| 倒双级时效对一种高强度铁镍基合金抗氢脆性能的影响 |
| 李秀艳 马禄铭 李依依 |
| 中国科学院金属研究所;沈阳110016 |
|
引用本文:
李秀艳; 马禄铭; 李依依 . 倒双级时效对一种高强度铁镍基合金抗氢脆性能的影响[J]. 金属学报, 2002, 38(6): 593-596 .
[1] Rothova V, Stloukal I, Ceermak J. Acta Metall, 2000; 48:827 [2] Olive J M, Puiggali M, Herms E. Mater Sci Eng, 1999;272: 279 [3] Thompson A W, Brooks J A. Metall Tran A, 1975; 6A:1431 [4] Moody N R, Robinson S L, Garrison W M. J Res Mech,1990; 143 [5] Ma L M, Liang G J, Fan C G, Li Y Y. Acta Metall Sin(English lett), 1997; 10: 206 [6] Huang Q Y, Li H K. Superalloy. Beijing: Scientific andTechnological Press, 2000: 40 (黄乾尧,李汉康.高温合金.北京:科学技术出版社,2000:40) |
|