| 强磁场对不同磁化率非磁性金属凝固组织的影响 |
| 王 强 王春江 王恩刚 赫冀成 |
| (东北大学材料电磁过程研究教育部重点实验室; 沈阳 110004) |
|
引用本文:
王强; 王春江; 王恩刚; 赫冀成 . 强磁场对不同磁化率非磁性金属凝固组织的影响[J]. 金属学报, 2005, 41(2): 128-132 .
[1] Zhou Y H, Hu Z Q, Qiao W Q. Solidification Technique. Beijing: China Machine Press, 1998: 416(周尧和,胡壮麒,乔万奇.凝固技术.北京:机械工业出版社,1998:416) [2] Burgoyne J W. Proceeding of the 3rd International Symposium on Electromagnetic Processing of Materials, Nagoya: ISIJ, Japan, 2000: 618 [3] Hamai M, Tagami M, Mogi I, Watanabe W, Motokawa M. Proceedings of the Second Meeting of Symposium on New Magneto-Science, Omiya: National Research Laboratoryfor Magnetic Science, Japan, 1998: 150 [4] Ikezoe Y, Kaihatsu T, Uetake H, Hirota N, Nakaqawa J,Kitazawa K. Trans Mater Res Soc Jpn, 2000; 25(1): 77 [5] Pilin B, Gillon P. Proceeding of the 1st InternationalSymposium on Electromagnetic Processing of Materials,Nagoya: ISIJ, Japan, 1994: 97 [6] Waki N, Sassa K, Asai S. Tetsu-to-Hagane, 2000; 86(6):363 [7] Tahashi M, Sassa K, Hirabayashi I, Asai S. Mater TransJIM, 2000; 41(8): 985 [8] Taniguchi T, Sassa K, Yamada T, Asai S. Mater TransJIM, 2000; 41(8): 981 [9] Sassa K, Morigawa H, Asai S. J Jpn Inst Metal, 1997;61(12): 1283 [10] Radjai A, Miwa K. Metall Mater Trans A, 2000; 31(3):755 [11] Wang Q, He J C, Kawai S, Iwai K, Asai S. Acta MetallSin, 2002; 38: 961(王强,赫冀成,川合 悟,岩井一彦,浅井滋生.金属学报,2002;38:961) [12] Martikainen H O, Lindroos V K. Scand J Metall, 1981; 10: 3 [13] Ren Z M, Li X, Deng K, Wang H, Zhuang Y Q. Proceeding of the 4th International Symposium on Electromagnetic Processing of Materials, Lyon: CNRS, COST P6, EDF, ATS, UIE, EFGP, SF2M and FEMS, France, 2003: B5.7.5 [14] Xu Y, Ohstuka H, Wada H. Trans Mater Res Soc Jpn, 2000; 25(2): 501 [15] Masahashi N, Matsuo M, Watanabe K. J Mater Res, 1998; 13(2): 457 [16] Choi J K, Oktsuka H, Xu Y, Chu W Y. Scr Mater, 2000; 43: 221 [17] Watanabe K, Motokawa M. Materials Science in Static High Magnetic Fields. Berlin: Springer, 2001: 3 [18] Asai S. J Jpn Inst Met, 1997; 61(12): 1271 [19] Sazaki G, Yoshida E, Komastu H, Nakada T, Miyashita S, Watanabe K. J Cryst Growth, 1997; 173: 231 [20] Saxena R C, Tandon J N. Nature, 1960; 4707: 158 [21] Kawai S, Wang Q, Iwai K, Asai S. Mater Trans, 2001; 42(2): 275 [22] Angus W R. Proc Roy Soc, 1932; 136: 569 [23] Yasuda H, Ohnaka I, Fujimoto S, Hayashi Y, Yamamoto M, Kishio K, Tsuchiyama A, Nakano T, Uesugi K. Proceeding of the 4th International Symposium on Electromagnetic Processing of Materials, Lyon: CNRS, COST P6, EDF, ATS, UIE, EFGP, SF2M and FEMS, France, 2003: 474 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|