  研究论文 本期目录 | 过刊浏览 |
热处理对GH4065A/IN718异质高温合金惯性摩擦焊接头界面微观组织的影响
秦志伟, 王彬, 赵强, 李家辰, 孙毓涛, 洪小龙, 李鹏, 董红刚()
大连理工大学 材料科学与工程学院 大连 116024
Effect of Heat Treatment on Interfacial Microstructure of Inertial Friction Welded Joints for GH4065A/IN718 Dissimilar Superalloys
QIN Zhiwei, WANG Bin, ZHAO Qiang, LI Jiachen, SUN Yutao, HONG Xiaolong, LI Peng, DONG Honggang()
School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
引用本文:

秦志伟, 王彬, 赵强, 李家辰, 孙毓涛, 洪小龙, 李鹏, 董红刚. 热处理对GH4065A/IN718异质高温合金惯性摩擦焊接头界面微观组织的影响[J]. 金属学报, 2026, 62(6): 1032-1042.
Zhiwei QIN, Bin WANG, Qiang ZHAO, Jiachen LI, Yutao SUN, Xiaolong HONG, Peng LI, Honggang DONG. Effect of Heat Treatment on Interfacial Microstructure of Inertial Friction Welded Joints for GH4065A/IN718 Dissimilar Superalloys[J]. Acta Metall Sin, 2026, 62(6): 1032-1042.

全文: PDF(5341 KB)   HTML
摘要: 

面对航空发动机领域对高推重比发展的不懈追求,本工作采用惯性摩擦焊接技术成功实现了GH4065A/IN718异质高温合金的高质量连接,并系统分析了焊后热处理对接头界面微观组织演变的影响规律。结果表明,接头界面结合良好且无明显焊接缺陷。可通过焊后热处理调控微观组织,热处理过程中的动态再结晶及晶界迁移使焊核区和热机械影响区宽度增加。焊后热处理导致GH4065A侧γ′相和IN718侧γ′′相均匀析出,γ′/γ′′强化相的体积分数和平均尺寸增加。焊后热处理态接头各区域晶粒轻微长大,且热机械影响区局部取向差明显降低,这表明应力集中现象得到有效缓解。此外,热处理态焊核区析出了细小的γ′/γ′′相,位错在切过强化相的过程中形成堆垛层错,进一步阻碍了位错运动,增强变形抗力。

关键词 : 焊后热处理,  惯性摩擦焊接,  强化相,  动态再结晶,  位错    
Abstract:

There has been a relentless pursuit for high thrust-to-weight ratio development in the aeroengine field. To tackle this, the study successfully achieved high-quality joining of GH4065A/IN718 dissimilar superalloys via inertia friction welding that demonstrated excellent interfacial bonding and no significant welding defects. A systematic investigation was performed on the influence of post-weld heat treatment on the microstructural evolution at the joint interface. The results indicated that post-weld heat treatment increased the width of the weld nugget and thermomechanically affected zones via dynamic recrystallization and grain boundary migration, which confirmed its regulatory effect on the microstructure. Heat treatment promoted uniform precipitation of γ′ and γ′′ phases on the GH4065A and IN718 sides, respectively, thereby increasing the volume fraction and average size of the γ′/γ′′ strengthening phases. After heat treatment, minor grain coarsening was observed in all the joint regions, along with a considerable reduction in local misorientation in the thermomechanically affected zone, indicating effective alleviation of stress concentration. Moreover, fine γ′/γ′′ phases precipitated in the heat-treated weld nugget zone, and dislocations that cut through these strengthening phases resulted in the formation of stacking faults, which further impeded dislocation motion and enhanced deformation resistance.

Key words: post-weld heat treatment    inertial friction welding    strengthening phase    dynamic recrystallization    dislocation
收稿日期: 2025-09-24     
ZTFLH:  TG132.3  
基金资助:国家自然科学基金项目(52275314);国家自然科学基金项目(52504402)
通讯作者: 董红刚,donghg@dlut.edu.cn,主要从事新材料及异种材料连接技术研究
Corresponding author: DONG Honggang, professor, Tel: (0411)84706283, E-mail: donghg@dlut.edu.cn
作者简介: 秦志伟,男,1997年生,博士
AlloyCCrCoWMoAlTiNbZrBFeNi
GH4065A0.01116.0013.04.04.002.103.700.700.050.0151.00Bal.
IN7180.01019.39--3.050.531.025.21--16.69Bal.
表1  GH4065A和IN718高温合金的化学成分 (mass fraction / %)
图1  焊态和热处理态接头沿轴向各区域显微组织的OM像
图2  焊态和热处理态接头沿轴向各区域微观组织的SEM像
图3  焊态和热处理态接头界面的SEM像和EPMA像
图4  焊态接头沿轴向各区域的EBSD分析
图5  热处理态接头沿轴向各区域的EBSD分析
图6  焊态接头焊核区(WZ)的TEM分析
图7  焊后热处理态接头WZ的TEM分析
图8  焊态和热处理态接头的强度和硬度
[1] Peng Z C, Luo J P, Zhao Y, et al. Evolution of microstructure during static recrystallization in FGH96 superalloy[J]. Acta Metall. Sin., 2025, 61: 235
[1] 彭子超, 罗俊鹏, 赵 宇 等. FGH96合金静态再结晶过程的显微组织演化[J]. 金属学报, 2025, 61: 235
doi: 10.11900/0412.1961.2022.00540
[2] Bai R S, Tan Y, Cui H Y, et al. Effect of electron beam smelting power on microstructure, segregation, and γ′ phase precipitation behavior of GH4068 alloy[J]. Acta Metall. Sin., 2024, 60: 1189
[2] 白如圣, 谭 毅, 崔弘阳 等. 电子束熔炼功率对GH4068合金微观组织、偏析和γ′相析出行为的影响[J]. 金属学报, 2024, 60: 1189
doi: 10.11900/0412.1961.2023.00263
[3] Qin Z W, Zhao Q, Zhang L, et al. Research progress on inertial friction welding of nickel-based superalloy GH4065A and IN718[J]. J. Netsh. Form. Eng., 2024, 16(10): 28
[3] 秦志伟, 赵 强, 张 露 等. 镍基高温合金GH4065A与IN718惯性摩擦焊接研究进展[J]. 精密成形工程, 2024, 16(10): 28
[4] Zhao P, Li P, Ding Z J, et al. Microstructural characterization and mechanical properties of inertia friction welded FGH96 joints[J]. Mater. Today Commun., 2025, 42: 111194
[5] Li C A, Qin G L, Wang H. Omnidirectional simulation analysis of thermo-mechanical coupling mechanism in inertia friction welding of Ni-based superalloy[J]. Chin. J. Aeronaut., 2025, 38: 103047
doi: 10.1016/j.cja.2024.05.003
[6] Tang T X, Shi Q Y, Zhang C B, et al. Elucidating the in-process interfacial friction regime and thermal responses during inertia friction welding of dissimilar superalloys[J]. J. Mater. Res. Technol., 2024, 30: 1650
doi: 10.1016/j.jmrt.2024.03.210
[7] Liu Y Y, Li J J, Tian W T, et al. Research status of inertial friction welding of dissimilar alloys[J]. Weld. Joining, 2021, (1): 35
[7] 刘莹莹, 李洁洁, 田万涛 等. 异种合金惯性摩擦焊的研究现状[J]. 焊接, 2021, (1): 35
[8] Senkov O N, Mahaffey D W, Semiatin S L. A comparison of the inertia friction welding behavior of similar and dissimilar Ni-based superalloys[J]. Metall. Mater. Trans., 2018, 49A: 5428
[9] Huang W Y, Zhang W, Yu Q, et al. A promising strategy of multicomponent alloy intermedium for enhancing the mechanical performance of inertia friction welding joints of Inconel 718 alloys[J]. Mater. Sci. Eng., 2024, A899: 146480
[10] Zhou J, Zhang Y Q, Qin F, et al. Analysis of microstructural evolution and mechanical properties of FGH101 powder superalloy and IN718 deformed superalloy via inertia friction welding[J]. Front. Mater., 2025, 11: 1544584
doi: 10.3389/fmats.2024.1544584
[11] Tong Y Q, Zhang L L, Li C, et al. Microstructure and mechanical properties of IN690 Ni-based alloy/316LN stainless-steel dissimilar ring joint welded by inertia friction welding[J]. Materials, 2024, 17: 695
doi: 10.3390/ma17030695
[12] Li J, An X H, Wang T, et al. Thermal deformation behavior and dynamic recrystallization mechanism of GH4065A alloy considering the effect of γ′ phase[J]. Intermetallics, 2024, 175: 108545
doi: 10.1016/j.intermet.2024.108545
[13] Ramakrishna M, Divya K, Chandrasekhar S B, et al. Heterogeneous precipitation of γ′′ along LAGBs during post-heat treatment of powder bed fusion additively manufactured IN718 superalloy[J]. Scr. Mater., 2025, 268: 116898
doi: 10.1016/j.scriptamat.2025.116898
[14] Bai Y B, Zhang R, Cui C Y, et al. Eliminating embrittlement of GH4065A superalloy at intermediate temperature by a novel grain boundary strengthening mechanism[J]. Mater. Lett., 2023, 335: 133798
doi: 10.1016/j.matlet.2022.133798
[15] Li X G, Liu J T, Liu Q, et al. High-temperature fatigue behavior of inertia friction welded joints of GH4065A Ni-based superalloy[J]. Acta Metall. Sin. (Engl. Lett.), 2024, 37: 1935
doi: 10.1007/s40195-024-01739-4
[16] Wang Z T, Huang S, Zhang W Y, et al. Microstructure characterization and mechanical property of the GH4065A superalloy inertia friction welded joints[J]. Metals, 2022, 12: 1390
doi: 10.3390/met12081390
[17] Tang T X, Shi Q Y, Zhou J, et al. Kissing bond defects in inertia friction welds of IN718 alloys: Experiment and prediction[J]. J. Mater. Process. Technol., 2025, 338: 118786
doi: 10.1016/j.jmatprotec.2025.118786
[18] Huang W Y, Li Y, Yuan J, et al. Study on the enhanced accelerated-creep resistance and microstructural features of IN718 superalloy inertia friction welding joint containing a high entropy alloy interlayer[J]. Mater. Today Commun., 2025, 46: 112639
[19] Huang Z W, Li H Y, Preuss M, et al. Inertia friction welding dissimilar nickel-based superalloys alloy 720Li to IN718[J]. Metall. Mater. Trans., 2007, 38A: 1608
[20] Liang W, Zhou J, Zhang C B, et al. High temperature tensile fracture characteristics of FGH96/IN718 inertial friction welded joint[J]. Trans. China Weld. Inst., 2023, 44(9): 44
[20] 梁 武, 周 军, 张春波 等. FGH96/IN718惯性摩擦焊接头高温拉伸断裂特征[J]. 焊接学报, 2023, 44(9): 44
[21] Zhang L, Zhang C B, Liao Z X, et al. Microstructure and texture distribution characteristics in weld zone of IN718/FGH96 inertial friction welded joint[J]. Electr. Weld. Mach., 2022, 52(4): 8
[21] 张 露, 张春波, 廖仲祥 等. IN718/FGH96惯性摩擦焊接头焊缝区微观组织状态与织构分布特征[J]. 电焊机, 2022, 52(4): 8
[22] Sun Y T, Zhao Q, Qin Z W, et al. Radial microstructural uniformity in inertia friction welded IN718/FGH96 dissimilar joints with post-weld heat treatment[J]. J. Mater. Sci., 2026, 61: 1962
doi: 10.1007/s10853-025-11989-x
[23] Zhou X M, Feng Y F, Zeng W H, et al. Effect of aging treatment on the behavior of room temperature tensile of P/M superalloys used for inertia friction welding joints[J]. Powder Metall. Technol., 2021, 39: 41
[23] 周晓明, 冯业飞, 曾维虎 等. 时效处理对粉末高温合金惯性摩擦焊接头室温拉伸行为的影响[J]. 粉末冶金技术, 2021, 39: 41
doi: 10.19591/j.cnki.cn11-1974/tf.2020030010
[24] Cao S, Li X G, Liu J T, et al. Effect of post-welding aging treatment on the microstructure and high-temperature properties of inertia friction welded GH4065A joint[J]. Materials, 2023, 16: 3639
doi: 10.3390/ma16103639
[25] Huang W P, Yang J J, Yang H H, et al. Heat treatment of Inconel 718 produced by selective laser melting: Microstructure and mechanical properties[J]. Mater. Sci. Eng., 2019, A750: 98
[26] Chamanfar A, Sarrat L, Jahazi M, et al. Microstructural characteristics of forged and heat treated Inconel-718 disks[J]. Mater. Des., 2013, 52: 791
doi: 10.1016/j.matdes.2013.06.004
[27] Zhang C B, Liang W, Zhou J, et al. Effect of heat treatment on microstructure and microhardness of FGH96 inertia friction welding[J]. Trans. China Weld. Inst., 2023, 44(8): 57
[27] 张春波, 梁 武, 周 军 等. 热处理工艺对FGH96合金惯性摩擦焊组织与显微硬度的影响[J]. 焊接学报, 2023, 44(8): 57
[28] Wang B, Huang J H, Zhang T C, et al. Effects of rotation rate on microstructures and mechanical properties of FGH96/GH4169 superalloy inertia friction welding joints[J]. Trans. China Weld. Inst., 2018, 39(4): 41
[28] 王 彬, 黄继华, 张田仓 等. 压力对FGH96/GH4169高温合金惯性摩擦焊接头性能的影响[J]. 焊接学报, 2018, 39(4): 41
[29] Mantri S A, Dasari S, Sharma A, et al. Effect of micro-segregation of alloying elements on the precipitation behaviour in laser surface engineered alloy 718[J]. Acta Mater., 2021, 210: 116844
doi: 10.1016/j.actamat.2021.116844
[30] Zhao P F, Hou K L, Wang M, et al. Effects of sub-solvus ageing on the tensile and creep properties of a new cast nickel-based superalloy[J]. J. Mater. Sci. Technol., 2025, 212: 289
doi: 10.1016/j.jmst.2024.06.014
[31] Gallmeyer T G, Moorthy S, Kappes B B, et al. Knowledge of process-structure-property relationships to engineer better heat treatments for laser powder bed fusion additive manufactured Inconel 718[J]. Addit. Manuf., 2020, 31: 100977
[32] Wang Z Y, Xue C C, Liu Y J, et al. Effects of phosphorus and boron on the γ″ precipitate evolution and creep properties of IN718 superalloy during long-term thermal exposure at 680 oC[J]. J. Alloys Compd., 2024, 995: 174743
doi: 10.1016/j.jallcom.2024.174743
[1] 王彬, 赵鹏, 刘家伟, 张春波, 秦志伟, 董红刚, 李鹏. 热处理对FGH96高温合金惯性摩擦焊接头微观组织演变及力学性能的影响[J]. 金属学报, 2026, 62(6): 1043-1058.
[2] 吴帆, 刘华辉, 边文珊, 蔡竣宇, 金士杰, 罗忠兵. TC4钛合金循环变形微观组织演化与滑移机制[J]. 金属学报, 2026, 62(6): 1082-1090.
[3] 张哲峰, 侯嘉鹏, 刘睿, 李孝滔, 张振军, 张鹏. 金属材料强度-塑性及强度-电导率定量关系[J]. 金属学报, 2026, 62(2): 253-262.
[4] 赵霞, 王旻, 郝宪朝, 张龙, 高明, 马颖澈, 刘奎. 晶界碳化物和动态再结晶对690合金柱状晶凝固组织高温塑性的影响[J]. 金属学报, 2026, 62(2): 339-350.
[5] 郑德宇, 夏玉峰, 曾扬, 周杰. 水平集法模拟GH4706合金动态再结晶过程[J]. 金属学报, 2025, 61(9): 1425-1437.
[6] 杨帆, 裴世超, 罗新蕊, 陈宇翔, 李宁宇, 常永勤. 6061铝合金搅拌摩擦增材制造显微组织演变及力学性能[J]. 金属学报, 2025, 61(8): 1129-1140.
[7] 张洺川, 徐勤思, 刘意, 蔡雨升, 牟义强, 任德春, 吉海宾, 雷家峰. 热压温度对TC4合金扩散连接区组织与性能的影响[J]. 金属学报, 2025, 61(8): 1183-1192.
[8] 李夫顺, 刘志鹏, 丁灿灿, 胡斌, 罗海文. 一种新型高强奥氏体低密度钢的强塑性机理[J]. 金属学报, 2025, 61(6): 909-916.
[9] 包成利, 李豪, 胡励, 周涛, 唐明, 何曲波, 刘相果. 固溶态Mg-10Gd-6Y-1.5Zn-0.5Zr合金热加工图构建及微观组织演变[J]. 金属学报, 2025, 61(4): 632-642.
[10] 曾小勤, 于铭迪, 王静雅. 镁合金的多系滑移与塑性调控[J]. 金属学报, 2025, 61(3): 361-371.
[11] 周雯慧, 熊锦涛, 黄思程, 王鹏昊, 刘勇. AZ31镁合金双峰组织形成机制及其变形行为[J]. 金属学报, 2025, 61(3): 488-498.
[12] 周生玉, 胡明昊, 李冲, 丁海民, 郭乾应, 刘永长. 一种 γ'/γ'' 相强化镍基高温合金的蠕变行为[J]. 金属学报, 2025, 61(2): 226-234.
[13] 韩婧, 邵琛玮, 邱子浩, 张振军, 张哲峰. 晶粒尺寸对Fe-Mn-Al-C系第三代TWIP钢低周疲劳性能的影响[J]. 金属学报, 2025, 61(12): 1873-1883.
[14] 王方圆, 张玉龙, 王章维, 熊志平, 王辉, 宋旼, 夏文真. 纳米压痕下VCoNi 中熵合金的塑性变形行为[J]. 金属学报, 2025, 61(10): 1567-1578.
[15] 韩英, 吴雨航, 赵春禄, 张靖实, 李振民, 冉旭. 选区激光熔化成形Al-Si-Fe-Mn-Ni合金的高温蠕变行为[J]. 金属学报, 2025, 61(1): 154-164.