Please wait a minute...
金属学报  2004, Vol. 40 Issue (3): 263-269     
  论文 本期目录 | 过刊浏览 |
奥氏体形变对仿晶界型铁素体/粒状贝氏体复相钢组织和强韧性能的影响
王建平;杨志刚;白秉哲;方鸿生;冯 勇;徐洪庆
清华大学材料科学与工程系
Influence of Austenite Deformation on the Microstructure Strength and Toughness of the Grain Boundary Allotriomorphic Ferrite/Granular Bainite (F GBA/Bg) Duplex Steel
WANG Jianping; YANG Zhigang; BAI Bingzhe; FANG Hongsheng;FENG Yong; XU Hongqing
Department of Materials Science and Engineering; Tsinghua University
引用本文:

王建平; 杨志刚; 白秉哲; 方鸿生; 冯勇; 徐洪庆 . 奥氏体形变对仿晶界型铁素体/粒状贝氏体复相钢组织和强韧性能的影响[J]. 金属学报, 2004, 40(3): 263-269 .
, , , , , . Influence of Austenite Deformation on the Microstructure Strength and Toughness of the Grain Boundary Allotriomorphic Ferrite/Granular Bainite (F GBA/Bg) Duplex Steel[J]. Acta Metall Sin, 2004, 40(3): 263-269 .

全文: PDF(26143 KB)  
摘要: 通过Gleeble--1500热力模拟实验机对仿晶界型铁素体/粒状贝氏体复相钢进行了A r3以上不同温度、不同形变量的平面应变压缩实验. SEM和TEM观察表明, 奥氏体形变不仅细化仿晶界型铁素体, 而且促进先共析铁素体在原奥氏体晶内形核, 从而有利于细化粒状贝氏体晶团及其内部的铁素体片条和MA岛.给出的组织变化模型可阐述形变对粒状贝氏体精细结构的影响. 经过780℃下30%形变, 即使在形变后空冷的条件下也获得了平均长度小于5 m、平均宽度小于2.5 m的仿晶界型铁素体晶粒、平均粒径小于3 m的晶内铁素体. 与未经过形变的试样相比, CVN常温冲击韧性值从未形变的43 J提高到108 J, Vickers硬度从242提高到312, 为工业生产工艺的改进提供了重要根据.
关键词 : 晶粒细化,  奥氏体形变,  粒状贝氏体    
Abstract:The plane strain compressive deformation experiments with various deformation amounts have been carried out on the grain boundary allotriomorphic ferrite/granular bainite F GBA/G Bduplex steel at temperatures above A r3 using Gleeble--1500 machine. SEM and TEM observations indicate that the prior austenite deformation not only refines the allotriomorphic ferrite grain but also promotes the nucleation of intragranular ferrite, both of which in turn contribute to the refinement of granular bainite cluster including its ferrite platelets and MA islands. A model was proposed to elucidate the effect of prior deformation on the refinement of granular bainite cluster and its detailed microstructure. For specimens deformed by 30% at 780℃ and subsequent air cooling, F GBA grains of an average size less than 5 m and intragranular ferrite grains less than 3 m were gained. Compared with specimens without prior deformation, the Charpy V--notch (CVN) impact energy and Vickers hardness is increase from 43 J to 108 J and from 242 to 312, respectively.
Key words: grain refinement    austenite deformation    granular bainite   
收稿日期: 2003-03-11     
ZTFLH:  TG142. 1  
[1] Hulka K, Hesterkamp F, Nachtel L. Processing, M(?)crostructure and Properties of HSLA Steels. Warrendale, PA: TMS, 1988:153
[2] Czyryca E J. Key Eng Mater, 1993; 84-85:491
[3] Garcia C I, Lis A K, Pytel S M, DeArdo A J. ISS Transactions, 1992; 13:103
[4] Chiaki OUCHI. ISIJ International, 2001; 41(6) : 542
[5] Fang H S, Xu P G, Bai B Z, Liu D Y. Heat Treat Met, 2000; 11:1(方鸿生,徐平光,白秉哲,刘东雨.金属热处理,2000;11:1)
[6] Xu P G, Fang H S, Bai B Z, Wang Z J, Yang Z G, Huang J G. J Iron Steel Res Int, 2002; 9(2) : 33
[7] Gibbs R K, Hodgson P D, Parker B A. In: Liaw P K ed, Morris E. Fine Sympos(?)um, Warrendale, PA: TMS, 1991:73
[8] Yada H, Matsumura Y, Senuma T. In: Tamura I ed, Proceedings of the International Conference on Physical Metallurgy of Thermomechanical Processing of Steels and Other metals, Tokyo: Iron and Steel Institute of Japan, 1988:200
[9] Fang H S, Wang J J, Yang Z G, Li C M, Bo X Z, Zheng Y K. Bainite Transformation. Beijing: Science Press, 1999:11(方鸿生,王家军,杨志刚,李春明,薄祥正,郑燕康.贝氏体相变.科学出版社,1999:11)
[10] Fang H S, Deng H J, Zhao R F, Zheng Y K. Mater Mech Eng, 1981; 5(1) :5(方鸿生,邓海金,赵如发,郑燕康.机械工程材料,1981;5(1) :5)\
[1] 李小兵, 潜坤, 舒磊, 张孟殊, 张金虎, 陈波, 刘奎. W含量对Ti-42Al-5Mn-xW合金相转变行为的影响[J]. 金属学报, 2023, 59(10): 1401-1410.
[2] 吴国华, 童鑫, 蒋锐, 丁文江. 铸造Mg-RE合金晶粒细化行为研究现状与展望[J]. 金属学报, 2022, 58(4): 385-399.
[3] 丁宁, 王云峰, 刘轲, 朱训明, 李淑波, 杜文博. 高应变速率多向锻造Mg-8Gd-1Er-0.5Zr合金的微观组织、织构及力学性能[J]. 金属学报, 2021, 57(8): 1000-1008.
[4] 蒋中华, 杜军毅, 王培, 郑建能, 李殿中, 李依依. M-A岛高温回火转变产物对核电SA508-3钢冲击韧性影响机制[J]. 金属学报, 2021, 57(7): 891-902.
[5] 李秀程,孙明煜,赵靖霄,王学林,尚成嘉. 铁素体-贝氏体/马氏体双相钢中界面的定量化晶体学表征[J]. 金属学报, 2020, 56(4): 653-660.
[6] 武华健, 程仁山, 李景仁, 谢东升, 宋锴, 潘虎成, 秦高梧. Al含量对Mg-Sn-Ca合金微观组织与力学性能的影响[J]. 金属学报, 2020, 56(10): 1423-1432.
[7] 张军,介子奇,黄太文,杨文超,刘林,傅恒志. 镍基铸造高温合金等轴晶凝固成形技术的研究和进展[J]. 金属学报, 2019, 55(9): 1145-1159.
[8] 邓丽萍,崔凯旋,汪炳叔,向红亮,李强. AZ31镁合金室温多道次压缩过程微观组织和织构演变的研究[J]. 金属学报, 2019, 55(8): 976-986.
[9] 李淑波, 杜文博, 王旭东, 刘轲, 王朝辉. Zr对Mg-Gd-Er合金晶粒细化机理的影响[J]. 金属学报, 2018, 54(6): 911-917.
[10] 毛轶哲, 李建国, 封蕾. 573 K高温时效处理的Al-10Mg合金中粗大β(Al3Mg2)相对热压缩组织演化的影响及机理[J]. 金属学报, 2018, 54(10): 1451-1460.
[11] 胡小锋, 姜海昌, 赵明久, 闫德胜, 陆善平, 戎利建. 一种Fe-Cr-Ni-Mo高强高韧合金钢焊接接头的组织和力学性能[J]. 金属学报, 2018, 54(1): 1-10.
[12] 张丽丽, 江鸿翔, 赵九洲, 李璐, 孙倩. 溶质Ti对Al-Ti-B中间合金细化Al影响的新认识:TiB2粒子的动力学行为及溶质Ti的影响[J]. 金属学报, 2017, 53(9): 1091-1100.
[13] 张志强,董利民,关少轩,杨锐. TC16钛合金辊模拉丝过程中的显微组织和力学性能[J]. 金属学报, 2017, 53(4): 415-422.
[14] 李宁,张蓉,张利民,邢辉,殷鹏飞,吴耀燕. 低压交流电脉冲下Al-7%Si合金晶粒细化机理研究[J]. 金属学报, 2017, 53(2): 192-200.
[15] 左锦荣,侯陇刚,史金涛,崔华,庄林忠,张济山. 两阶段轧制变形过程中高强铝合金析出相与晶粒结构演变及其对性能的影响*[J]. 金属学报, 2016, 52(9): 1105-1114.