| Co、Si共掺杂调控Ni-Mn-Ti合金马氏体相变、磁性能和力学性能的第一性原理研究 |
刘丹1,2, 白静1,2,3( ), 章羽1, 郭珂良1, 刘新2, 左良1 |
1 东北大学 材料各向异性与织构教育部重点实验室 沈阳 110819 2 东北大学秦皇岛分校 资源与材料学院 秦皇岛 066004 3 东北大学秦皇岛分校 河北省电介质与电解质功能材料重点实验室 秦皇岛 066004 |
|
| First-Principles Study on the Regulation of Martensitic Transformation and Magnetic and Mechanical Properties of Ni-Mn-Ti Alloy via Co and Si Codoping |
LIU Dan1,2, BAI Jing1,2,3( ), ZHANG Yu1, GUO Keliang1, LIU Xin2, ZUO Liang1 |
1 Key Laboratory for Anisotropy and Texture of Materials Ministry of Education, Northeastern University, Shenyang 110819, China 2 School of Resources and Materials, Northeastern University at Qinhuangdao, Qinhuangdao 066004, China 3 Key Laboratory of Dielectric and Electrolyte Functional Material Hebei Province, Northeastern University at Qinhuangdao, Qinhuangdao 066004, China |
引用本文:
刘丹, 白静, 章羽, 郭珂良, 刘新, 左良. Co、Si共掺杂调控Ni-Mn-Ti合金马氏体相变、磁性能和力学性能的第一性原理研究[J]. 金属学报, 2026, 62(7): 1310-1322.
Dan LIU,
Jing BAI,
Yu ZHANG,
Keliang GUO,
Xin LIU,
Liang ZUO.
First-Principles Study on the Regulation of Martensitic Transformation and Magnetic and Mechanical Properties of Ni-Mn-Ti Alloy via Co and Si Codoping[J]. Acta Metall Sin, 2026, 62(7): 1310-1322.
| [1] |
Moya X, Kar-Narayan S, Mathur N D. Caloric materials near ferroic phase transitions [J]. Nat. Mater., 2014, 13: 439
doi: 10.1038/nmat3951
pmid: 24751772
|
| [2] |
Lloveras P, Stern-Taulats E, Barrio M, et al. Giant barocaloric effects at low pressure in ferrielectric ammonium sulphate [J]. Nat. Commun., 2015, 6: 8801
doi: 10.1038/ncomms9801
pmid: 26607989
|
| [3] |
Kainuma R, Imano Y, Ito W, et al. Magnetic-field-induced shape recovery by reverse phase transformation [J]. Nature, 2006, 439: 957
doi: 10.1038/nature04493
|
| [4] |
Yu S Y, Cao Z X, Ma L, et al. Realization of magnetic field-induced reversible martensitic transformation in NiCoMnGa alloys [J]. Appl. Phys. Lett., 2007, 91: 102507
doi: 10.1063/1.2783188
|
| [5] |
Wei Z Y, Liu E K, Li Y, et al. Magnetostructural martensitic transformations with large volume changes and magneto-strains in all-d-metal Heusler alloys [J]. Appl. Phys. Lett., 2016, 109: 071904
|
| [6] |
Wei Z Y, Liu E K, Chen J H, et al. Realization of multifunctional shape-memory ferromagnets in all-d-metal Heusler phases [J]. Appl. Phys. Lett., 2015, 107: 022406
|
| [7] |
Huang Y J, Hu Q D, Bruno N M, et al. Giant elastocaloric effect in directionally solidified Ni-Mn-In magnetic shape memory alloy [J]. Scr. Mater., 2015, 105: 42
doi: 10.1016/j.scriptamat.2015.04.024
|
| [8] |
Xiao F, Fukuda T, Jin X J, et al. Elastocaloric effect associated with different types of martensitic transformations: Typical first-order and weak first-order ones [J]. Phys. Status Solidi, 2018, 255B: 1700246
|
| [9] |
Sutou Y, Imano Y, Koeda N, et al. Magnetic and martensitic transformations of NiMnX (X = In, Sn, Sb) ferromagnetic shape memory alloys [J]. Appl. Phys. Lett., 2004, 85: 4358
doi: 10.1063/1.1808879
|
| [10] |
Cong D Y, Xiong W X, Planes A, et al. Colossal elastocaloric effect in ferroelastic Ni-Mn-Ti alloys [J]. Phys. Rev. Lett., 2019, 122: 255703
doi: 10.1103/PhysRevLett.122.255703
|
| [11] |
Wei Z Y, Sun W, Shen Q, et al. Elastocaloric effect of all-d-metal Heusler NiMnTi(Co) magnetic shape memory alloys by digital image correlation and infrared thermography [J]. Appl. Phys. Lett., 2019, 114: 101903
doi: 10.1063/1.5077076
|
| [12] |
Liu S L, Xuan H C, Cao T, et al. Magnetocaloric and elastocaloric effects in all-d-Metal Ni37Co9Fe4Mn35Ti15 magnetic shape memory alloy [J]. Phys. Status Solidi, 2019, 216A: 1900563
|
| [13] |
Yan H L, Wang L D, Liu H X, et al. Giant elastocaloric effect and exceptional mechanical properties in an all-d-metal Ni-Mn-Ti alloy: experimental and ab-initio studies [J]. Mater. Des., 2019, 184: 108180
doi: 10.1016/j.matdes.2019.108180
|
| [14] |
Wei Z Y, Shen Y, Zhang Z, et al. Low-pressure-induced giant barocaloric effect in an all-d-metal Heusler Ni35.5Co14.5Mn35Ti15 magnetic shape memory alloy [J]. APL Mater., 2020, 8: 051101
|
| [15] |
Guan Z Q, Bai J, Zhang Y, et al. Ultrahigh cyclic stability and giant elastocaloric effect in directionally solidified (Ni50Mn28Fe2.5-Ti19.5)99.4B0.6 alloy [J]. Scr. Mater., 2023, 229: 115353
doi: 10.1016/j.scriptamat.2023.115353
|
| [16] |
Taubel A, Beckmann B, Pfeuffer L, et al. Tailoring magnetocaloric effect in all-d-metal Ni-Co-Mn-Ti Heusler alloys: A combined experimental and theoretical study [J]. Acta Mater., 2020, 201: 425
doi: 10.1016/j.actamat.2020.10.013
|
| [17] |
Liu K, Han X Q, Yu K, et al. Magnetic-field-induced metamagnetic reverse martensitic transformation and magnetocaloric effect in all-d-metal Ni36.0Co14.0Mn35.7Ti14.3 alloy ribbons [J]. Intermetallics, 2019, 110: 106472
doi: 10.1016/j.intermet.2019.106472
|
| [18] |
Neves Bez H, Pathak A K, Biswas A, et al. Giant enhancement of the magnetocaloric response in Ni-Co-Mn-Ti by rapid solidification [J]. Acta Mater., 2019, 173: 225
doi: 10.1016/j.actamat.2019.05.004
|
| [19] |
Huang S Y, Qin L, Li Y, et al. The study of martensitic transformation and magnetocaloric effect in rare earth Y-doped all-d-metal Ni-Co-Mn-Ti Heusler alloys [J]. Mater. Lett., 2021, 302: 130376
doi: 10.1016/j.matlet.2021.130376
|
| [20] |
Wang J M, Yu Q, Xu K Y, et al. Large room-temperature elastocaloric effect of Ni57Mn18Ga21In4 alloy undergoing a magnetostructural coupling transition [J]. Scr. Mater., 2017, 130: 148
doi: 10.1016/j.scriptamat.2016.11.024
|
| [21] |
Recarte V, Pérez-Landazábal J I, Sánchez-Alarcos V, et al. Entropy change linked to the martensitic transformation in metamagnetic shape memory alloys [J]. Acta Mater., 2012, 60: 3168
doi: 10.1016/j.actamat.2012.02.022
|
| [22] |
Recarte V, Pérez-Landazábal J I, Gómez-Polo C, et al. Vibrational and magnetic contributions to the entropy change associated with the martensitic transformation of Ni-Fe-Ga ferromagnetic shape memory alloys [J]. J. Phys., 2010, 22: 416001
|
| [23] |
Liu K, Ma S C, Ma C C, et al. Martensitic transformation and giant magneto-functional properties in all-d-metal Ni-Co-Mn-Ti alloy ribbons [J]. J. Alloys Compd., 2019, 790: 78
doi: 10.1016/j.jallcom.2019.03.173
|
| [24] |
Guan Z Q, Jiang X J, Gu J L, et al. Large magnetocaloric effect and excellent mechanical properties near room temperature in Ni-Co-Mn-Ti non-textured polycrystalline alloys [J]. Appl. Phys. Lett., 2021, 119: 051904
|
| [25] |
Li Q S, Liang Z Y, Sun K C, et al. Martensitic transformation and magnetic properties of Heusler alloys Co-V-(Al, Ga, In) [J]. Comput. Mater. Sci., 2019, 168: 11
doi: 10.1016/j.commatsci.2019.05.055
|
| [26] |
Aznar A, Gràcia-Condal A, Planes A, et al. Giant barocaloric effect in all-d-metal Heusler shape memory alloys [J]. Phys. Rev. Mater., 2019, 3: 044406
|
| [27] |
Sivaprakash P, Arumugam S, Esakki Muthu S, et al. Correlation of magnetocaloric effect through magnetic and electrical resistivity on Si doped Ni-Mn-In Heusler melt spun ribbon [J]. Intermetallics, 2021, 137: 107285
doi: 10.1016/j.intermet.2021.107285
|
| [28] |
Li Z Z, Li Z B, Lu Y Z, et al. Enhanced elastocaloric effect and refrigeration properties in a Si-doped Ni-Mn-In shape memory alloy [J]. J. Mater. Sci. Technol., 2022, 117: 167
doi: 10.1016/j.jmst.2021.11.051
|
| [29] |
Zhang R C, Qian M F, Zhang X X, et al. Magnetocaloric effect with low magnetic hysteresis loss in ferromagnetic Ni-Mn-Sb-Si alloys [J]. J. Magn. Magn. Mater., 2017, 428: 464
doi: 10.1016/j.jmmm.2016.12.138
|
| [30] |
Wójcik A, Maziarz W, Szczerba M, et al. Structure and inverse magnetocaloric effect in Ni-Co-Mn-Sn(Si) Heusler alloys [J]. Intermetallics, 2018, 100: 88
doi: 10.1016/j.intermet.2018.06.004
|
| [31] |
Venkatesan S, Kavita S, Perumal S. Structure stability driven large magnetocaloric response in Ni-Co-Mn-In-Si Heusler alloy [J]. Ceram. Int., 2022, 48: 29059
doi: 10.1016/j.ceramint.2022.04.300
|
| [32] |
Bai J, Shi S F, Wang J L, et al. First-principles calculations of phase stability and magnetic properties of Ni-Mn-Ga-Ti ferromagnetic shape memory alloys [J]. Acta Metall. Sin., 2019, 55: 369
|
| [32] |
白 静, 石少锋, 王锦龙 等. Ni-Mn-Ga-Ti铁磁形状记忆合金的相稳定性和磁性能的第一性原理计算 [J]. 金属学报, 2019, 55: 369
|
| [33] |
Guan Z Q, Bai J, Zhang Y, et al. Revealing essence of magnetostructural coupling of Ni-Co-Mn-Ti alloys by first-principles calculations and experimental verification [J]. Rare Met., 2022, 41: 1933
doi: 10.1007/s12598-021-01947-2
|
| [34] |
Guan Z Q, Bai J, Zhang Y, et al. Ni-Co-Mn-Ti-B high performance multiferroic phase transformation material: Simultaneous modulation of mechanical properties and successive caloric effects by B doping [J]. Mater. Today Phys., 2023, 36: 101183
|
| [35] |
Zhang Y, Bai J, Guo K L, et al. An alloying strategy for tuning magnetism, thermal hysteresis, and mechanical properties in Ni-Mn-Sn-based Heusler alloys[J]. J. Alloys Compd., 2024, 979: 173593
doi: 10.1016/j.jallcom.2024.173593
|
| [36] |
Liang X Z, Bai J, Wang J L, et al. Effect of Co doping on martensitic transformation and magnetic properties of Ni50Mn35. 4In14. 6 alloy by first-principles calculations [J]. J. Alloys Compd., 2019, 804: 111
doi: 10.1016/j.jallcom.2019.06.380
|
| [37] |
Wei Z Y. Design of magnetostructural coupling and magnetic martensitic transformations in hexagonal MM'X and all-d-metal Heusler shape memory alloys [D]. Beijing: University of Chinese Academy of Sciences (Institute of Physics), 2017.
|
| [37] |
魏志阳. MM'X合金和全d-metal Heusler合金中的磁相变设计 [D]. 北京: 中国科学院大学(中国科学院物理研究所), 2017
|
| [38] |
Kresse G, Joubert D. From ultrasoft pseudopotentials to the projector augmented-wave method [J]. Phys. Rev., 1999, 59B: 1758
|
| [39] |
Perdew J P, Burke K, Ernzerhof M. Generalized gradient approximation made simple [J]. Phys. Rev. Lett., 1996, 77: 3865
doi: 10.1103/PhysRevLett.77.3865
pmid: 10062328
|
| [40] |
Monkhorst H J, Pack J D. Special points for Brillouin-zone integrations [J]. Phys. Rev., 1976, 13B: 5188
|
| [41] |
Guan Z Q, Bai J, Gu J L, et al. First-principles investigation of B2 partial disordered structure, martensitic transformation, elastic and magnetic properties of all-d-metal Ni-Mn-Ti Heusler alloys [J]. J. Mater. Sci. Technol., 2021, 68: 103
doi: 10.1016/j.jmst.2020.08.002
|
| [42] |
Pathak A K, Dubenko I, Stadler S, et al. The effect of partial substitution of In by Si on the phase transitions and respective magnetic entropy changes of Ni50Mn35In15 Heusler alloy [J]. J. Phys., 2008, 41D: 202004
|
| [43] |
Li Z B, Dong S Y, Li Z Z, et al. Giant low-field magnetocaloric effect in Si alloyed Ni-Co-Mn-In alloys [J]. Scr. Mater., 2019, 159: 113
doi: 10.1016/j.scriptamat.2018.09.029
|
| [44] |
Esakki Muthu S, Kanagaraj M, Singh S, et al. Hydrostatic pressure effects on martensitic transition, magnetic and magnetocaloric effect in Si doped Ni-Mn-Sn Heusler alloys [J]. J. Alloys Compd., 2014, 584: 175
doi: 10.1016/j.jallcom.2013.09.007
|
| [45] |
Ozdemir Kart S, Cagın. T. Elastic properties of Ni2MnGa from first-principles calculations [J]. J. Alloys Compd., 2010, 508: 177
doi: 10.1016/j.jallcom.2010.08.039
|
| [46] |
Zhao X G, Yang J L, Wang X E, et al. Magnetocaloric and electrical properties in annealed Si-doped Ni-Mn-In Heusler alloy ribbons [J]. IEEE Trans. Magn., 2011, 47: 2455
doi: 10.1109/TMAG.20
|
| [47] |
Glavatskyy I, Glavatska N, Söderberg O, et al. Transformation temperatures and magnetoplasticity of Ni-Mn-Ga alloyed with Si, In, Co or Fe [J]. Scr. Mater., 2006, 54: 1891
doi: 10.1016/j.scriptamat.2006.02.010
|
| [48] |
Xiong C C, Bai J, Li Y S, et al. First-principles investigation on phase stability, elastic and magnetic properties of boron doping in Ni-Mn-Ti alloy [J]. Acta Metall. Sin. (Engl. Lett.), 2022, 35: 1175
doi: 10.1007/s40195-021-01360-9
|
| [49] |
Song Y T, Chen X, Dabade V, et al. Enhanced reversibility and unusual microstructure of a phase-transforming material [J]. Nature, 2013, 502: 85
doi: 10.1038/nature12532
|
| [50] |
Cui J, Chu Y S, Famodu O O, et al. Combinatorial search of thermoelastic shape-memory alloys with extremely small hysteresis width [J]. Nat. Mater., 2006, 5: 286
pmid: 16518396
|
| [51] |
Li B, Liu Z P, Li D, et al. Large reversible multicaloric effects over a broad refrigeration temperature range in Co and B co-doped Ni-Mn-Ti alloys [J]. Mater. Sci. Eng., 2024, A896: 146260
|
| [52] |
Liu D, Gou J M, Xu Z T, et al. Atomic scale understanding the periodic modulation in ferroelastic alloy Ni-Mn-Ti [J]. Acta Mater., 2023, 248: 118768
doi: 10.1016/j.actamat.2023.118768
|
| [53] |
Li G J, Liu E K, Wu G H. d-d hybridization controlled large-volume-change martensitic phase transition in Ni-Mn-Ti-based all-d-metal Heusler compounds [J]. J. Alloys Compd., 2022, 923: 166369
doi: 10.1016/j.jallcom.2022.166369
|
| [54] |
Wang J L, Bai J, Liu D, et al. Understanding the magneto-structural coupling of Ni50Mn35.4In14.6 alloy from first-principles calculations [J]. J. Magn. Magn. Mater., 2019, 488: 165339
doi: 10.1016/j.jmmm.2019.165339
|
| [55] |
Ghosh S, Ghosh S. Role of composition, site ordering, and magnetic structure for the structural stability of off-stoichiometric Ni2MnSb alloys with excess Ni and Mn [J]. Phys. Rev., 2019, 99B: 064112
|
| [56] |
Liang X Z, Bai J, Gu J L, et al. Probing martensitic transformation, kinetics, elastic and magnetic properties of Ni2 - x Mn1.5In0.5Co x alloys [J]. J. Mater. Sci. Technol., 2020, 44: 31
doi: 10.1016/j.jmst.2020.01.034
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|