| SiC颗粒增强铝基梯度复合材料的制备与性能 |
| 许富民 齐民 朱世杰 赵杰 王富岗 |
| 大连理工大学材料工程系;大连116024 |
|
引用本文:
许富民; 齐民; 朱世杰; 赵杰; 王富岗 . SiC颗粒增强铝基梯度复合材料的制备与性能[J]. 金属学报, 2002, 38(9): 998-1001 .
[1] Shih C H. Mater Sci Prog, 1990; 4: 97 (师昌绪.材料科学进展,1990;4:97) [2] Markworth A J, Ramesh K S, Parks W P. J Mater Sci,1995; 30: 2183 [3] Koizumi M. Compos Part B, 1997; 28: 1 [4] Wakashima K, Hirano T, Nino M. Space Applicationof Advance Structure Materials. ESP SP-303(EuropeanSpace Agency), 1990: 97 [5] Sugimura Y, Suresh S. Metal Trans, 1992; 23A: 2231 [6] Shang J K, Ritchie R O. Acta Metall, 1989; 37: 2267 [7] Zhu S J, Peng L M, Ma Z Y, Bi J, Wang F G, Wang Z G.Mater Sci Eng, 1996; A215: 120 [8] Peng L M, Zhu S J, Wang F G, Chen H R, Ma Z Y, Bi J.J Mater Sci, 1998; 33: 5643 [9] Lin C-Y, McShane H B, Rawlings R D. Mater Sci Technol,1994; 10: 659 [10] Suresh S. Metall Trans, 1985; 16A: 249 |
|