| 三元合金高温理论氧化图 II.低氧压下的近似分析 |
| 牛焱 王文 曹中秋 |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室;沈阳110016 |
|
引用本文:
牛焱; 王文; 曹中秋 . 三元合金高温理论氧化图 II.低氧压下的近似分析[J]. 金属学报, 2001, 37(4): 411-414 .
[1] Kofstad P. High Temperature Corrosion. New York: Elsevier Applied Science, 1988: 389 [2] Stott F H, Wood G C, Stringer J. Oxid Met, 1995; 44: 113 [3] Gesmundo F, Gleeson B. Oxid Met, 1995; 44: 211 [4] Stringer J, Wright I G. Oxid Met, 1995; 44: 265 [5] Nesbitt J A. Oxid Met, 1995; 44: 309 [6] Kirkaldy J, Young D J. Diffusion in the Condensed State.London: The Institute of Metals, 1987: 174 [7] Smialek J L, Meier G M. In: Sims C T, Stoloff N S, HagelW C eds., Superalloys II, New York: Wiley, 1987: 293 [8] Wagner C J. Electrochem Soc, 1952; 99: 369 [9] Niu Y, Cao Z Q, Wang W, Wu W T. Acta Metall Sin,2000; 36: 744(牛焱,曹中秋,王 文,吴维,金属学报, 2000; 36: 744) |
|