| 热处理对GH4065A/IN718异质高温合金惯性摩擦焊接头界面微观组织的影响 |
秦志伟, 王彬, 赵强, 李家辰, 孙毓涛, 洪小龙, 李鹏, 董红刚( ) |
| 大连理工大学 材料科学与工程学院 大连 116024 |
|
| Effect of Heat Treatment on Interfacial Microstructure of Inertial Friction Welded Joints for GH4065A/IN718 Dissimilar Superalloys |
QIN Zhiwei, WANG Bin, ZHAO Qiang, LI Jiachen, SUN Yutao, HONG Xiaolong, LI Peng, DONG Honggang( ) |
| School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China |
引用本文:
秦志伟, 王彬, 赵强, 李家辰, 孙毓涛, 洪小龙, 李鹏, 董红刚. 热处理对GH4065A/IN718异质高温合金惯性摩擦焊接头界面微观组织的影响[J]. 金属学报, 2026, 62(6): 1032-1042.
Zhiwei QIN,
Bin WANG,
Qiang ZHAO,
Jiachen LI,
Yutao SUN,
Xiaolong HONG,
Peng LI,
Honggang DONG.
Effect of Heat Treatment on Interfacial Microstructure of Inertial Friction Welded Joints for GH4065A/IN718 Dissimilar Superalloys[J]. Acta Metall Sin, 2026, 62(6): 1032-1042.
| [1] |
Peng Z C, Luo J P, Zhao Y, et al. Evolution of microstructure during static recrystallization in FGH96 superalloy[J]. Acta Metall. Sin., 2025, 61: 235
|
| [1] |
彭子超, 罗俊鹏, 赵 宇 等. FGH96合金静态再结晶过程的显微组织演化[J]. 金属学报, 2025, 61: 235
doi: 10.11900/0412.1961.2022.00540
|
| [2] |
Bai R S, Tan Y, Cui H Y, et al. Effect of electron beam smelting power on microstructure, segregation, and γ′ phase precipitation behavior of GH4068 alloy[J]. Acta Metall. Sin., 2024, 60: 1189
|
| [2] |
白如圣, 谭 毅, 崔弘阳 等. 电子束熔炼功率对GH4068合金微观组织、偏析和γ′相析出行为的影响[J]. 金属学报, 2024, 60: 1189
doi: 10.11900/0412.1961.2023.00263
|
| [3] |
Qin Z W, Zhao Q, Zhang L, et al. Research progress on inertial friction welding of nickel-based superalloy GH4065A and IN718[J]. J. Netsh. Form. Eng., 2024, 16(10): 28
|
| [3] |
秦志伟, 赵 强, 张 露 等. 镍基高温合金GH4065A与IN718惯性摩擦焊接研究进展[J]. 精密成形工程, 2024, 16(10): 28
|
| [4] |
Zhao P, Li P, Ding Z J, et al. Microstructural characterization and mechanical properties of inertia friction welded FGH96 joints[J]. Mater. Today Commun., 2025, 42: 111194
|
| [5] |
Li C A, Qin G L, Wang H. Omnidirectional simulation analysis of thermo-mechanical coupling mechanism in inertia friction welding of Ni-based superalloy[J]. Chin. J. Aeronaut., 2025, 38: 103047
doi: 10.1016/j.cja.2024.05.003
|
| [6] |
Tang T X, Shi Q Y, Zhang C B, et al. Elucidating the in-process interfacial friction regime and thermal responses during inertia friction welding of dissimilar superalloys[J]. J. Mater. Res. Technol., 2024, 30: 1650
doi: 10.1016/j.jmrt.2024.03.210
|
| [7] |
Liu Y Y, Li J J, Tian W T, et al. Research status of inertial friction welding of dissimilar alloys[J]. Weld. Joining, 2021, (1): 35
|
| [7] |
刘莹莹, 李洁洁, 田万涛 等. 异种合金惯性摩擦焊的研究现状[J]. 焊接, 2021, (1): 35
|
| [8] |
Senkov O N, Mahaffey D W, Semiatin S L. A comparison of the inertia friction welding behavior of similar and dissimilar Ni-based superalloys[J]. Metall. Mater. Trans., 2018, 49A: 5428
|
| [9] |
Huang W Y, Zhang W, Yu Q, et al. A promising strategy of multicomponent alloy intermedium for enhancing the mechanical performance of inertia friction welding joints of Inconel 718 alloys[J]. Mater. Sci. Eng., 2024, A899: 146480
|
| [10] |
Zhou J, Zhang Y Q, Qin F, et al. Analysis of microstructural evolution and mechanical properties of FGH101 powder superalloy and IN718 deformed superalloy via inertia friction welding[J]. Front. Mater., 2025, 11: 1544584
doi: 10.3389/fmats.2024.1544584
|
| [11] |
Tong Y Q, Zhang L L, Li C, et al. Microstructure and mechanical properties of IN690 Ni-based alloy/316LN stainless-steel dissimilar ring joint welded by inertia friction welding[J]. Materials, 2024, 17: 695
doi: 10.3390/ma17030695
|
| [12] |
Li J, An X H, Wang T, et al. Thermal deformation behavior and dynamic recrystallization mechanism of GH4065A alloy considering the effect of γ′ phase[J]. Intermetallics, 2024, 175: 108545
doi: 10.1016/j.intermet.2024.108545
|
| [13] |
Ramakrishna M, Divya K, Chandrasekhar S B, et al. Heterogeneous precipitation of γ′′ along LAGBs during post-heat treatment of powder bed fusion additively manufactured IN718 superalloy[J]. Scr. Mater., 2025, 268: 116898
doi: 10.1016/j.scriptamat.2025.116898
|
| [14] |
Bai Y B, Zhang R, Cui C Y, et al. Eliminating embrittlement of GH4065A superalloy at intermediate temperature by a novel grain boundary strengthening mechanism[J]. Mater. Lett., 2023, 335: 133798
doi: 10.1016/j.matlet.2022.133798
|
| [15] |
Li X G, Liu J T, Liu Q, et al. High-temperature fatigue behavior of inertia friction welded joints of GH4065A Ni-based superalloy[J]. Acta Metall. Sin. (Engl. Lett.), 2024, 37: 1935
doi: 10.1007/s40195-024-01739-4
|
| [16] |
Wang Z T, Huang S, Zhang W Y, et al. Microstructure characterization and mechanical property of the GH4065A superalloy inertia friction welded joints[J]. Metals, 2022, 12: 1390
doi: 10.3390/met12081390
|
| [17] |
Tang T X, Shi Q Y, Zhou J, et al. Kissing bond defects in inertia friction welds of IN718 alloys: Experiment and prediction[J]. J. Mater. Process. Technol., 2025, 338: 118786
doi: 10.1016/j.jmatprotec.2025.118786
|
| [18] |
Huang W Y, Li Y, Yuan J, et al. Study on the enhanced accelerated-creep resistance and microstructural features of IN718 superalloy inertia friction welding joint containing a high entropy alloy interlayer[J]. Mater. Today Commun., 2025, 46: 112639
|
| [19] |
Huang Z W, Li H Y, Preuss M, et al. Inertia friction welding dissimilar nickel-based superalloys alloy 720Li to IN718[J]. Metall. Mater. Trans., 2007, 38A: 1608
|
| [20] |
Liang W, Zhou J, Zhang C B, et al. High temperature tensile fracture characteristics of FGH96/IN718 inertial friction welded joint[J]. Trans. China Weld. Inst., 2023, 44(9): 44
|
| [20] |
梁 武, 周 军, 张春波 等. FGH96/IN718惯性摩擦焊接头高温拉伸断裂特征[J]. 焊接学报, 2023, 44(9): 44
|
| [21] |
Zhang L, Zhang C B, Liao Z X, et al. Microstructure and texture distribution characteristics in weld zone of IN718/FGH96 inertial friction welded joint[J]. Electr. Weld. Mach., 2022, 52(4): 8
|
| [21] |
张 露, 张春波, 廖仲祥 等. IN718/FGH96惯性摩擦焊接头焊缝区微观组织状态与织构分布特征[J]. 电焊机, 2022, 52(4): 8
|
| [22] |
Sun Y T, Zhao Q, Qin Z W, et al. Radial microstructural uniformity in inertia friction welded IN718/FGH96 dissimilar joints with post-weld heat treatment[J]. J. Mater. Sci., 2026, 61: 1962
doi: 10.1007/s10853-025-11989-x
|
| [23] |
Zhou X M, Feng Y F, Zeng W H, et al. Effect of aging treatment on the behavior of room temperature tensile of P/M superalloys used for inertia friction welding joints[J]. Powder Metall. Technol., 2021, 39: 41
|
| [23] |
周晓明, 冯业飞, 曾维虎 等. 时效处理对粉末高温合金惯性摩擦焊接头室温拉伸行为的影响[J]. 粉末冶金技术, 2021, 39: 41
doi: 10.19591/j.cnki.cn11-1974/tf.2020030010
|
| [24] |
Cao S, Li X G, Liu J T, et al. Effect of post-welding aging treatment on the microstructure and high-temperature properties of inertia friction welded GH4065A joint[J]. Materials, 2023, 16: 3639
doi: 10.3390/ma16103639
|
| [25] |
Huang W P, Yang J J, Yang H H, et al. Heat treatment of Inconel 718 produced by selective laser melting: Microstructure and mechanical properties[J]. Mater. Sci. Eng., 2019, A750: 98
|
| [26] |
Chamanfar A, Sarrat L, Jahazi M, et al. Microstructural characteristics of forged and heat treated Inconel-718 disks[J]. Mater. Des., 2013, 52: 791
doi: 10.1016/j.matdes.2013.06.004
|
| [27] |
Zhang C B, Liang W, Zhou J, et al. Effect of heat treatment on microstructure and microhardness of FGH96 inertia friction welding[J]. Trans. China Weld. Inst., 2023, 44(8): 57
|
| [27] |
张春波, 梁 武, 周 军 等. 热处理工艺对FGH96合金惯性摩擦焊组织与显微硬度的影响[J]. 焊接学报, 2023, 44(8): 57
|
| [28] |
Wang B, Huang J H, Zhang T C, et al. Effects of rotation rate on microstructures and mechanical properties of FGH96/GH4169 superalloy inertia friction welding joints[J]. Trans. China Weld. Inst., 2018, 39(4): 41
|
| [28] |
王 彬, 黄继华, 张田仓 等. 压力对FGH96/GH4169高温合金惯性摩擦焊接头性能的影响[J]. 焊接学报, 2018, 39(4): 41
|
| [29] |
Mantri S A, Dasari S, Sharma A, et al. Effect of micro-segregation of alloying elements on the precipitation behaviour in laser surface engineered alloy 718[J]. Acta Mater., 2021, 210: 116844
doi: 10.1016/j.actamat.2021.116844
|
| [30] |
Zhao P F, Hou K L, Wang M, et al. Effects of sub-solvus ageing on the tensile and creep properties of a new cast nickel-based superalloy[J]. J. Mater. Sci. Technol., 2025, 212: 289
doi: 10.1016/j.jmst.2024.06.014
|
| [31] |
Gallmeyer T G, Moorthy S, Kappes B B, et al. Knowledge of process-structure-property relationships to engineer better heat treatments for laser powder bed fusion additive manufactured Inconel 718[J]. Addit. Manuf., 2020, 31: 100977
|
| [32] |
Wang Z Y, Xue C C, Liu Y J, et al. Effects of phosphorus and boron on the γ″ precipitate evolution and creep properties of IN718 superalloy during long-term thermal exposure at 680 oC[J]. J. Alloys Compd., 2024, 995: 174743
doi: 10.1016/j.jallcom.2024.174743
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|