| 动态与静态纯腐蚀对定量研究材料冲刷腐蚀交互作用的影响 |
| 张安峰 邢建东 鲍崇高 贾焕如 |
| 西安交通大学机械工程学院;西安710049 |
|
引用本文:
张安峰; 邢建东; 鲍崇高; 贾焕如 . 动态与静态纯腐蚀对定量研究材料冲刷腐蚀交互作用的影响[J]. 金属学报, 2002, 38(5): 521-524 .
[1] Fontana M G. Greene N D. Corrosion Engineering. Lon-don: Mc Graw-Hiff Book Company, 1987: 11 [2]Zelders H G. Met Corros, 1949; 65(1): 25 [3] Weiser P F. Beck F H, Fontana M G. Mater Performance, 1973; 12(3): 34 [4] Kim K Y, Bhattacharyya S, Agarwala V. In: Rhee S K, Ruff A W. Ludema K G eds. Inter Conf on Wear of Ma-terials. Som Franciso: ASME. 1981: 772 [5] Zheng Y G. Yao Z M, Wei X Y, Kei W. Wear, 1995; 186-187: 555 [6] Madsen B W.Wear, 1988; 123:127 [7]Watson S W.Wear, 1995; 181-183: 469 [8] Batchelor A W. Stachowiak G W. Wear. 1998; 123: 281 [9]Povarov O A. Tomarov G V. Therm Eng, 1985; 32(9): 511 |
|