| 玻璃与Kovar合金电场辅助阳极连接时紧密接触面积扩大过程的动力学 |
| 陈铮 董师润 |
| 华东船舶工业学院材料与环境工程系; 镇江212003 |
|
引用本文:
陈铮; 董师润 . 玻璃与Kovar合金电场辅助阳极连接时紧密接触面积扩大过程的动力学[J]. 金属学报, 2001, 37(2): 139-143 .
[1] Mack S, Baumann H, Gosele U, Werner H, Schlogl R. JElectrochem Soc, 1997; 144: 1106 [2] Albaugh K B. J Am Ceram Soc, 1992; 75: 2644 [3] Albaugh K B. J Electrochem Soc, 1991; 138: 3089 [4] Nitzsche P, Lange K, Schmidt B, Grigull S, Kreissig U. JElectrochem Soc, 1998; 145: 1755 [5] Morsy M A, Ishizaki K, Ikeuchi K, Ushio M. Q J Jpn WeldSoc, 1998; 16: 157 [6] Anthony T R. J Appl Phys, 1983; 54: 2419 [7] Morsy A, Ikeuchi K, Ushio M. Mater Trans JIM, 1996;37: 1511 [8] Guan Z Z. Physics Properties of Inorganic Materials. Beijing: Tsinghua University Press, 1992: 219(关振择主编. 无机材料物理性能. 北京: 清华大学出版社, 1992:219)? |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|