Please wait a minute...
金属学报  2026, Vol. 62 Issue (10): 1727-1736    DOI: 10.11900/0412.1961.2024.00347
  研究论文 本期目录 | 过刊浏览 |
Ti掺杂的SmFe12 基纳米晶永磁合金物相组成和组织性能
程锋, 吕皓(), 刘雪梅, 宋晓艳()
北京工业大学 材料循环低碳再生全国重点实验室 新型功能材料教育部重点实验室材料科学与工程学院 北京 100124
Phase Constitution, Microstructure, and Properties of Ti-Doped SmFe12-Based Nanocrystalline Permanent Magnetic Alloys
CHENG Feng, LU Hao(), LIU Xuemei, SONG Xiaoyan()
State Key Laboratory of Materials Low-Carbon Recycling, Key Laboratory of Advanced Functional Materials, MOE, College of Materials Science and Engineering, Beijing University of Technology, Beijing 100124, China
引用本文:

程锋, 吕皓, 刘雪梅, 宋晓艳. Ti掺杂的SmFe12 基纳米晶永磁合金物相组成和组织性能[J]. 金属学报, 2026, 62(10): 1727-1736.
Feng CHENG, Hao LU, Xuemei LIU, Xiaoyan SONG. Phase Constitution, Microstructure, and Properties of Ti-Doped SmFe12-Based Nanocrystalline Permanent Magnetic Alloys[J]. Acta Metall Sin, 2026, 62(10): 1727-1736.

全文: PDF(2107 KB)   HTML
摘要: 

随着稀土永磁材料需求量的增加和稀土资源的过度开发,ThMn12型SmFe12基合金得到广泛关注。然而,SmFe12相结构稳定性差,室温下会分解生成α-Fe相而大幅降低合金的矫顽力。本工作采用合金化、纳米化与热处理协同调控SmFe12基块体合金物相组成和微观组织的方法提高合金矫顽力。通过优化Ti掺杂量,得到了接近单相的SmFe12 - x Ti x 铸态合金,合金具有高饱和磁化强度,但是其矫顽力较低。利用高能球磨法制备了SmFe11Ti1合金的非晶粉末,通过快速热压烧结使非晶粉末晶化,得到了具有高比例SmFe12相的纳米晶SmFe12基烧结磁体。匹配高能球磨与快速热压烧结工艺使烧结磁体的矫顽力相比合金铸锭得到了大幅度提升。通过优化热处理工艺调控合金的晶粒尺寸和物相组成,热处理后合金的主相依然为SmFe12相,晶粒尺寸更接近SmFe12的单畴尺寸,从而进一步提高了合金的矫顽力。

关键词 : SmFe12基合金,  纳米晶,  合金化,  相稳定性,  矫顽力    
Abstract:

With the growing demand for rare-earth permanent magnetic materials and the overexploitation of rare-earth resources, ThMn12-type SmFe12-based alloys have attracted significant research interest. However, the SmFe12 phase exhibits poor structural stability and decomposes into the α-Fe phase at room temperature, drastically reducing the alloy's coercivity. The challenge of developing bulk SmFe12-based alloys with high coercivity has hindered their application as permanent magnetic materials. This study optimized Ti doping concentrations to achieve nearly single-phase SmFe12-based alloys. The SmFe12-based alloy ingot demonstrated high saturation magnetization but low coercivity. Amorphous SmFe11Ti1 alloy powder was prepared via high-energy ball milling, followed by rapid hot-pressing sintering, which induced crystallization and yielded nanocrystalline SmFe12-based sintered magnets with high phase purity. The combination of high-energy ball milling and rapid hot-pressing sintering significantly enhanced the coercivity of the sintered magnets compared to the original ingot. By optimizing the heat treatment process, the grain size and phase constitution of the alloy were effectively controlled. After heat treatment, the main phase remained SmFe12, with grain sizes approaching the single-domain dimension of SmFe12, leading to further coercivity enhancement. The approach proposed in this study—synergistically tailoring the phase constitution and microstructure of SmFe12-based alloys through alloying, nanocrystallization, and heat treatment—offers a new pathway for developing high-coercivity SmFe12-based magnets.

Key words: SmFe12-based alloy    nanocrystalline    alloying    phase stability    coercivity
收稿日期: 2024-10-18     
ZTFLH:  TG146.4  
基金资助:国家重点研发计划项目(2021YFB3501502);国家重点研发计划项目(2021YFB3501504)
通讯作者: 吕皓,haolu@bjut.edu.cn,主要从事基于多尺度计算的合金新材料设计开发研究;
宋晓艳,xysong@bjut.edu.cn,主要从事金属纳米材料与计算材料学研究
Corresponding author: LU Hao, Tel: (010)67392829, E-mail: haolu@bjut.edu.cn;
SONG Xiaoyan, professor, Tel: (010)67392311, E-mail: xysong@bjut.edu.cn
作者简介: 程锋,男,2000年生,硕士生
图1  SmFe12 - x Ti x (x = 0、0.5、1、1.5和2)铸锭的XRD谱及铸态合金的SEM-BSE像
图2  SmFe12 - x Ti x (x = 0、0.5、1、1.5和2)铸态合金第一象限和第二象限部分的磁滞回线
图3  不同高能球磨时间下SmFe11Ti1粉末的XRD谱及球磨4 h后粉末的HRTEM像和SAED花样
图4  粉末球磨时间对烧结合金物相组成和磁性能的影响
图5  快速热压烧结温度对SmFe11Ti1合金的物相组成和磁性能的影响
Sintering temperature / oCHc / (kA⋅m-1)Js / TJr / Tρ / (g⋅cm-3)(BH)max / (kJ⋅m-3)
600161.70.860.336.538.84
650226.40.900.416.8015.92
680257.70.880.416.9116.88
表1  不同烧结温度下SmFe11Ti1纳米晶合金的磁性能和密度
图6  600 ℃烧结得到的SmFe11Ti1试样的微观组织分析
图7  680 ℃烧结得到的SmFe11Ti1试样的微观组织结构分析
图8  纳米晶SmFe11Ti1合金经不同淬火工艺后的物相组成和磁性能
图9  800 ℃保温15 min后淬火得到的SmFe11Ti1试样的微观组织分析
[1] Jones N. Materials science: The pull of stronger magnets[J]. Nature, 2011, 472: 22
doi: 10.1038/472022a
[2] Xu W W, Song X Y, Zhang Z X. Thermodynamic study on metastable phase: From polycrystalline to nanocrystalline system[J]. Appl. Phys. Lett., 2010, 97: 181911
doi: 10.1063/1.3509407
[3] Takahashi Y, Sepehri-Amin H, Ohkubo T. Recent advances in SmFe12-based permanent magnets[J]. Sci. Technol. Adv. Mater., 2021, 22: 449
doi: 10.1080/14686996.2021.1913038
[4] Guo Z H, Li W. Room- and high-temperature magnetic properties of Sm(CobalFe x Cu0.088Zr0.025)7.5 (x = 0-0.30) sintered magnets[J]. Acta Metall. Sin., 2002, 38: 866
[4] 郭朝晖, 李 卫. Sm(CobalFe x Cu0.088Zr0.025)7.5 (x = 0~ 0.30)烧结永磁体的磁性及其高温特性[J]. 金属学报, 2002, 38: 866
[5] Li J, Tang X, Sepehri-Amin H, et al. Angular dependence and thermal stability of coercivity of Nd-rich Ga-doped Nd-Fe-B sintered magnet[J]. Acta Mater., 2020, 187: 66
doi: 10.1016/j.actamat.2020.01.035
[6] Pathak A K, Khan M, Gschneidner Jr K A, et al. Cerium: An unlikely replacement of dysprosium in high performance Nd-Fe-B permanent magnets[J]. Adv. Mater., 2015, 27: 2663
doi: 10.1002/adma.v27.16
[7] Sato T, Ohsuna T, Yano M, et al. Permanent magnetic properties of NdFe12N x sputtered films epitaxially grown on V buffer layer[J]. J. Appl. Phys., 2017, 122: 053903
[8] Liu Z W, He J Y. Several issues on the development of grain boundary diffusion process for Nd-Fe-B permanent magnets[J]. Acta Metall. Sin., 2021, 57: 1155
[8] 刘仲武, 何家毅. 钕铁硼永磁晶界扩散技术和理论发展的几个问题[J]. 金属学报, 2021, 57: 1155
doi: 10.11900/0412.1961.2020.00438
[9] Hirayama Y, Takahashi Y K, Hirosawa S, et al. Intrinsic hard magnetic properties of Sm (Fe1 - x Co x )12 compound with the ThMn12 structure[J]. Scr. Mater., 2017, 138: 62
doi: 10.1016/j.scriptamat.2017.05.029
[10] Li Y C, Yu N J, Pan M X, et al. Research progress on SmFe12-based permanent magnet alloys[J]. J. Magn. Mater. Devices, 2022, 53(6): 111
[10] 李迎畅, 俞能君, 泮敏翔 等. SmFe12基永磁合金研究进展[J]. 磁性材料及器件, 2022, 53(6): 111
[11] Ohashi K, Tawara Y, Osugi R, et al. Identification of the intermetallic compound consisting of Sm, Ti, Fe[J]. J. Less-Common Met., 1998, 139: L1
doi: 10.1016/0022-5088(88)90020-3
[12] Harashima Y, Fukazawa T, Kino H, et al. Effect of R-site substitution and the pressure on stability of RFe12: A first-principles study[J]. J. Appl. Phys., 2018, 124: 163902
doi: 10.1063/1.5050057
[13] Harashima Y, Terakura K, Kino H, et al. First-principles study on stability and magnetism of NdFe11 M and NdFe11Mn for M = Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn[J]. J. Appl. Phys., 2016, 120: 203904
doi: 10.1063/1.4968798
[14] Yang Y C, Kong L S, Sun S H, et al. Intrinsic magnetic properties of SmTiFe10 [J]. J. Appl. Phys., 1988, 63: 3702
doi: 10.1063/1.340667
[15] De Mooij D B, Buschow K H J. Some novel ternary ThMn12-type compounds[J]. J. Less-Common Met., 1988, 136: 207
doi: 10.1016/0022-5088(88)90424-9
[16] Dirba I, Harashima Y, Sepehri-Amin H, et al. Thermal decomposition of ThMn12-type phase and its optimum stabilizing elements in SmFe12-based alloys[J]. J. Alloys Compd., 2020, 813: 152224
doi: 10.1016/j.jallcom.2019.152224
[17] Tang X, Li J, Srinithi A K, et al. Role of V on the coercivity of SmFe12-based melt-spun ribbons revealed by machine learning and microstructure characterizations[J]. Scr. Mater., 2021, 200: 113925
doi: 10.1016/j.scriptamat.2021.113925
[18] Hadjipanayis G C, Gabay A M, Schönhöbel A M, et al. ThMn12-type alloys for permanent magnets[J]. Engineering, 2020, 6: 141
doi: 10.1016/j.eng.2018.12.011
[19] Saito T, Watanabe F, Nishio-Hamane D. Magnetic properties of SmFe12-based magnets produced by spark plasma sintering method[J]. J. Alloys Compd., 2019, 773: 1018
doi: 10.1016/j.jallcom.2018.09.297
[20] Li Y C, Yu N J, Wu Q, et al. Novel method for preparation of high-performance SmFe12/α-Fe nanocomposite magnets by rapid thermal processing[J]. J. Alloys Compd., 2023, 954: 170056
doi: 10.1016/j.jallcom.2023.170056
[21] Qian H D, Lim J T, Kim J W, et al. Phase transformation and magnetic properties of fully dense Sm(Fe0.8Co0.2)11Ti bulk magnets[J]. Scr. Mater., 2021, 193: 17
doi: 10.1016/j.scriptamat.2020.10.030
[22] Zhang D L. Processing of advanced materials using high-energy mechanical milling[J]. Prog. Mater. Sci., 2004, 49: 537
doi: 10.1016/S0079-6425(03)00034-3
[23] Luo Y, Yu D B, LI H W, et al. Structure and permanent magnetic properties of SmFe x (x = 3~8) melt spun ribbons during heat treatment[J]. J. Rare Earth, 2014, 32: 960
doi: 10.1016/S1002-0721(14)60169-1
[24] Maât N, Lardé R, Nachbaur V, et al. Investigation by Mössbauer spectroscopy and atom probe tomography of the phase transformation of Nd-Fe-B alloys after high-energy ball milling[J]. J. Appl. Phys., 2018, 124: 223905
doi: 10.1063/1.5048619
[25] Liu K, Wang S H, Feng Y L, et al. Phase transformation mechanism and magnetic properties of Sm-Fe alloys produced by melt-spinning and high-energy ball milling[J]. J. Magn. Magn. Mater., 2020, 513: 167229
doi: 10.1016/j.jmmm.2020.167229
[26] Xiao Q F, Sun X K, Geng D Y, et al. Structure and magnetic properties of rapidly quenched Sm-Fe-Ti alloys[J]. J. Magn. Magn. Mater., 1995, 140-144: 1093
doi: 10.1016/0304-8853(94)01251-2
[27] Sun H, Otani Y, Coey J M D, et al. Coercivity and microstructure of melt-spun Sm(Fe11Ti)[J]. J. Appl. Phys., 1990, 67: 4659
doi: 10.1063/1.344845
[28] Tozman P, Sepehri-Amin H, Hono K. Prospects for the development of SmFe12-based permanent magnets with a ThMn12-type phase[J]. Scr. Mater., 2021, 194: 113686
doi: 10.1016/j.scriptamat.2020.113686
[29] Jang T S, Stadelmaier H H. Phase equilibria and magnetic properties of iron-rich Fe-Nd-Ti and Fe-Sm-Ti alloys[J]. J. Appl. Phys., 1990, 67: 4957
doi: 10.1063/1.344746
[30] Schrefl T, Fidler J, Kronmüller H. Remanence and coercivity in isotropic nanocrystalline permanent magnets[J]. Phys. Rev., 1994, 49B: 6100
[31] Polin N, Gabay A M, Han C Y, et al. Understanding high coercivity in ThMn12-type Sm-Zr-Fe-Co-Ti permanent magnet powders through nanoscale analysis[J]. Scr. Mater., 2025, 259: 116537
doi: 10.1016/j.scriptamat.2025.116537
[32] Coey J M D, Sun H. Improved magnetic properties by treatment of iron-based rare earth intermetallic compounds in anmonia[J]. J. Magn. Magn. Mater., 1990, 87: L251
doi: 10.1016/0304-8853(90)90756-G
[1] 施博文, 李艳辉, 冯拓, 王雨, 蒋丽, 于凤云, 杨陆, 张伟. 带材厚度对Fe75.2Si13B8Cu1Nb2.8纳米晶软磁合金磁畴结构和高频磁性能的影响[J]. 金属学报, 2026, 62(6): 1128-1136.
[2] 梁雨雨, 倪培远, 刘麒麟, 厉英. 稀土合金化石油套管钢精炼-连铸-轧制过程夹杂物演变行为[J]. 金属学报, 2026, 62(4): 611-626.
[3] 孙玉崇, 刘志敏, 徐振, 田双永, 田爽. Zr含量对Al-Mg-Si铸轧薄板再结晶行为和力学性能的影响[J]. 金属学报, 2026, 62(3): 421-430.
[4] 李云龙, 张子润, 于君, 赵占勇, 林鑫, 白培康. 合金化调控Nb-Si基超高温合金强韧化与抗氧化性能的研究进展[J]. 金属学报, 2026, 62(10): 1635-1654.
[5] 熊杰, 蓝慧芳, 李林鲜, 唐帅, 刘振宇, 王国栋. Cr对低碳含Ti微合金钢奥氏体等温分解行为的影响[J]. 金属学报, 2026, 62(10): 1773-1786.
[6] 张林杰, 张栩菁, 宁杰. 钼合金焊接接头高温蠕变性能研究进展[J]. 金属学报, 2026, 62(1): 47-63.
[7] 曹睿, 刘梓申. 高强钢焊缝金属强韧性研究进展[J]. 金属学报, 2026, 62(1): 64-80.
[8] 朱春健, 李艳辉, 朱正旺, 吴立成, 张海峰, 张伟. B含量调控Fe98.5 -x B x Cu1.5 纳米晶合金组织结构和磁性能[J]. 金属学报, 2025, 61(8): 1174-1182.
[9] 韩晓东, 安子冰, 毛圣成, 龙海波, 杨鲁岩, 张泽. 负混合焓合金化推动高强韧合金发展[J]. 金属学报, 2025, 61(7): 953-960.
[10] 李夫顺, 刘志鹏, 丁灿灿, 胡斌, 罗海文. 一种新型高强奥氏体低密度钢的强塑性机理[J]. 金属学报, 2025, 61(6): 909-916.
[11] 雷云龙, 杨康, 辛越, 姜自滔, 童宝宏, 张世宏. 机械合金化AlCrCu0.5Mo0.5Ni高熵合金及其后续退火态的结构演化[J]. 金属学报, 2025, 61(5): 731-743.
[12] 杨康, 辛越, 姜自滔, 刘侠, 薛召露, 张世宏. 纳米ZrB2 增强CoNiCrAlY复合粉末的机械合金化制备及其涂层的组织与性能[J]. 金属学报, 2025, 61(4): 619-631.
[13] 孙军, 刘刚, 杨冲, 张鹏, 薛航. 耐热铝合金:组织设计与合金制备[J]. 金属学报, 2025, 61(4): 521-525.
[14] 王升, 朱彦丞, 潘虎成, 李景仁, 曾志浩, 秦高梧. Yb含量对Mg-Gd-Y-Zn-Zr合金微观组织与力学性能的影响[J]. 金属学报, 2025, 61(3): 499-508.
[15] 李天瑞, 许瑜倩, 吴文平, 甘文萱, 杨永, 刘国怀, 王昭东. V和B元素对Ti-44Al-5Nb-1Mo合金显微组织及热变形机制的影响[J]. 金属学报, 2024, 60(5): 650-660.