| 机械合金化制备的Al-Pb-Cu合金结构与摩擦性能 |
| 曾美琴 张耀 欧阳柳章 罗堪昌 朱敏 |
| 华南理工大学机电工程系;广州510640 |
|
引用本文:
曾美琴; 张耀; 欧阳柳章; 罗堪昌; 朱敏 . 机械合金化制备的Al-Pb-Cu合金结构与摩擦性能[J]. 金属学报, 2002, 38(8): 814-818 .
[1] Mohan S, Agarwala V, Ray S. Mater Sci Eng, 1991; 144A:215 [2] Ichikawa K, Ishizuka S. Trans Jpn Inst Met, 1987; 28: 145 [3] Mackay M L. Met Prog, 1977; 32: 111 [4] Zhu M, Li B L, Gao Y, Li L, Li Z X. Scr Mater, 1997; 36:443 [5] Zhu M, Lai J K L, Che X Z, Li Z X. J Mater Sci, 1998;33: 5873 [6] Zhu M, Gao Y, Chung C Y, Che X Z, Luo K C, Li B L.Wear, 2000; 242: 47 [7] Pkthak J P, Sing V, Tiwari S N. J Mater Sci Lett, 1993;12: 1450 [8] Sharma A, Rajia T V. Wear, 1996; 197: 105 [9] Kim H M, Kim T S, Suryanarayana C, Chun B S. MaterSci Eng, 2000; 287A: 59 [10] Xi S Q, Qu X Y, Ma M L. J Alloy Compound, 1998; 268:211 [11] Ling DY, Zhang D L. J Alloy Compound, 2000; 311: 275 [12] Michels A, Krill C E, Ehrhardt H E, Birringer R, Wu DT. Acta Mater, 1999; 47: 2143 |
|