| Fe-6.5Si合金热轧板显微组织的TEM观察 |
| 王聪 林栋梁 单爱党 陈家光 曹涵清 宋洪伟 |
| 上海交通大学高温合金和高温测试教育部重点实验室;上海200030 |
|
引用本文:
王聪; 林栋梁; 单爱党; 陈家光; 曹涵清; 宋洪伟 . Fe-6.5Si合金热轧板显微组织的TEM观察[J]. 金属学报, 2002, 38(5): 517-520 .
[1]Raviprasad K,Chattopadhyay K. Acta Matall Mater,1993; 41: 609 [2] Raviprasad K, Chattopadhyay K. Mater Sci Eng, 1988;98: 281 [3]Viala B, Degauque J, Fagot M, Baricco M, Ferrara E, Fio-rillo F. Mater Sci Eng, 1996; A212: 62 [4]Monstadt H, Hornbogen E Rohde J.J Magn Magn Mater,1992;112: 245 [5] Raviprasad K, Aoki K, Chattopadhyay K. Mater Sci Eng,1993; A172:125 [6]Watanabe T. Mater Sci Forum, 1993; 126-128: 295* |
|