新型镍基粉末冶金高温合金中γ'相扇形组织形成以及演化行为研究 |
胡本芙1), 刘国权1, 2), 吴凯1), 胡鹏辉1) |
1)北京科技大学材料科学与工程学院, 北京 100083
2)北京科技大学新金属材料国家重点实验室, 北京 100083 |
|
MORPHOLOGICAL CHANGES BEHAVIOR OF FAN-TYPE STRUCTURES OF γ' PRECIPITATES IN NICKEL-BASED POWDER METALLURGY SUPERALLOYS |
HU Benfu1), LIU Guoquan1, 2), WU Kai1), HU Penghui1) |
1) School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
2) State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
胡本芙 刘国权 吴凯 胡鹏辉. 新型镍基粉末冶金高温合金中γ'相扇形组织形成以及演化行为研究[J]. 金属学报, 2012, 48(7): 830-836.
,
,
,
.
MORPHOLOGICAL CHANGES BEHAVIOR OF FAN-TYPE STRUCTURES OF γ' PRECIPITATES IN NICKEL-BASED POWDER METALLURGY SUPERALLOYS[J]. Acta Metall Sin, 2012, 48(7): 830-836.
[1] KaufmanM J, Voorhees PW, JohnsonWC, Biancanniello F S. Metall Trans, 1989; 20A: 2171[2] Calderon H A, Kostorz G, Qu Y Y, Dorantes H J, Cruz J J, Cabanas–Moreno J G. Mater Sci Eng, 1997; A238: 13[3] Minoru D, Toru M, Teruyaki W. Mater Sci Eng, 1984; A67: 249[4] Via P C, Yu J J. Trans Nonferrous Met Soc China, 2005; 15(93): 90[5] Jackson J J, Donachie M J. Metall Trans, 1977; 8A: 1615[6] Larson J M, Volin T G, Larson F G. In: Braun J D, Arrowsmith H W, McCall J L, eds., Microstruct Sci, 1997; 5: 209[7] Furrer D U. Scr Mater, 1999; 40: 1215[8] Furrer D U. In: CSM, BISC, eds., Proc 11th Int Symposium on Advanced Superalloys–Production and Application, Shanghai: the Chinese Society for Metals, 2007: 192[9] Mitchell R J, Li H Y, Huang Z W. J Mater Process Technol, 2009; 209: 1011[10] Lu X D, Deng Q, Du J H, Qu J L, Zhuang J Y, Zhong Z Y. J Alloys Compd, 2009; 477: 100[11] Lu X D, Du J H, Deng Q, Zhong Z Y. J Alloys Compd, 2009; 486: 195[12] Wu K, Liu G Q, Hu B F. J Univ Sci Technol Beijing, 2009; 31: 722[13] Lemsky J. NASA/CR–2004–212950[14] Gabb T P, Gayda J. NASA/TM–2005–213649[15] Hamid A, Schroers J. Acta Mater, 2002; 50: 89[16] Staron P, Kampmann R. Acta Mater, 2000; 48: 701[17] Williams D B, Butler E P. Int Mater Rev, 1981, 26: 153[18] Staron P, Kampmann R. Acta Mater, 2000; 48: 713[19] Mitchell R J, Preuss M. Mater Sci Eng, 2008; A473: 158[20] Doi M, Miyazaki T. Mater Sci Eng, 1985; 74: 139[21] Lifshitz I M, Slyozov V V. J Phys Chem Solids, 1961; 19: 35[22] Wagner C. Z Electrochem, 1961; 65: 581 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|