| 形状记忆合金Ti444Ni47Nb9的抗高温氧化性能 |
| 陶斌武;刘建华;李松梅 |
| 北京航空航天大学材料科学与工程学院; 北京 100083 |
|
| Oxidation Behaviors of Ti44Ni47Nb9 Shape Memory Alloy at High Temperature |
| TAO Binwu; LIU Jianhua; LI Songmei |
| School of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083 |
引用本文:
陶斌武; 刘建华; 李松梅 . 形状记忆合金Ti444Ni47Nb9的抗高温氧化性能[J]. 金属学报, 2005, 41(6): 633-637 .
,
,
.
Oxidation Behaviors of Ti44Ni47Nb9 Shape Memory Alloy at High Temperature[J]. Acta Metall Sin, 2005, 41(6): 633-637 .
[1]Kajiwara S.Mater Sci Eng,1999;A273-275:67 [2]Piao M,Miyazakai S,Otsuka K.Mater Trans JIM,1992; 33:337 [3]Cai W,Zhang C C.J Mater Sci Technol,1994;10:27 [4]Yang H B,Yin W H,Lin J Y,Zhang X M,Guo J H.Rare Met Mater Eng,1999;28:81 (杨华斌,殷为宏,吝靖玉,张小明,郭继红.稀有金属材料与工程,1999;28:81) [5]Dong Z Z,Liu W X,Jia D,Tang Z L,Wang D F.Rare Met Mater Eng,2000;29:182 (董治中,刘文西,贾堤,唐子龙,王德法.稀有金属材料与工程,2000;29:182) [6]Mo H Q,Li C,Wang C L,Qiu S Y,Huang D C,Shen B L.Nucl Power Eng,2003;24:559 (莫华强,李聪,王丛林,邱绍宇,黄德成,沈保罗.核动力工程,2003;24:559) [7]Long N D,Zhu J H.Rare Met Mater Eng,2003;32:740 (龙霓东,朱金华.稀有金属材料与工程,2003;32:740) [8]He X M,Rong L J,Yan D S,Jiang Z M,Li Y Y.Ada Metall Sin,2004;40:721 (何向明,戎利建,阎德胜,姜志民,李依依.金属学报,2004;40:721) [9]Xu C H,Ma X Q,Shi S Q,Wo C H.Mater Sci Eng,2004;A371:45 [10]Liu Y H.Theory of Metal Corrosion.Beijing:Aeronautics Industry Press,1993:186 (刘永辉.金属腐蚀原理.北京:航空工业出版社,1993:186) [11]Gesmundo F,Niu Y,Viani F.Oxid Met,1996;46:441 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|