| 描述不锈钢材料单轴棘轮行为的一元参量体系 |
| 蔡力勋 牛清勇 刘宇杰 |
| 西南交通大学应用力学与工程系;成都610031 |
|
引用本文:
蔡力勋; 牛清勇; 刘宇杰 . 描述不锈钢材料单轴棘轮行为的一元参量体系[J]. 金属学报, 2002, 38(9): 966-973 .
[1] Chaboche J L, Nouailhas D. J Eng Mater Technol, 1989;111: 384 [2] Hassan T, Kriakides S. Int J Plasticity, 1992; 8: 91 [3] Ohno N, Wang J D. Int J Plasticity, 1993; 9: 375 [4] Jiang Y Y, Sehitoglu H. J Appl Mechan, 1996; 63: 720 [5] Jiang Y Y, Sehitoglu H. J Appl Mechan, 1996; 63: 726 [6] Yang X J, Gao Q, Cai L X. Acta Aeronautica AstronauticaSin, 1997; 18: 395 (杨显杰,高 庆,蔡力勋,航空学报,1997;18:395) [7] Cai L X, Luo H F, Gao Q. Acta Aeronautica AstrohouticaSin, 2002; 23: 17 (蔡力勋,罗海丰,高庆,航空学报,2002;23:17) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|