金属学报  2026, Vol. 62 Issue (7): 1297-1309    DOI: 10.11900/0412.1961.2024.00322
  研究论文 本期目录 | 过刊浏览 |
Cu/Ta纳米双层膜拉伸变形及Al、W原子掺杂对其变形影响的分子动力学模拟
石腾龙1,2, 陈娟2, 赵彬3, 史俊勤1()
1 西北工业大学 材料学院 先进润滑与密封材料研究中心 西安 710072
2 太原科技大学 材料科学与工程学院 太原 030024
3 西安赛福斯材料防护有限责任公司 西安 710200
Molecular Dynamics Simulations of Tensile Deformation of Cu/Ta Nano-Bilayer Films and the Effect of Al and W Atoms Doping on the Deformation
SHI Tenglong1,2, CHEN Juan2, ZHAO Bin3, SHI Junqin1()
1 Center of Advanced Lubrication and Seal Materials, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi'an 710072, China
2 School of Materials Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030024, China
3 Xi'an Surface Material Protection Co. Ltd., Xi'an 710200, China
引用本文:

石腾龙, 陈娟, 赵彬, 史俊勤. Cu/Ta纳米双层膜拉伸变形及Al、W原子掺杂对其变形影响的分子动力学模拟[J]. 金属学报, 2026, 62(7): 1297-1309.
Tenglong SHI, Juan CHEN, Bin ZHAO, Junqin SHI. Molecular Dynamics Simulations of Tensile Deformation of Cu/Ta Nano-Bilayer Films and the Effect of Al and W Atoms Doping on the Deformation[J]. Acta Metall Sin, 2026, 62(7): 1297-1309.

全文: PDF(5703 KB)   HTML
摘要: 

Cu/Ta纳米双层膜常被用于半导体和微电子器件等领域,在复杂服役环境下会发生变形损伤,导致微尺度设备或器件失效,因此有必要研究Cu/Ta纳米双层膜的拉伸变形行为。本工作采用分子动力学模拟方法研究了Cu/Ta纳米双层膜的拉伸性能及变形机制,并且通过在Cu层中掺杂Al或W原子研究掺杂原子对其变形行为的影响。结果表明,拉伸方向对Cu/Ta纳米双层膜的塑性变形方式有较大影响;在掺杂Al或W原子后,Cu/Ta纳米双层膜的屈服强度增加;掺杂W原子的Cu/Ta纳米双层膜在平行于界面方向拉伸时出现两种取向的堆垛层错,在垂直于界面方向拉伸时Cu层发生fcc→bcc的相变。

关键词 : Cu/Ta界面,  拉伸变形,  合金强化,  分子动力学    
Abstract:

Nano-multilayers composed of immiscible metals have been widely investigated over the past decades due to their exceptional microstructural stability. The Cu/Ta system, which is also immiscible, is particularly notable because Ta offers higher melting point, strength, and superior wear and corrosion resistance compared to metals like Nb. Cu/Ta nano-bilayer films are extensively used in the electronics industry for semiconductors, microelectronic devices, optical systems, and magnetic applications. However, the presence of interfaces and the distinct deformation responses of the Cu and Ta layers during processing, fabrication, and service conditions make mechanical deformation and subsequent failure inevitable, potentially compromising the performance of microscale devices. Therefore, understanding the deformation mechanisms and enhancing the mechanical strength of Cu/Ta nano-bilayer films at the microscopic scale is essential. In this study, molecular dynamics simulations were employed to investigate the tensile behavior and deformation mechanisms of Cu/Ta nano-bilayer films. In addition, the effects of Al and W doping in the Cu layer on the deformation behavior were analyzed. The results indicate that tensile loading direction significantly influences the plastic deformation mode. When the bilayer films were stretched parallel to the interface, both Cu and Ta layers exhibited sequential plastic deformation. In contrast, when the loading was applied perpendicular to the interface, only the Cu layer deformed plastically, while the Ta layer remained elastically constrained throughout. Doping with Al or W atoms enhanced the overall hardness and yield strength of the nano-bilayer films. Furthermore, W doping induced stacking faults in both loading directions when stretched parallel to the interface, and a martensitic transformation from fcc to bcc structure occurred in the Cu layer under perpendicular tension.

Key words: Cu/Ta interface    stretching deformation    alloying strengthening    molecular dynamics
收稿日期: 2024-09-11     
ZTFLH:  TG146.1  
基金资助:国家科技重大专项项目(2025ZD0618600);西安市科技计划项目(24ZDCYJSGG0050)
通讯作者: 史俊勤,junqin.shi@nwpu.edu.cn,主要从事材料变形及摩擦磨损行为的研究
Corresponding author: SHI Junqin, associate professor, Tel: (029)88460311, E-mail: junqin.shi@nwpu.edu.cn
作者简介: 石腾龙,男,1999年生,硕士
图1  Cu/Ta、Cu95Al5/Ta和Cu95W5/Ta纳米双层膜的分子动力学模型及其界面失配位错结构
图2  各模型沿平行于界面方向(X方向)和垂直于界面方向(Z方向)拉伸时的应力-应变曲线
图3  Cu/Ta双层膜沿X方向拉伸过程中不同应变下的晶体结构
图4  Cu95Al5/Ta双层膜沿X方向拉伸过程中不同应变下的晶体结构
图5  Cu95W5/Ta双层膜沿X方向拉伸过程中不同应变下的晶体结构
图6  各模型沿X方向拉伸过程中Cu层和Ta层不同晶体结构原子的数量变化曲线
图7  Cu/Ta、Cu95Al5/Ta和Cu95W5/Ta双层膜沿X方向拉伸过程中不同应变下的位错结构
图8  各模型沿X方向拉伸过程中Cu层和Ta层位错线长度的变化曲线
图9  Cu/Ta双层膜沿Z方向拉伸过程中不同应变下的晶体结构
图10  Cu95Al5/Ta双层膜沿Z方向拉伸过程中不同应变下的晶体结构
图11  Cu95W5/Ta双层膜沿Z方向拉伸过程中不同应变下的晶体结构
图12  各模型初始时刻内部缺陷示意图及沿Z方向拉伸时位错结构产生示意图
图13  各模型沿Z方向拉伸过程中不同类型原子数目和位错线长度变化曲线
[1] Chen H B. Fabrication and property of Ta-based diffusion barrier for Cu interconnection in new generation IC [D]. Changsha: Central South University, 2007
[1] 陈海波. 新一代集成电路Cu互连用Ta基扩散阻挡层的制备及特性研究 [D]. 长沙: 中南大学, 2007
[2] Holloway K, Fryer P M, Cabral Jr C, et al. Tantalum as a diffusion barrier between copper and silicon: Failure mechanism and effect of nitrogen additions [J]. J. Appl. Phys., 1992, 71: 5433
doi: 10.1063/1.350566
[3] Fullwood D T, Niezgoda S R, Adams B L, et al. Microstructure sensitive design for performance optimization [J]. Prog. Mater. Sci., 2010, 55: 477
doi: 10.1016/j.pmatsci.2009.08.002
[4] Mondal S, Polley D, Pattabi A, et al. Single-shot switching in Tb/Co-multilayer based nanoscale magnetic tunnel junctions [J]. J. Magn. Magn. Mater., 2023, 581: 170960
doi: 10.1016/j.jmmm.2023.170960
[5] Sakhonenkov S S, Filatova E O. Nanoscale W/Be multilayers: Intermixing during magnetron sputtering deposition and effect of heat treatment [J]. Appl. Surf. Sci., 2022, 571: 151265
doi: 10.1016/j.apsusc.2021.151265
[6] Tran A S, Fang T H. Dislocation interaction and fracture of Cu/Ta bilayer interfaces [J]. Phys. Scr., 2019, 94: 095402
[7] Feng X T, Lin Z J, Xin K, et al. The deformation mechanisms and mechanical properties of Cu/Fe multilayer during compression process [J]. J. Mater. Res., 2021, 36: 3203
doi: 10.1557/s43578-021-00333-z
[8] Zhang R F, Wang J, Beyerlein I J, et al. Dislocation nucleation mechanisms from fcc/bcc incoherent interfaces [J]. Scr. Mater., 2011, 65: 1022
doi: 10.1016/j.scriptamat.2011.09.008
[9] Chen Y, Li N, Hoagland R G, et al. Effects of three-dimensional Cu/Nb interfaces on strengthening and shear banding in nanoscale metallic multilayers [J]. Acta Mater., 2020, 199: 593
doi: 10.1016/j.actamat.2020.08.019
[10] Wang Y, Zhu X Y, Liu G M, et al. Strain rate sensitivity of Cu/Ni and Cu/Nb nanoscale multilayers [J]. Acta Metall. Sin., 2017, 53: 183
[10] 王 尧, 朱晓莹, 刘贵民 等. Cu/Ni和Cu/Nb纳米多层膜的应变率敏感性 [J]. 金属学报, 2017, 53: 183
[11] Zhang R F, Wang J, Beyerlein I J, et al. Atomic-scale study of nucleation of dislocations from fcc-bcc interfaces [J]. Acta Mater., 2012, 60: 2855
doi: 10.1016/j.actamat.2012.01.050
[12] Lu L, Huang C, Pi W L, et al. Molecular dynamics simulation of effects of interface imperfections and modulation periods on Cu/Ta multilayers [J]. Comp. Mater. Sci., 2018, 143: 63
doi: 10.1016/j.commatsci.2017.10.034
[13] Shi T L, Xu L L, Chen J, et al. Influence of grain boundary and twin boundary on the stretching deformation behaviors of Cu/Ta interface material [J]. Mater. Today Commun., 2024, 39: 108633
[14] Tu A D, Teng C Y, Wang H, et al. Molecular dynamics simulation of the structure and deformation behavior of γ/α2 interface in TiAl alloys [J]. Acta Metall. Sin., 2019, 55: 291
[14] 涂爱东, 滕春禹, 王 皞 等. Ti-Al合金γ/α2界面结构及拉伸变形行为的分子动力学模拟 [J]. 金属学报, 2019, 55: 291
doi: 10.11900/0412.1961.2018.00182
[15] Karimzadeh A, Rouhaghdam A S, Aliofkhazraei M, et al. Sliding wear behavior of Ni-Co-P multilayer coatings electrodeposited by pulse reverse method [J]. Tribol. Int., 2020, 141: 105914
doi: 10.1016/j.triboint.2019.105914
[16] Major L, Lackner J M, Kot M, et al. Nanostructural aspects of the wear process of multilayer tribological coatings [J]. Tribol. Int., 2020, 151: 106411
doi: 10.1016/j.triboint.2020.106411
[17] Shi J Q, Li L L, Wang J Y, et al. Alloy strengthening toward improving mechanical and tribological performances of Cu x Ni100 - x /Ta nano multilayer materials [J]. Tribol. Int., 2023, 190: 109039
doi: 10.1016/j.triboint.2023.109039
[18] Bai Z W, Ding Z G, Zhou A L, et al. Molecular dynamics simulation of thermo-kinetics of tensile deformation of α-Fe single crystal [J]. Acta Metall. Sin., 2024, 60: 848
[18] 柏智文, 丁志刚, 周爱龙 等. α-Fe单晶拉伸变形热-动力学的分子动力学模拟 [J]. 金属学报, 2024, 60: 848
doi: 10.11900/0412.1961.2022.00606
[19] Zhang J Y, Qu Q M, Wang Y Q, et al. Research progress on irradiation effects and mechanical properties of metal/high-entropy alloy nanostructured multilayers [J]. Acta Metall. Sin., 2022, 58: 1371
doi: 10.11900/0412.1961.2022.00113
[19] 张金钰, 屈启蒙, 王亚强 等. 金属/高熵合金纳米多层膜的力学性能及其辐照效应研究进展 [J]. 金属学报, 2022, 58: 1371
doi: 10.11900/0412.1961.2022.00113
[20] Abraham F F. Computational statistical mechanics methodology, applications and supercomputing [J]. Adv. Phys., 1986, 35: 1
doi: 10.1080/00018738600101851
[21] Stukowski A. Structure identification methods for atomistic simulations of crystalline materials [J]. Modell. Simul. Mater. Sci. Eng., 2012, 20: 045021
[22] Choudhuri D, Srinivasan S G, Mishra R S. Deformation of lamellar FCC-B2 nanostructures containing Kurdjumov-Sachs interfaces: Relation between interfacial structure and plasticity [J]. Int. J. Plast., 2020, 125: 191
doi: 10.1016/j.ijplas.2019.09.014
[23] Zhou Q, Ren Y, Du Y, et al. Cracking and toughening mechanisms in nanoscale metallic multilayer films: A brief review [J]. Appl. Sci., 2018, 8: 1821
doi: 10.3390/app8101821
[24] Mendelev M I, Han S, Srolovitz D J, et al. Development of new interatomic potentials appropriate for crystalline and liquid iron [J]. Philos. Mag., 2003, 83: 3977
doi: 10.1080/14786430310001613264
[25] Wei M Z, Cao Z H, Shi J, et al. Anomalous plastic deformation in nanoscale Cu/Ta multilayers [J]. Mater. Sci. Eng., 2014, A598: 355
[26] Zhao X, Lu C, Tieu A K, et al. Deformation mechanisms and slip-twin interactions in nanotwinned body-centered cubic iron by molecular dynamics simulations [J]. Comput. Mater. Sci., 2018, 147: 34
[27] An M R, Song H Y, Deng Q, et al. Influence of interface with mismatch dislocations on mechanical properties of Ti/Al nanolaminate [J]. J. Appl. Phys., 2019, 125: 165307
doi: 10.1063/1.5085455
[28] Liu Y, Yang K M, Hay J, et al. The effect of coherent interface on strain-rate sensitivity of highly textured Cu/Ni and Cu/V multilayers [J]. Scr. Mater., 2019, 162: 33
doi: 10.1016/j.scriptamat.2018.10.021
[29] Yin F X, Zhao Y Z, Yu S Y, et al. Molecular dynamics studies on the interface evolution characteristics and deformation mechanisms of Cu/Al multilayers during compression process [J]. J. Appl. Phys., 2019, 125: 025112
[30] Eder S J, Rodríguez Ripoll M, Cihak-Bayr U, et al. Unraveling and mapping the mechanisms for near-surface microstructure evolution in CuNi alloys under sliding [J]. ACS Appl. Mater. Interfaces, 2020, 12: 32197
doi: 10.1021/acsami.0c09302
[31] Wang J Y, Shi J Q, Lu Y, et al. Deformation evolution of Cu/Ta nanoscale multilayer during nanoindentation by a molecular dynamics study [J]. Surf. Coat. Technol., 2022, 441: 128562
doi: 10.1016/j.surfcoat.2022.128562
[32] Shi J Q, Wang J Y, Yi X B, et al. Nanoscratching-induced plastic deformation mechanism and tribology behavior of Cu/Ta bilayer and multilayer by a molecular dynamics study [J]. Appl. Surf. Sci., 2022, 586: 152775
doi: 10.1016/j.apsusc.2022.152775
[33] Wang T, Jin L, Shi T L, et al. Effect of Al and W atom doping on the deformation mechanism and tribological properties of Cu95 X5/Ta nanobilayer by molecular dynamics simulation [J]. Tribol. Int., 2025, 210: 110818
doi: 10.1016/j.triboint.2025.110818
[34] Faken D, Jónsson H. Systematic analysis of local atomic structure combined with 3D computer graphics [J]. Comput. Mater. Sci., 1994, 2: 279
doi: 10.1016/0927-0256(94)90109-0
[35] Stukowski A, Bulatov V V, Arsenlis A. Automated identification and indexing of dislocations in crystal interfaces [J]. Modell. Simul. Mater. Sci. Eng., 2012, 20: 085007
[36] Fu E G, Li N, Misra A, et al. Mechanical properties of sputtered Cu/V and Al/Nb multilayer films [J]. Mater. Sci. Eng., 2008, A493: 283
[37] Bain E C. Factors affecting the inherent hardenability of steel [J]. J. Heat Treat., 1979, 1: 57
[38] Burgers W G. On the process of transition of the cubic-body-centered modification into the hexagonal-close-packed modification of zirconium [J]. Physica, 1934, 1: 561
doi: 10.1016/S0031-8914(34)80244-3
[39] Bertin N, Carson R, Bulatov V V, et al. Crystal plasticity model of BCC metals from large-scale MD simulations [J]. Acta Mater., 2023, 260: 119336
doi: 10.1016/j.actamat.2023.119336
[1] 江国龙, 周霞. 超声辅助下Mg/Mg-Zn-Al钎焊界面行为的分子动力学模拟[J]. 金属学报, 2026, 62(2): 372-382.
[2] 袁航, 张燕云, 王聪. 第一性原理分子动力学研究MnO对埋弧焊剂导电机制的影响[J]. 金属学报, 2026, 62(1): 191-202.
[3] 周婷婷, 赵福祺, 周洪强, 张凤国, 殷建伟. 含He泡液态金属铝的动态拉伸断裂机制与损伤模型[J]. 金属学报, 2025, 61(4): 643-652.
[4] 王书成, 彭平. Al液滴等温结晶的形核特征分析[J]. 金属学报, 2025, 61(12): 1925-1932.
[5] 柏智文, 丁志刚, 周爱龙, 侯怀宇, 刘伟, 刘峰. α-Fe单晶拉伸变形热-动力学的分子动力学模拟[J]. 金属学报, 2024, 60(6): 848-856.
[6] 孟子凯, 孟智超, 高长源, 郭辉, 陈汉森, 陈刘涛, 徐东生, 杨锐. 不同条件下纳米晶 α-Zr蠕变行为的分子动力学模拟[J]. 金属学报, 2024, 60(5): 699-712.
[7] 刘瑞, 于治, 赵洋, 李晓齐, 喻海龙, 何娟, 聂鹏程, 王春雨, 邰凯平, 刘畅. 柔性、可拉伸变形微型热电器件的设计与集成[J]. 金属学报, 2024, 60(3): 348-356.
[8] 任军强, 邵珊, 王启, 卢学峰, 薛红涛, 汤富领. 含氧纳米多晶 α-Ti拉伸力学性能与变形机制的分子动力学模拟[J]. 金属学报, 2024, 60(2): 220-230.
[9] 刘仕, 黄佳玮, 武静. 机器学习势在铁电材料研究中的应用[J]. 金属学报, 2024, 60(10): 1312-1328.
[10] 陈名毅, 胡俊伟, 余耀辰, 牛海洋. 机器学习分子动力学辅助材料凝固形核研究进展[J]. 金属学报, 2024, 60(10): 1329-1344.
[11] 李志尚, 赵龙, 宗洪祥, 丁向东. 机器学习型分子力场在金属材料相变与变形领域的研究进展[J]. 金属学报, 2024, 60(10): 1388-1404.
[12] 田妮, 石旭, 刘威, 刘春城, 赵刚, 左良. 预拉伸变形对欠时效7N01铝合金板材疲劳断裂的影响[J]. 金属学报, 2022, 58(6): 760-770.
[13] 李海勇, 李赛毅. 纯Al <111>对称倾斜晶界迁移行为温度相关性的分子动力学研究[J]. 金属学报, 2022, 58(2): 250-256.
[14] 梁晋洁, 高宁, 李玉红. 体心立方Fe中微裂纹与间隙型位错环相互作用的分子动力学模拟[J]. 金属学报, 2020, 56(9): 1286-1294.
[15] 李源才, 江五贵, 周宇. 纳米孔洞对单晶/多晶Ni复合体拉伸性能的影响[J]. 金属学报, 2020, 56(5): 776-784.