| TiC/AZ91D镁基复合材料高温压缩变形行为 |
| 陈礼清;董群;郭金花;毕敬;徐永波 |
| 中国科学院金属研究所; 沈阳110016 |
|
| Compressive deformation behavior of TiC/AZ91Dcomposites at elevated temperatures |
| CHEN Liqing; DONG Qun; GUO Jinhua; BI Jing; XU Yongbo |
| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
陈礼清; 董群; 郭金花; 毕敬; 徐永波 . TiC/AZ91D镁基复合材料高温压缩变形行为[J]. 金属学报, 2005, 41(3): 326-332 .
,
,
,
,
.
Compressive deformation behavior of TiC/AZ91Dcomposites at elevated temperatures[J]. Acta Metall Sin, 2005, 41(3): 326-332 .
[1] Lloyd D J. Int Mater Rev, 1994; 39: 1 [2] Hu H, Yu A, Li N Y, Allison J E. Mater Manufact Process, 2003; 18: 687 [3] Krishnadev M R, Angers R, Krishnadas Nair C G, Huard G. JOM, 1993; 45: 52 [4] Mordike B L, Ebert T. Mater Sci Eng, 2001; A302: 37 [5] Saravanan R A, Surappa M K. Mater Sci Eng, 2000; A276: 108 [6] Cai Y, Taplin D, Tan M J, Zhou W. Scr Mater, 1999; 41: 967 [7] Dong Q, Chen L Q, Zhao M J, Bi J. Mater Lett, 2004; 58: 920 [8] Chen L Q, Dong Q, Zhao M J, Bi J. Chin J Mater Res, 2004; 18: 193 (陈礼清,董群,赵明久,毕敬.材料研究学报,2004;18: 193) [9] Dong Q, Chen L Q, Zhao M J, Bi J. J Mater Sci Technol, 2004; 20: 3 [10] Chen L Q, Dong Q, Zhao M J, Bi J, Kanetake N. Mater Sci Eng, 2005; A, in press [11] Li S B, Wu K, Zheng M Y, Yao Z K. Mater Eng, 2003; (2): 15 (李淑波,吴昆,郑明毅,姚忠凯.材料工程,2003;(2):15) [12] Jiang D T, Guo J T, Li G S, Shi C X. Acta Metall Sin, 1998; 34: 1143 (姜东涛,郭建亭,李谷松,师昌绪.金属学报,1998;34:1143) [13] Roberts W, Kraussed G. In: Kraussed G ed., Deformation, Processing and Structure. Metals Park, OH: American Society for Metals, 1984: 109 [14] Barbagallo S, Cavaliere P, Cerri E. Mater Sci Eng, 2004; A367: 9 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|