| 圆坯方坯凝固定律的导出和验证 |
| 张兴中;那贤昭;王忠英;刘爱强;干 勇 |
| 钢铁研究总院连铸技术国家工程研究中心 |
|
| Deduction and Validation of Solidification Law for Round and Square Blooms |
| ZHANG Xingzhong; NA Xianzhao; WANG Zhongying; LIU Aiqiang; GAN Yong |
| National Engineering Research Center of Continuous Casting Technology; Central Iron and Steel Research Institute |
引用本文:
张兴中; 那贤昭; 王忠英; 刘爱强; 干勇 . 圆坯方坯凝固定律的导出和验证[J]. 金属学报, 2004, 40(3): 281-284 .
,
,
,
,
.
Deduction and Validation of Solidification Law for Round and Square Blooms[J]. Acta Metall Sin, 2004, 40(3): 281-284 .
[1] Adams M C. Liquid Metals and Solidification, Cleveland Ohio: American Society for Metals, 1958:187 [2] Okamoto T. Casting, 1977; 49(10) : 624 [3] Mizikar E A. Trans Metall Soc AIME, 1967; 239:1747 [4] Yang H L, Zhao L G, Zhang X Z, Deng K W, Gan Y. Metall Mater Trans, 1998; 29B: 1345 [5] Gautie J J R, Morillon Y, Dumont-Fillon J. JISI, 1970; 208:1053 |
|