| 齿轮选材及热处理工艺智能专家系统 |
| 李新城 陈 光 朱伟兴 王 匀 张开华 汪建敏 |
| 江苏大学机械工程学院; 镇江 212013 |
|
| Intelligent Expert System Used in Gear Material Selection and its Heat Treatment |
| LI Xincheng; CHEN Guang; ZHU Weixing; WANG Yun; ZHANG KAihua; WANG Jianmin |
| School of Mechanical Engineering; Jiangsu Univercity; Zhenjiang 212013 |
引用本文:
李新城; 陈光; 朱伟兴; 王匀; 张开华; 汪建敏 . 齿轮选材及热处理工艺智能专家系统[J]. 金属学报, 2004, 40(10): 1051-1054 .
,
,
,
,
,
.
Intelligent Expert System Used in Gear Material Selection and its Heat Treatment[J]. Acta Metall Sin, 2004, 40(10): 1051-1054 .
[1] Zakarian V I, Kaiser M J. Expert System Appl, 1999; 16: 233 [2] Mizoguchi R. IEEE Expert, 1995; 8: 23 [3] Kim H S, Im Y T. Mater Proc Technol, 1999; 95: 262 [4] Chan Y W. Computer Appl Technol, 1998; 11: 66 [5] Sonar R M. Expert System Appl, 1999; 17: 45 [6] Phillip W G. Eng Appl Artificial Intelligence, 1996; 2: 163 [7] Lucas W. Weld World, 1994; 34: 9 [8] Andrew R G, Paul S R. Artificial Intelligence, 1996; 87:215 [9] ASM Handbook Committee. Metal Handbook (Vol.6) .New York: McGraw-Hill, 1996: 158 [10] Lange K. Handbook of Metal Forming. New York:McGraw-Hill, 1995: 116 |
|