362 [2] Zhu P Smith W. Acta Metall, 1992; 40: 683 [3] Rappaz M, Gandin Ch. -A. Acta Metall, 1993; 41: 345 [4] Gandin Ch. -A, Rappaz M. Metall Trans, 1993; 24A: 467 [5] Beckermann C, Vishanta R. Appl Mech Rev, 1993; 46: 1 [6] Saito Y, Goldbeck-Wood G, Muller-Krumbhaar H. PhysRev A, 1988; 38: 2148 [7] Lipton J, Glicksman M E, Kurz W. Mater Sci Eng, 1984;65: 57 [8] Hesselbarth H W, Gobel I R. Acta Metall, 1991; 39: 2135 [9] Kremeyer K. J Comp Phys, 1998; 142: 2432 |
|