| 纵向强磁场对MnBi/Bi共晶定向凝固组织的影响 |
| 李 喜;任忠鸣;邓 康;壮云乾;徐匡迪 |
| 上海大学材料科学与工程学院; 上海 200072 |
|
| Effect of High Vertical Magnetic Field on Directional Solidification Structure of Eutectic MnBi/Bi |
| LI Xi; REN Zhongming; DENG Kang; ZHUANG Yunqian; XU Kuangdi |
| Department of Materials Science and Engineering; Shanghai University; Shanghai 200072 |
引用本文:
李喜; 任忠鸣; 邓; 康; 壮云乾; 徐匡迪 . 纵向强磁场对MnBi/Bi共晶定向凝固组织的影响[J]. 金属学报, 2005, 41(6): 588-592 .
,
,
,
,
,
.
Effect of High Vertical Magnetic Field on Directional Solidification Structure of Eutectic MnBi/Bi[J]. Acta Metall Sin, 2005, 41(6): 588-592 .
[1]Guo X,Altounian Z,Stromolser J O.J Appl Phys,1991;69:6067 [2]Pirich R G.Metall Trans,1984;15A:2139 [3]Savas M A,Smith R W.J Cryst Growth,1986;76:880 [4]Notis M R,Shah D M,Young S P,Graham C D.IEEE Trans Magn,1979;3:957 [5]Chen T.J Appl Phys,1974;45:2358 [6]Decarlo J L,Pirich R G.Metall Trans,1984;15A:2155 [7]Pirich R G.In:Rindone G E,ed.,Materials Processing in the Reduced Gravity Environment of Space.New York: Elsevier Science Publishing Co.,1982:593 [8]Pirich R G,Larson D J.In:Rindone G E,ed.,Materials Processing in the Reduced Gravity Environment of Space. New York:Elsevier Science Publishing Co.,1982:523 [9]Wang H,Ren Z M,Deng K,Xu K D.Acta Metall Sin, 2002;38:41 (王晖,任忠鸣,邓康,徐匡迪.金属学报,2002;38:41) [10]Yasuda H,Ohnaka I,Yamamoto Y,Tokieda K,Kishio K. Mater Trans,2003;44:2207 [11]Li X,Ren Z M,Wang H,Li W X,Deng K,Zhuang Y Q. Acta Metall Sin,2004;40:40 (李喜,任忠鸣,王晖,李伟轩,邓康,壮云乾.金属学报,2004;40:40) [12]Gaber F E,Wilcox W R.J Cryst Growth,1986;78:159 [13]Elloit R.Eutectic Solidification Processing Crystalline and Glossy Alloy.London:Butterworths & Co.,1983:165 [14]Feng D,Ding S Y,Zhai H R.Physics of Metal.Vol.4,Beijing:Science Press,1998:460 (冯端,丁世英,翟宏如.金属物理学(第4卷).北京;科学出版社,1998:460) [15]Yu J,Wang W,Jinag J Q,Shu G J.J Southeast Univ,1992;22(2):59 (于金,王武,蒋建清,舒光冀.东南大学学报,1992;22(2):59) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|